Oxidation resistance and strength retention of ZrB2-SiC ceramics

Author keywords

B. Microstructure; C. Strength; Kinetics; Oxidation; ZrB2 SiC

Indexed keywords

B. MICROSTRUCTURE; C. STRENGTH; FLEXURAL STRENGTH; GLASS LAYERS; GLASSY LAYERS; LAYER THICKNESS; OXIDATION BEHAVIORS; OXIDE SCALE; ROOM TEMPERATURE; SIC CERAMICS; STRENGTH RETENTION; SURFACE FLAW; VISCOSITY INCREASE; WEIGHT GAIN;

EID: 77953536794     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2010.01.028     Document Type: Article
Times cited : (117)

References (20)
  • 1
    • 34248350351 scopus 로고    scopus 로고
    • Refractory diborides of zirconium and hafnium
    • Fahrenholtz W.G., Hilmas G.E. Refractory diborides of zirconium and hafnium. J Am Ceram Soc 2007, 90:1347-1364.
    • (2007) J Am Ceram Soc , vol.90 , pp. 1347-1364
    • Fahrenholtz, W.G.1    Hilmas, G.E.2
  • 3
    • 33748936677 scopus 로고    scopus 로고
    • Oxidation of zirconium diboride-silicon carbide at 1500°C at a low partial pressure of oxygen
    • Rezaie A., Fahrenholtz W.G., Hilmas G.E. Oxidation of zirconium diboride-silicon carbide at 1500°C at a low partial pressure of oxygen. J Am Ceram Soc 2006, 89:3240-3245.
    • (2006) J Am Ceram Soc , vol.89 , pp. 3240-3245
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 5
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C
    • Rezaie A., Fahrenholtz W.G., Hilmas G.E. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C. J Eur Ceram Soc 2007, 27:2495-2501.
    • (2007) J Eur Ceram Soc , vol.27 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 6
    • 33846188476 scopus 로고    scopus 로고
    • 2-SiC oxidation: formation of a SiC-depleted region
    • 2-SiC oxidation: formation of a SiC-depleted region. J Am Ceram Soc 2007, 90:143-148.
    • (2007) J Am Ceram Soc , vol.90 , pp. 143-148
    • Fahrenholtz, W.G.1
  • 8
    • 37849006084 scopus 로고    scopus 로고
    • Zirconia transport by liquid convection during oxidation of zirconium diboride-silicon carbide
    • Karlsdottir S.N., Halloran J.W., Grundy A.N. Zirconia transport by liquid convection during oxidation of zirconium diboride-silicon carbide. J Am Ceram Soc 2008, 91:272-277.
    • (2008) J Am Ceram Soc , vol.91 , pp. 272-277
    • Karlsdottir, S.N.1    Halloran, J.W.2    Grundy, A.N.3
  • 9
    • 60849108043 scopus 로고    scopus 로고
    • 2-SiC: influence of SiC content on solid and liquid oxide phase formation
    • 2-SiC: influence of SiC content on solid and liquid oxide phase formation. J Am Ceram Soc 2009, 92:481-486.
    • (2009) J Am Ceram Soc , vol.92 , pp. 481-486
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 10
    • 34247200063 scopus 로고    scopus 로고
    • Resistance to thermal shock and to oxidation of metal diborides-SiC ceramics for aerospace application
    • Monteverde F., Scatteia L. Resistance to thermal shock and to oxidation of metal diborides-SiC ceramics for aerospace application. J Am Ceram Soc 2007, 90:1130-1138.
    • (2007) J Am Ceram Soc , vol.90 , pp. 1130-1138
    • Monteverde, F.1    Scatteia, L.2
  • 12
    • 69649095305 scopus 로고    scopus 로고
    • Oxidation behavior of zirconium diboride silicon carbide produced by the spark plasma sintering method
    • Carney C.M., Mogilvesky P., Parthasarathy T.A. Oxidation behavior of zirconium diboride silicon carbide produced by the spark plasma sintering method. J Am Ceram Soc 2009, 92:2046-2052.
    • (2009) J Am Ceram Soc , vol.92 , pp. 2046-2052
    • Carney, C.M.1    Mogilvesky, P.2    Parthasarathy, T.A.3
  • 13
    • 0032672858 scopus 로고    scopus 로고
    • Effect of oxidation on the room-temperature flexural strength of reaction-bonded silicon carbides
    • Kim H.W., Kim H.E., Song H., Ha J. Effect of oxidation on the room-temperature flexural strength of reaction-bonded silicon carbides. J Am Ceram Soc 1999, 82:1601-1604.
    • (1999) J Am Ceram Soc , vol.82 , pp. 1601-1604
    • Kim, H.W.1    Kim, H.E.2    Song, H.3    Ha, J.4
  • 17
    • 0028529166 scopus 로고
    • Kinetics and mechanism of oxidation of silicon nitride bonded silicon carbide ceramic
    • Thorley M., Banks R. Kinetics and mechanism of oxidation of silicon nitride bonded silicon carbide ceramic. J Thermal Anal Calorim 1994, 42:811-822.
    • (1994) J Thermal Anal Calorim , vol.42 , pp. 811-822
    • Thorley, M.1    Banks, R.2
  • 19
    • 0002830402 scopus 로고
    • Multiple law modelling for the oxidation of advanced ceramics and a model-independent figure of merit
    • Kluwer Academic Pub., Dordrecht (NL), K.G. Nickel (Ed.)
    • Nickel K.G. Multiple law modelling for the oxidation of advanced ceramics and a model-independent figure of merit. Corrosion of advanced ceramics-measurement and modelling 1994, 59-72. Kluwer Academic Pub., Dordrecht (NL). K.G. Nickel (Ed.).
    • (1994) Corrosion of advanced ceramics-measurement and modelling , pp. 59-72
    • Nickel, K.G.1
  • 20
    • 0031167886 scopus 로고    scopus 로고
    • Effect of oxide devitrification on oxidation kinetics of SiC
    • Ogbuji L.U.J.T. Effect of oxide devitrification on oxidation kinetics of SiC. J Am Ceram Soc 1997, 80:1544-1550.
    • (1997) J Am Ceram Soc , vol.80 , pp. 1544-1550
    • Ogbuji, L.U.J.T.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.