Volumn 28, Issue 2, 2010, Pages 161-180

Influence of magnesium hydroxide and huntite hydromagnesite on mechanical properties of ethylene vinyl acetate compounds crosslinked by dicumyl peroxide and ionizing radiation

Author keywords

EVA; Flame retardancy; Halogen free; Huntite hydromagnesite; Magnesium hydroxide; Wire and cable

Indexed keywords

FLAME RETARDANCY; HALOGEN-FREE; HUNTITE; HYDROMAGNESITE; MAGNESIUM HYDROXIDE; WIRE AND CABLE;

EID: 77952605076     PISSN: 07349041     EISSN: 15308049     Source Type: Journal    
DOI: 10.1177/0734904109340765     Document Type: Article
Times cited : (29)

References (15)
  • 1
    • 77952636668 scopus 로고    scopus 로고
    • Flame retardants based on ammonium polyphosphate and combinations for plastics
    • Mans, V. and Tortosa, E. (1998). Flame Retardants Based on Ammonium Polyphosphate and Combinations for Plastics, Flame Retardants, 98: 183-193.
    • (1998) Flame Retardants , vol.98 , pp. 183-193
    • Mans, V.1    Tortosa, E.2
  • 2
    • 34547240857 scopus 로고    scopus 로고
    • Inorganic flame retardants - Alone and in combinations
    • Rai, M. and Brown, S. (1998). Inorganic Flame Retardants - Alone and in Combinations, Flame Retardants, 98: 83-91.
    • (1998) Flame Retardants , vol.98 , pp. 83-91
    • Rai, M.1    Brown, S.2
  • 4
    • 14844320824 scopus 로고    scopus 로고
    • Spent refinery catalyst as a synergistic agent in intumescent formulations: Influence of the catalyst's particle size and constituents
    • Luciana, R., Estevao, M., Le Bras, M., Delobel, R. and Nascimento, R.S.V. (2005). Spent Refinery Catalyst as a Synergistic Agent in Intumescent Formulations: Influence of the Catalyst's Particle Size and Constituents, Polymer Degradation Stability, 88(3): 444-455.
    • (2005) Polymer Degradation Stability , vol.88 , Issue.3 , pp. 444-455
    • Luciana, R.1    Estevao, M.2    Le Bras, M.3    Delobel, R.4    Nascimento, R.S.V.5
  • 5
    • 77952623066 scopus 로고    scopus 로고
    • International Patent, Improved Cross-linked Automotive Wire WO2006/026256 A1
    • Cogen, J.M., Lin, T.S., Klier, J. and Whaley, P.D. (2006). International Patent, Improved Cross-linked Automotive Wire WO2006/026256 A1.
    • (2006)
    • Cogen, J.M.1    Lin, T.S.2    Klier, J.3    Whaley, P.D.4
  • 6
    • 84902641618 scopus 로고    scopus 로고
    • Intumescent systems for polyolefines-performance profile in electrical applications
    • Wanzke, W., Goihl, A. and Nass, B. (1998). Intumescent Systems for Polyolefines-performance Profile in Electrical Applications, Flame Retardants, 98: 195-206.
    • (1998) Flame Retardants , vol.98 , pp. 195-206
    • Wanzke, W.1    Goihl, A.2    Nass, B.3
  • 8
    • 33845447634 scopus 로고    scopus 로고
    • Effects of polystyrene-encapsulated magnesium hydroxide on rheological and flame-retarding properties of HIPS composites
    • Chang, S., Xie, T. and Yang, G. (2006). Effects of Polystyrene- encapsulated Magnesium Hydroxide on Rheological and Flame-retarding Properties of HIPS Composites, Polymer Degradation Stability, 91(12): 3266-3273.
    • (2006) Polymer Degradation Stability , vol.91 , Issue.12 , pp. 3266-3273
    • Chang, S.1    Xie, T.2    Yang, G.3
  • 9
    • 31444454576 scopus 로고    scopus 로고
    • Flammability characteristics and synergistic effect of hydrotalcite with microencapsulate red phosphorus in halogen-free flame retardant EVA composite
    • Du, L., Qu, B. and Xu, Z. (2006). Flammability Characteristics and Synergistic Effect of Hydrotalcite with Microencapsulate Red Phosphorus in Halogen-free Flame Retardant EVA Composite, Polymer Degradation Stability, 91(5): 995-1001.
    • (2006) Polymer Degradation Stability , vol.91 , Issue.5 , pp. 995-1001
    • Du, L.1    Qu, B.2    Xu, Z.3
  • 10
    • 33845438400 scopus 로고    scopus 로고
    • Melamine cyanurte-microencapsulated red phosphorus flame retard unreinforced and glass fiver reinforced polyamide 66
    • Liu, Y. and Wang, Q. (2006). Melamine Cyanurte-Microencapsulated Red Phosphorus Flame Retard Unreinforced and Glass Fiver Reinforced Polyamide 66, Polymer Degradation Stability, 91(12): 3103-3109.
    • (2006) Polymer Degradation Stability , vol.91 , Issue.12 , pp. 3103-3109
    • Liu, Y.1    Wang, Q.2
  • 11
    • 33845384843 scopus 로고    scopus 로고
    • Study of hydromagnesite and magneisum hydroxide based fire retardant systems for ethylene-vinyl acetate containing organo-modified montmorillonite
    • Laoutid, F., Gaudon, P., Taulemesse, J.M., Lopez Cuesta, J.M., Velasco, J.I. and Piechaczyk, A. (2006). Study of Hydromagnesite and Magneisum Hydroxide Based Fire Retardant Systems for Ethylene-vinyl Acetate Containing Organo-Modified Montmorillonite, Polymer Degradation Stability, 91(12): 3074-3082.
    • (2006) Polymer Degradation Stability , vol.91 , Issue.12 , pp. 3074-3082
    • Laoutid, F.1    Gaudon, P.2    Taulemesse, J.M.3    Lopez Cuesta, J.M.4    Velasco, J.I.5    Piechaczyk, A.6
  • 12
    • 33845412259 scopus 로고    scopus 로고
    • Studies of ABS-graftmaleic anhydride/clay nanocomposites: Morphologies, thermal stability and flammability properties
    • Ma, H., Xu, Z., Tong, L., Gu, A. and Fang, Z. (2006). Studies of ABS-graftmaleic Anhydride/Clay Nanocomposites: Morphologies, Thermal Stability and Flammability Properties, Polymer Degradation Stability, 91(8): 2951-2959.
    • (2006) Polymer Degradation Stability , vol.91 , Issue.8 , pp. 2951-2959
    • Ma, H.1    Xu, Z.2    Tong, L.3    Gu, A.4    Fang, Z.5
  • 13
    • 28244443310 scopus 로고    scopus 로고
    • Role of montmorillonite in flame retardancy of ethylene-vinyl acetate copolymer
    • Szep, A., Szabo, A., Toth, N., Anna, P. and Marosi, G. (2006). Role of Montmorillonite in Flame Retardancy of Ethylene-vinyl Acetate Copolymer, Polymer Degradation Stability, 9: 593-599.
    • (2006) Polymer Degradation Stability , vol.9 , pp. 593-599
    • Szep, A.1    Szabo, A.2    Toth, N.3    Anna, P.4    Marosi, G.5
  • 15
    • 77952656609 scopus 로고    scopus 로고
    • British Standard 600/1000V and 1900/3300V . BS 6724: 1997 and Thermosetting Insulated Cables for Electric Power and Lighting with Low Emission of Smoke and Corrosive Gases When Affected by Fire. BS7211
    • British Standard, 600/1000V and 1900/3300V (1998). Armoured Electric Cables Having Thermosetting Insulation and Low Emission of Smoke and Corrosive Gases When Affected By Fire. BS 6724: 1997 and Thermosetting Insulated Cables for Electric Power and Lighting with Low Emission of Smoke and Corrosive Gases When Affected by Fire. BS7211.
    • (1998) Armoured Electric Cables Having Thermosetting Insulation and Low Emission of Smoke and Corrosive Gases When Affected By Fire


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.