Volumn 25, Issue 3, 2010, Pages 327-331
|
Effect of heat-treatment temperature on the electrochemical performances of the Li2MnSiO4/C composite prepared through polyol process
|
Author keywords
Cathode material; Electrochemical performance; Lithium manganese silicate; Polyol process
|
Indexed keywords
AMORPHOUS CARBON LAYER;
CAPACITY RETENTION;
CATHODE MATERIALS;
DRIED POWDER;
ELECTROCHEMICAL EXPERIMENTS;
ELECTROCHEMICAL PERFORMANCE;
ELEMENTAL ANALYZERS;
ENERGY DISPERSIVE;
FIELD EMISSION SCANNING ELECTRON MICROSCOPES;
HEAT TREATMENT TEMPERATURE;
HIGH-RESOLUTION TRANSMISSION ELECTRON MICROSCOPES;
IMPURITY PHASE;
INITIAL DISCHARGE CAPACITIES;
INTERMEDIATE TEMPERATURES;
MANGANESE-SILICATE;
MEAN PARTICLE SIZE;
POLYOL PROCESS;
REFLUXING;
SPACE GROUPS;
ALCOHOLS;
AMORPHOUS CARBON;
ELECTRIC DISCHARGES;
ELECTRON MICROSCOPES;
ETHYLENE;
ETHYLENE GLYCOL;
FIELD EMISSION;
FIELD EMISSION CATHODES;
MANGANESE;
MANGANESE COMPOUNDS;
RIETVELD METHOD;
RIETVELD REFINEMENT;
SCANNING ELECTRON MICROSCOPY;
SILICATES;
SYNTHESIS (CHEMICAL);
TRANSMISSION ELECTRON MICROSCOPY;
X RAY DIFFRACTION;
X RAY POWDER DIFFRACTION;
LITHIUM;
|
EID: 77952006685
PISSN: 1000324X
EISSN: None
Source Type: Journal
DOI: 10.3724/SP.J.1077.2010.09472 Document Type: Article |
Times cited : (7)
|
References (18)
|