메뉴 건너뛰기




Volumn 93, Issue 5, 2010, Pages 1256-1259

Glass strengthening via high-intensity plasma-arc heating

Author keywords

[No Author keywords available]

Indexed keywords

ARC HEATING; CONSTANT SPEED; END USERS; FAILURE INITIATION; FAILURE STRESS; FOUR-POINT; HEAT-TREATED GLASS; MAXIMUM POWER DENSITY; NON-CONTACT; PROCESSING CONDITION; SODA LIME SILICATE GLASS; SPECTRUM ENERGY DISTRIBUTIONS; UNIMODAL; WEIBULL;

EID: 77951686535     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2009.03553.x     Document Type: Article
Times cited : (3)

References (22)
  • 2
    • 84977244580 scopus 로고
    • Effect of silicone quenching and acid polishing on the strength of glass
    • P. C. Fletcher J. J. Tillman Effect of Silicone Quenching and Acid Polishing on the Strength of Glass J. Am. Ceram. Soc., 47, 379 382 (1964).
    • (1964) J. Am. Ceram. Soc. , vol.47 , pp. 379-382
    • Fletcher, P.C.1    Tillman, J.J.2
  • 3
    • 0009201383 scopus 로고
    • Fracture of tempered glass
    • J. M. Barsom Fracture of Tempered Glass J. Am. Ceram. Soc., 51, 75 8 (1968).
    • (1968) J. Am. Ceram. Soc. , vol.51 , pp. 75-8
    • Barsom, J.M.1
  • 4
    • 84978559841 scopus 로고
    • Strength and static fatigue of abraded glass under controlled ambient conditions: III, Aging of fresh abrasions
    • R. E. Mould Strength and Static Fatigue of Abraded Glass Under Controlled Ambient Conditions: III, Aging of Fresh Abrasions J. Am. Ceram. Soc., 43, 160 167 (1960).
    • (1960) J. Am. Ceram. Soc. , vol.43 , pp. 160-167
    • Mould, R.E.1
  • 5
    • 0025418473 scopus 로고
    • Strengthening of glass by sol-gel coatings
    • B. D. Fabes D. R. Uhlmann Strengthening of Glass by Sol-Gel Coatings J. Am. Ceram. Soc., 73, 978 978 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 978-978
    • Fabes, B.D.1    Uhlmann, D.R.2
  • 7
    • 0023451541 scopus 로고
    • Strengthening of glass tubes and containers by flame-sprayed glazing
    • M. R. Sozanski A. K. Varshneya Strengthening of Glass Tubes and Containers by Flame-Sprayed Glazing Am. Ceram. Soc. Bull., 66, 1630 1634 (1987).
    • (1987) Am. Ceram. Soc. Bull. , vol.66 , pp. 1630-1634
    • Sozanski, M.R.1    Varshneya, A.K.2
  • 9
    • 8344245443 scopus 로고    scopus 로고
    • Oxycombustion for glass conditioning and fire polishing
    • P. Zuccelli Oxycombustion for Glass Conditioning and Fire Polishing Int. Glass J., 133, 26 31 (2004).
    • (2004) Int. Glass J. , vol.133 , pp. 26-31
    • Zuccelli, P.1
  • 10
    • 33646015399 scopus 로고    scopus 로고
    • The use of high density infrared heating for surface modification/ coatings processes
    • Edited by T. S. Sudarshan, M. Jeandin, and J. J. Stiglich. ASM International, Materials Park, OH
    • J. D. K. Rivard, C. A. Blue, A. Sabau, E. K. Ohriner, G. M. Ludtka, T. N. Tiegs J. J. Stiglich The Use of High Density Infrared Heating for Surface Modification/Coatings Processes pp.139-146 in Surface Modification Technologies XVIII, Edited by T. S. Sudarshan, M. Jeandin, and J. J. Stiglich. ASM International, Materials Park, OH, 2006.
    • (2006) Surface Modification Technologies XVIII , pp. 139-146
    • Rivard, J.D.K.1    Blue, C.A.2    Sabau, A.3    Ohriner, E.K.4    Ludtka, G.M.5    Tiegs, T.N.6    Stiglich, J.J.7
  • 11
    • 33845943022 scopus 로고    scopus 로고
    • Elastic property determination of WC spheres and estimation of compressive loads and impact velocities that initiate their yielding and cracking
    • A. A. Wereszczak Elastic Property Determination of WC Spheres and Estimation of Compressive Loads and Impact Velocities That Initiate Their Yielding and Cracking Ceram. Eng. Sci. Proc., 27 [7] 211 223 (2006).
    • (2006) Ceram. Eng. Sci. Proc. , vol.27 , Issue.7 , pp. 211-223
    • Wereszczak, A.A.1
  • 12
    • 0016482865 scopus 로고
    • Strength and dynamic fatigue of float glass surfaces
    • R. R. Tummala B. J. Foster Strength and Dynamic Fatigue of Float Glass Surfaces J. Am. Ceram. Soc., 58, 156 157 (1975).
    • (1975) J. Am. Ceram. Soc. , vol.58 , pp. 156-157
    • Tummala, R.R.1    Foster, B.J.2
  • 13
    • 85028830231 scopus 로고    scopus 로고
    • Fatigue behavior of surface flaws on air vs. Tin side of soda-lime-silica float glass. Paper T4.3 in glass in the new millennium: Challenges and break-through technologies
    • May 15-17, 2000, National Committee Netherlands Glass Industry (NCNG), Amsterdam, the Netherlands
    • R. Akcakaya, S. Gulati J. R. Varner Fatigue Behavior of Surface Flaws on Air vs. Tin Side of Soda-Lime-Silica Float Glass. Paper T4.3 in Glass in the New Millennium: Challenges and Break-Through Technologies Proceedings of the ICG Annual Meeting 2000, May 15-17, 2000, National Committee Netherlands Glass Industry (NCNG), Amsterdam, the Netherlands, 2000.
    • (2000) Proceedings of the ICG Annual Meeting 2000
    • Akcakaya, R.1    Gulati, S.2    Varner, J.R.3
  • 18
    • 0037355661 scopus 로고    scopus 로고
    • Weibull strength scaling for standardized rectangular flexure specimens
    • G. D. Quinn Weibull Strength Scaling for Standardized Rectangular Flexure Specimens J. Am. Ceram. Soc., 86, 508 510 (2003).
    • (2003) J. Am. Ceram. Soc. , vol.86 , pp. 508-510
    • Quinn, G.D.1
  • 20
    • 33845996139 scopus 로고    scopus 로고
    • Exclusivity of strength-limiting extrinsic surface and hybrid flaws
    • A. A. Wereszczak T. P. Kirkland Exclusivity of Strength-Limiting Extrinsic Surface and Hybrid Flaws Ceram. Eng. Sci. Proc., 27 [2] 593 601 (2006).
    • (2006) Ceram. Eng. Sci. Proc. , vol.27 , Issue.2 , pp. 593-601
    • Wereszczak, A.A.1    Kirkland, T.P.2
  • 21
    • 0020846971 scopus 로고
    • Compressive surface strengthening of brittle materials by a residual stress distribution
    • D. J. Green Compressive Surface Strengthening of Brittle Materials by a Residual Stress Distribution J. Am. Ceram. Soc., 66, 807 810 (1983).
    • (1983) J. Am. Ceram. Soc. , vol.66 , pp. 807-810
    • Green, D.J.1
  • 22
    • 0023362528 scopus 로고
    • How surface flaws affect glass strength
    • W. C. LaCourse How Surface Flaws Affect Glass Strength Glass Ind., 68 [7] 14 8 (1987).
    • (1987) Glass Ind. , vol.68 , Issue.7 , pp. 14-8
    • Lacourse, W.C.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.