BaTiO3 ferroelectric nanoparticles dispersed in 5CB nematic liquid crystal: Synthesis and electro-optical characterization

Author keywords

[No Author keywords available]

Indexed keywords

ELECTRO-OPTICAL; FERROELECTRIC PHASE; LIQUID CRYSTAL CELLS; ORDER PARAMETER; PURE MATERIALS; STRUCTURAL CHARACTERIZATION; SWITCHING TIME;

EID: 77951564415     PISSN: 00218979     EISSN: None     Source Type: Journal    
DOI: 10.1063/1.3369544     Document Type: Article
Times cited : (72)

References (27)
  • 2
    • 62749151023 scopus 로고    scopus 로고
    • 0370-1573,. 10.1016/S0370-1573(00)00144-7
    • H. Stark, Phys. Rep. 0370-1573 351, 387 (2001). 10.1016/S0370-1573(00) 00144-7
    • (2001) Phys. Rep. , vol.351 , pp. 387
    • Stark, H.1
  • 4
    • 33745242324 scopus 로고    scopus 로고
    • 3 nanoparticles synthesized by RF-plasma CVD
    • DOI 10.1016/j.jallcom.2005.08.075, PII S0925838805015306
    • K. Suzuki and K. Kijima, J. Alloys Compd. 0925-8388 419, 234 (2006). 10.1016/j.jallcom.2005.08.075 (Pubitemid 43928552)
    • (2006) Journal of Alloys and Compounds , vol.419 , Issue.1-2 , pp. 234-242
    • Suzuki, K.1    Kijima, K.2
  • 5
    • 40849124351 scopus 로고    scopus 로고
    • Ferroelectric nanoparticles in low refractive index liquid crystals for strong electro-optic response
    • DOI 10.1063/1.2884186
    • M. Kaczmarek, O. Buchnev, and I. Nandhakumar, Appl. Phys. Lett. 0003-6951 92, 103307 (2008). 10.1063/1.2884186 (Pubitemid 351393999)
    • (2008) Applied Physics Letters , vol.92 , Issue.10 , pp. 103307
    • Kaczmarek, M.1    Buchnev, O.2    Nandhakumar, I.3
  • 10
    • 24644436819 scopus 로고    scopus 로고
    • 3 nanocrystals: Hydrothermal synthesis and structural characterization
    • DOI 10.1016/j.jcrysgro.2005.05.080, PII S0022024805007943
    • X. Zhu, J. Zhu, S. Zhou, Z. Liu, N. Ming, and D. Hesse, J. Cryst. Growth 0022-0248 283, 553 (2005). 10.1016/j.jcrysgro.2005.05.080 (Pubitemid 41277211)
    • (2005) Journal of Crystal Growth , vol.283 , Issue.3-4 , pp. 553-562
    • Zhu, X.1    Zhu, J.2    Zhou, S.3    Liu, Z.4    Ming, N.5    Hesse, D.6
  • 12
    • 33645139075 scopus 로고    scopus 로고
    • 0002-7820,. 10.1111/j.1551-2916.2005.00908.x
    • H. Nakano, K. Suzuki, and K. Kizima, J. Am. Ceram. Soc. 0002-7820 89, 1461 (2006). 10.1111/j.1551-2916.2005.00908.x
    • (2006) J. Am. Ceram. Soc. , vol.89 , pp. 1461
    • Nakano, H.1    Suzuki, K.2    Kizima, K.3
  • 14
    • 58049196721 scopus 로고    scopus 로고
    • 0925-8388,. 10.1016/j.jallcom.2008.01.045
    • R. Kavian and A. Saidi, J. Alloys Compd. 0925-8388 468, 528 (2009). 10.1016/j.jallcom.2008.01.045
    • (2009) J. Alloys Compd. , vol.468 , pp. 528
    • Kavian, R.1    Saidi, A.2
  • 15
    • 33745946815 scopus 로고    scopus 로고
    • 3 from stable chelated titanium complex: Formation mechanism and dispersibility in organic solvents
    • DOI 10.1016/j.jcis.2006.04.028, PII S0021979706003249
    • N. C. Pramanik, S. I. Seok, and B. Y. Ahn, J. Colloid Interface Sci. 0021-9797 300, 569 (2006). 10.1016/j.jcis.2006.04.028 (Pubitemid 44055947)
    • (2006) Journal of Colloid and Interface Science , vol.300 , Issue.2 , pp. 569-576
    • Pramanik, N.C.1    Seok, S.I.2    Ahn, B.Y.3
  • 17
    • 0033731418 scopus 로고    scopus 로고
    • 0002-7820,. 10.1111/j.1151-2916.2000.tb01179.x
    • J. Xue, J. Wang, and D. Wan, J. Am. Ceram. Soc. 0002-7820 83, 232 (2000). 10.1111/j.1151-2916.2000.tb01179.x
    • (2000) J. Am. Ceram. Soc. , vol.83 , pp. 232
    • Xue, J.1    Wang, J.2    Wan, D.3
  • 21
    • 0000602466 scopus 로고
    • 0021-9606,. 10.1063/1.436508
    • K. Miyano, J. Chem. Phys. 0021-9606 69, 4807 (1978). 10.1063/1.436508
    • (1978) J. Chem. Phys. , vol.69 , pp. 4807
    • Miyano, K.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.