메뉴 건너뛰기




Volumn 157, Issue 5, 2010, Pages

Numerical investigation of mechanical durability in polymer electrolyte membrane fuel cells

Author keywords

[No Author keywords available]

Indexed keywords

FUEL CELL OPERATION; IN-PLANE; LOAD OPERATIONS; MECHANICAL BEHAVIOR; MECHANICAL CONSTRAINTS; MECHANICAL DURABILITY; MECHANICAL RESPONSE; MEMBRANE ELECTRODE ASSEMBLIES; NUMERICAL INVESTIGATIONS; PERFLUOROSULFONIC ACID; PFSA MEMBRANES; POLYMER ELECTROLYTE MEMBRANE FUEL CELLS; REINFORCED COMPOSITES; REINFORCED MEMBRANES; UNIFORM DISTRIBUTION; WATER DISTRIBUTIONS; WATER TRANSPORT;

EID: 77951186145     PISSN: 00134651     EISSN: None     Source Type: Journal    
DOI: 10.1149/1.3328496     Document Type: Article
Times cited : (53)

References (59)
  • 1
    • 34548688889 scopus 로고    scopus 로고
    • The United States Department of Energy's high temperature, low relative humidity membrane program
    • DOI 10.1016/j.jpowsour.2007.01.025, PII S0378775307001346
    • N. L. Garland and J. P. Kopasz, J. Power Sources 0378-7753, 172, 94 (2007). 10.1016/j.jpowsour.2007.01.025 (Pubitemid 47418483)
    • (2007) Journal of Power Sources , vol.172 , Issue.1 , pp. 94-99
    • Garland, N.L.1    Kopasz, J.P.2
  • 6
    • 33846959064 scopus 로고    scopus 로고
    • 1938-5862. 10.1149/1.2356174
    • W. Liu and M. Crum, ECS Trans. 1938-5862, 3 (1), 531 (2006). 10.1149/1.2356174
    • (2006) ECS Trans. , vol.3 , Issue.1 , pp. 531
    • Liu, W.1    Crum, M.2
  • 8
    • 33847004317 scopus 로고    scopus 로고
    • 1938-5862. 10.1149/1.2356175
    • M. Crum and W. Liu, ECS Trans. 1938-5862, 3 (1), 541 (2006). 10.1149/1.2356175
    • (2006) ECS Trans. , vol.3 , Issue.1 , pp. 541
    • Crum, M.1    Liu, W.2
  • 10
    • 33744517283 scopus 로고    scopus 로고
    • Morphological features (defects) in fuel cell membrane electrode assemblies
    • DOI 10.1016/j.jpowsour.2005.12.027, PII S0378775305016964
    • S. Kundu, M. W. Fowler, L. C. Simon, and S. Grot, J. Power Sources 0378-7753, 157, 650 (2006). 10.1016/j.jpowsour.2005.12.027 (Pubitemid 43816199)
    • (2006) Journal of Power Sources , vol.157 , Issue.2 , pp. 650-656
    • Kundu, S.1    Fowler, M.W.2    Simon, L.C.3    Grot, S.4
  • 13
    • 33750950631 scopus 로고    scopus 로고
    • Mechanical response of fuel cell membranes subjected to a hygro-thermal cycle
    • DOI 10.1016/j.jpowsour.2006.05.020, PII S0378775306008986
    • A. Kusoglu, A. M. Karlsson, M. H. Santare, S. Cleghorn, and W. B. Johnson, J. Power Sources 0378-7753, 161, 987 (2006). 10.1016/j.jpowsour.2006. 05.020 (Pubitemid 44738752)
    • (2006) Journal of Power Sources , vol.161 , Issue.2 , pp. 987-996
    • Kusoglu, A.1    Karlsson, A.M.2    Santare, M.H.3    Cleghorn, S.4    Johnson, W.B.5
  • 18
    • 36749083010 scopus 로고    scopus 로고
    • Mechanical properties of a reinforced composite polymer electrolyte membrane and its simulated performance in PEM fuel cells
    • DOI 10.1016/j.jpowsour.2007.09.093, PII S037877530702023X
    • Y. Tang, A. Kusoglu, A. M. Karlsson, M. H. Santare, S. Cleghorn, and W. B. Johnson, J. Power Sources 0378-7753, 175, 817 (2008). 10.1016/j.jpowsour. 2007.09.093 (Pubitemid 350213293)
    • (2008) Journal of Power Sources , vol.175 , Issue.2 , pp. 817-825
    • Tang, Y.1    Kusoglu, A.2    Karlsson, A.M.3    Santare, M.H.4    Cleghorn, S.5    Johnson, W.B.6
  • 19
    • 34249871936 scopus 로고    scopus 로고
    • Mechanical behavior of fuel cell membranes under humidity cycles and effect of swelling anisotropy on the fatigue stresses
    • DOI 10.1016/j.jpowsour.2007.03.063, PII S0378775307006994
    • A. Kusoglu, A. M. Karlsson, M. H. Santare, S. Cleghorn, and W. B. Johnson, J. Power Sources 0378-7753, 170, 345 (2007). 10.1016/j.jpowsour.2007. 03.063 (Pubitemid 46873863)
    • (2007) Journal of Power Sources , vol.170 , Issue.2 , pp. 345-358
    • Kusoglu, A.1    Karlsson, A.M.2    Santare, M.H.3    Cleghorn, S.4    Johnson, W.B.5
  • 20
    • 34147122220 scopus 로고    scopus 로고
    • On mechanical behavior and in-plane modeling of constrained PEM fuel cell membranes subjected to hydration and temperature cycles
    • DOI 10.1016/j.jpowsour.2007.02.025, PII S0378775307003655
    • R. Solasi, Y. Zou, X. Huang, K. Reifsnider, and D. Condit, J. Power Sources 0378-7753, 167, 366 (2007). 10.1016/j.jpowsour.2007.02.025 (Pubitemid 46575128)
    • (2007) Journal of Power Sources , vol.167 , Issue.2 , pp. 366-377
    • Solasi, R.1    Zou, Y.2    Huang, X.3    Reifsnider, K.4    Condit, D.5
  • 25
    • 77951181409 scopus 로고    scopus 로고
    • ABAQUS, Documentation and User's Manual, ABAQUS Inc.
    • ABAQUS, Documentation and User's Manual, ABAQUS Inc. (2003).
    • (2003)
  • 30
    • 77951188213 scopus 로고    scopus 로고
    • SGL, Product Information for Sigracet GDL, SGL Carbon Grou
    • SGL, Product Information for Sigracet GDL, SGL Carbon Group.
  • 32
    • 33744542045 scopus 로고    scopus 로고
    • An experimental investigation of humidity and temperature effects on the mechanical properties of perfluorosulfonic acid membrane
    • DOI 10.1016/j.msea.2006.03.055, PII S0921509306003182
    • Y. Tang, A. M. Karlsson, M. H. Santare, M. Gilbert, S. Cleghorn, and W. B. Johnson, Mater. Sci. Eng., A 0921-5093, 425, 297 (2006). 10.1016/j.msea.2006. 03.055 (Pubitemid 43811890)
    • (2006) Materials Science and Engineering A , vol.425 , Issue.1-2 , pp. 297-304
    • Tang, Y.1    Karlsson, A.M.2    Santare, M.H.3    Gilbert, M.4    Cleghorn, S.5    Johnson, W.B.6
  • 40
    • 0018681248 scopus 로고
    • 0021-8995. 10.1002/ap1979.070241102
    • A. E. T. Takamatsu, J. Appl. Polym. Sci. 0021-8995, 24, 2221 (1979). 10.1002/app.1979.070241102
    • (1979) J. Appl. Polym. Sci. , vol.24 , pp. 2221
    • Takamatsu, A.E.T.1
  • 43
    • 0242425870 scopus 로고    scopus 로고
    • 0013-4651. 10.1149/1.1611489
    • A. A. Kulikovsky, J. Electrochem. Soc. 0013-4651, 150, A1432 (2003). 10.1149/1.1611489
    • (2003) J. Electrochem. Soc. , vol.150 , pp. 1432
    • Kulikovsky, A.A.1
  • 46
    • 0032317133 scopus 로고    scopus 로고
    • 0013-4686. 10.1016/S0013-4686(97)10099-8
    • T. Okada, G. Xie, and M. Meeg, Electrochim. Acta 0013-4686, 43, 2141 (1998). 10.1016/S0013-4686(97)10099-8
    • (1998) Electrochim. Acta , vol.43 , pp. 2141
    • Okada, T.1    Xie, G.2    Meeg, M.3
  • 52
  • 55
    • 35748969892 scopus 로고    scopus 로고
    • Physical degradation of membrane electrode assemblies undergoing freeze/thaw cycling: Micro-structure effects
    • DOI 10.1016/j.jpowsour.2007.08.111, PII S0378775307017636, Hybrid Electric Vehicles
    • S. Kim and M. M. Mench, J. Power Sources 0378-7753, 174, 206 (2007). 10.1016/j.jpowsour.2007.08.111 (Pubitemid 350051659)
    • (2007) Journal of Power Sources , vol.174 , Issue.1 , pp. 206-220
    • Kim, S.1    Mench, M.M.2
  • 57
    • 33845274285 scopus 로고    scopus 로고
    • Freeze/thaw effects in PEM fuel cells
    • DOI 10.1149/1.2214572, Durability and Reliability of Low-Temperature Fuel Cells Systems
    • R. Mukundan, S. K. Yu, F. Garzon, and B. Pivovar, ECS Trans. 1938-5862, 1 (8) 403 (2005). 10.1149/1.2214572 (Pubitemid 44866264)
    • (2005) ECS Transactions , vol.1 , Issue.8 , pp. 403-413
    • Mukundan, R.1    Yu, S.K.2    Garzon, F.3    Pivovar, B.4
  • 58
    • 77649235159 scopus 로고    scopus 로고
    • 0032-3861. 10.1016/j.polymer.2010.01.046
    • A. Kusoglu, A. Karlsson, and M. Santare, Polymer 0032-3861, 51, 1457 (2010). 10.1016/j.polymer.2010.01.046
    • (2010) Polymer , vol.51 , pp. 1457
    • Kusoglu, A.1    Karlsson, A.2    Santare, M.3
  • 59
    • 33947722781 scopus 로고    scopus 로고
    • PEM fuel cell electrocatalyst durability measurements
    • DOI 10.1016/j.jpowsour.2006.03.009, PII S0378775306004101
    • R. L. Borup, J. R. Davey, F. H. Garzon, D. L. Wood, and M. A. Inbody, J. Power Sources 0378-7753, 163, 76 (2006). 10.1016/j.jpowsour.2006.03.009 (Pubitemid 46505294)
    • (2006) Journal of Power Sources , vol.163 , Issue.1 SPEC. ISS. , pp. 76-81
    • Borup, R.L.1    Davey, J.R.2    Garzon, F.H.3    Wood, D.L.4    Inbody, M.A.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.