Volumn 30, Issue 8, 2004, Pages 2067-2073

Low temperature sintering and microwave dielectric properties of 0.5LaAlO3-0.5SrTiO3 ceramics using copper oxide additions

Author keywords

LaAlO3 SrTiO3 ceramics; Microwave dielectric properties; Sintering aid

Indexed keywords

ALUMINUM COMPOUNDS; CERAMIC MATERIALS; COPPER OXIDES; DOPING (ADDITIVES); MICROWAVES; RESONANCE; RESONATORS; THERMAL EFFECTS; VACUUM; X RAY DIFFRACTION;

EID: 7544243453     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ceramint.2003.10.016     Document Type: Article
Times cited : (14)