메뉴 건너뛰기




Volumn 18, Issue SPEC. ISSUE 1, 2008, Pages

Corrosion and mechanical properties of hot-extruded AZ31 magnesium alloys

Author keywords

AZ31 magnesium alloy; Corrosion properties; Hot extrusion; Mechanical properties

Indexed keywords

CORROSION RESISTANCE; CORROSION RESISTANT ALLOYS; CORROSIVE EFFECTS; EXTRUSION; GALVANIC CORROSION; GRAIN REFINEMENT; MECHANICAL PROPERTIES; TENSILE STRENGTH; TENSILE TESTING;

EID: 71649103647     PISSN: 10036326     EISSN: None     Source Type: Journal    
DOI: 10.1016/s1003-6326(10)60190-2     Document Type: Article
Times cited : (24)

References (15)
  • 4
    • 37049039425 scopus 로고    scopus 로고
    • Microstructures and mechanical properties of double hot-extruded AZ80+xSr wrought alloys [J]
    • GUAN Shao-kang, ZHU Shi-jie, WANG Li-guo, YANG Qing, CAO Wen-bo. Microstructures and mechanical properties of double hot-extruded AZ80+xSr wrought alloys [J]. Trans Nonferrous Met Soc China, 2007,17(6): 1143-1151.
    • (2007) Trans Nonferrous Met Soc China , vol.17 , Issue.6 , pp. 1143-1151
    • Guan, S.-K.1    Zhu, S.-J.2    Wang, L.-G.3    Yang, Q.4    Cao, W.-B.5
  • 5
    • 34447277906 scopus 로고    scopus 로고
    • 12 intermetallic compounds on the hot extruded microstructures and mechanical properties of Mg-9Al-1Zn alloy [J]
    • 12 intermetallic compounds on the hot extruded microstructures and mechanical properties of Mg-9Al-1Zn alloy [J]. Materials Science and Engineering A, 2007, 466: 134-139.
    • (2007) Materials Science and Engineering a , vol.466 , pp. 134-139
    • Li, Z.-F.1    Dong, J.2    Zeng, X.-Q.3    Lu, C.4    Ding, W.-J.5
  • 6
    • 0031351412 scopus 로고    scopus 로고
    • Microstructural development in Mg alloy AZ31 during hot working
    • PII S1359646297003448
    • MWEMBELA A, KONOPLEVA E B, MCQUEEN H J. Microstructural development in Mg alloy AZ31 during hot working [J]. Scripta Materialia, 1997, 37(11): 1789-1795. (Pubitemid 127395337)
    • (1997) Scripta Materialia , vol.37 , Issue.11 , pp. 1789-1795
    • Mwembela, A.1    Konopleva, E.B.2    McQueen, H.J.3
  • 7
    • 71649087678 scopus 로고    scopus 로고
    • Effects of hot extrusion and annealing treatment on microstructures, properties and texture of AZ31 Mg alloy [J]
    • ZHANG Hui, YAN Yun-qi, WENG Wen-ping, ZHONG Hao, CHEN Qi. Effects of hot extrusion and annealing treatment on microstructures, properties and texture of AZ31 Mg alloy [J]. Trans Nonferrous Met Soc China, 2006, 16(s3): s1732-s1735.
    • (2006) Trans Nonferrous Met Soc China , vol.16 , Issue.S3
    • Zhang, H.1    Yan, Y.-Q.2    Weng, W.-P.3    Zhong, H.4    Chen, Q.5
  • 8
    • 33947260152 scopus 로고    scopus 로고
    • Influence of hot extrusion on microstructure and mechanical properties of AZ31 magnesium alloy [J]
    • WANG Ling, TIAN Su-gui, MENG Fan-lai, DU Hong-qiang. Influence of hot extrusion on microstructure and mechanical properties of AZ31 magnesium alloy [J]. Trans Nonferrous Met Soc China, 2006, 16(s3): s1770-s1773.
    • (2006) Trans Nonferrous Met Soc China , vol.16 , Issue.S3
    • Wang, L.1    Tian, S.-G.2    Meng, F.-L.3    Du, H.-Q.4
  • 9
    • 33748058500 scopus 로고    scopus 로고
    • Effect of extrusion conditions on grain refinement and fatigue behaviour in magnesium alloys
    • DOI 10.1016/j.msea.2006.06.117, PII S0921509306012123
    • UEMATSU Y, TOKAJI K, KAMAKURA M, UCHIDA K, SHIBATA H, BEKKU N. Effect of extrusion conditions on grain refinement and fatigue behaviour in magnesium alloys [J]. Materials Science and Engineering A, 2006, 434(1/2): 131-140. (Pubitemid 44296300)
    • (2006) Materials Science and Engineering a , vol.434 , Issue.1-2 , pp. 131-140
    • Uematsu, Y.1    Tokaji, K.2    Kamakura, M.3    Uchida, K.4    Shibata, H.5    Bekku, N.6
  • 10
    • 13844267489 scopus 로고    scopus 로고
    • Galvanic corrosion properties of differently PVD-treated magnesium die cast alloy AZ91D [J]
    • HPCHE H, BLAWERT C, BROSZEIT E, BERGER C. Galvanic corrosion properties of differently PVD-treated magnesium die cast alloy AZ91D [J]. Surface & Coating Technology, 2005, 193: 223-229.
    • (2005) Surface & Coating Technology , vol.193 , pp. 223-229
    • Hpche, H.1    Blawert, C.2    Broszeit, E.3    Berger, C.4
  • 11
    • 0001680694 scopus 로고    scopus 로고
    • Corrosion Behavior of Rapidly Solidified Magnesium-Aluminum-Zinc Alloys
    • DALOZ D, STEINMETZ P, MICHOT G. Corrosion behavior of rapidly solidified magnesium-aluminum-zinc alloys [J]. Corrosion, 1997, 53(12): 944-954. (Pubitemid 127479599)
    • (1997) Corrosion (Houston) , vol.53 , Issue.12 , pp. 944-954
    • Daloz, D.1    Steinmetz, P.2    Michot, G.3
  • 13
    • 0033196585 scopus 로고    scopus 로고
    • Corrosion mechanisms of magnesium alloys [J]
    • SONG G L, ATRENS A. Corrosion mechanisms of magnesium alloys [J]. Advanced Engineering Materials, 1999, 1(1): 11-33.
    • (1999) Advanced Engineering Materials , vol.1 , Issue.1 , pp. 11-33
    • Song, G.L.1    Atrens, A.2
  • 14
    • 0345711477 scopus 로고    scopus 로고
    • Influence of microstructure on the corrosion of diecast AZ91D
    • DOI 10.1016/S0010-938X(98)00121-8, PII S0010938X98001218
    • SONG G L, ATRENS A, DARGUSCH M. Influence of microstructure on the corrosion of die cast AZ91D [J]. Corrosion Science, 1999, 41: 249-273. (Pubitemid 29306162)
    • (1999) Corrosion Science , vol.41 , Issue.2 , pp. 249-273
    • Song, G.1    Atrens, A.2    Dargusch, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.