Structural and transport evolution in the LixAg2V4O11 system

Author keywords

Ag2V4O11; Cathode; ICD; In situ XRD measurements; Primary lithium batteries; SVO

Indexed keywords

AMORPHOUS STRUCTURES; DC CONDUCTIVITY; DIFFERENT SLOPES; DISPLACEMENT REACTIONS; ELECTROCHEMICAL DISCHARGE; ELECTROCHEMICAL PERFORMANCE; ELECTRONIC CONDUCTIVITY; ESR SPECTROSCOPY; ICD; IN-SITU XRD; IONIC RADIUS; LOW TEMPERATURES; NANO-SIZED; ORIGINAL STRUCTURES; SILVER METAL; SILVER REDUCTION; STRUCTURAL COLLAPSE; THERMOPOWER MEASUREMENTS;

EID: 71549161818     PISSN: 03787753     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jpowsour.2009.08.091     Document Type: Article
Times cited : (34)

References (35)
  • 23
    • 72249119511 scopus 로고    scopus 로고
    • Fullprof (v. Dec. 2005), T. Roisnel (LCSIM, Rennes), J. Rodriguez-Carjaval (LLB, CEA-CNRS), France, 2005.
    • Fullprof (v. Dec. 2005), T. Roisnel (LCSIM, Rennes), J. Rodriguez-Carjaval (LLB, CEA-CNRS), France, 2005.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.