1
-
-
33845383173
-
The effects of ageing by ultraviolet degradation of recycled polyolefin blends
-
Attwood, J. Philip, M. Hulme, A. Williams, G. and Shipton, P. 2006. The effects of ageing by ultraviolet degradation of recycled polyolefin blends. Pol. Deg. Stab. 91:3407-3415.
-
(2006)
Pol. Deg. Stab
, vol.91
, pp. 3407-3415
-
-
Attwood, J.1
Philip, M.2
Hulme, A.3
Williams, G.4
Shipton, P.5
-
2
-
-
0013352561
-
Characterization of polyolefins by Differential Thermal Analysis
-
Bacon, KE 1960. Characterization of polyolefins by Differential Thermal Analysis. J. Pol. Sci. XLII:15-23.
-
(1960)
J. Pol. Sci
, vol.42
, pp. 15-23
-
-
Bacon, K.E.1
-
3
-
-
3042766087
-
Degradation Characterisation of Agricultural Low Density Polyethylene Films
-
Briassoulis, D., Aristopoulou, A., Bonora, M. and Verlodt, I. 2004. Degradation Characterisation of Agricultural Low Density Polyethylene Films. Bio. Eng. 88:131-143.
-
(2004)
Bio. Eng
, vol.88
, pp. 131-143
-
-
Briassoulis, D.1
Aristopoulou, A.2
Bonora, M.3
Verlodt, I.4
-
4
-
-
14844315724
-
The Effects of Tensile Stress and the Agrochemical Vapam on the Ageing of Low Density Polyethylene (LDPE) Agricultural Films. Part I. Mechanical Behaviour
-
Briassoulis, D. 2005. The Effects of Tensile Stress and the Agrochemical Vapam on the Ageing of Low Density Polyethylene (LDPE) Agricultural Films. Part I. Mechanical Behaviour. Pol. Deg. Stab. 88:489-503.
-
(2005)
Pol. Deg. Stab
, vol.88
, pp. 489-503
-
-
Briassoulis, D.1
-
5
-
-
71449093900
-
-
Cabot company
-
Cabot company. http://www.cabot-corp.com/cws/
-
-
-
-
6
-
-
0000482430
-
Degradation and Stabilisation of Low Density Polyethylene (LDPE) Films Used as Greenhouse Covering Materials
-
Dilara, P.A. and Briassoulis, D. 2000. Degradation and Stabilisation of Low Density Polyethylene (LDPE) Films Used as Greenhouse Covering Materials. J. Ag. Eng. Res. 76:309-321.
-
(2000)
J. Ag. Eng. Res
, vol.76
, pp. 309-321
-
-
Dilara, P.A.1
Briassoulis, D.2
-
8
-
-
0030196973
-
Comparison of the UV-degradation chemistry of unstabilized and HALS-stabilized polyethylene and polypropylene
-
Gijsman, P. and Dozeman, A. 1996. Comparison of the UV-degradation chemistry of unstabilized and HALS-stabilized polyethylene and polypropylene. Pol. Deg. Stab. 53:45-50.
-
(1996)
Pol. Deg. Stab
, vol.53
, pp. 45-50
-
-
Gijsman, P.1
Dozeman, A.2
-
9
-
-
33646337166
-
Degradation of pre-aged polymers exposed to simulated recycling: Properties and thermal stability
-
Luzuriaga, Sh. Kovarova, J. and Fortelny, I. 1996. Degradation of pre-aged polymers exposed to simulated recycling: Properties and thermal stability. Pol. Deg. Stab. 91:1226-1232.
-
(1996)
Pol. Deg. Stab
, vol.91
, pp. 1226-1232
-
-
Luzuriaga, S.1
Kovarova, J.2
Fortelny, I.3
-
10
-
-
17644406418
-
Test reference year generation from meteorological and simulated solar radiation data
-
Miguel, A. and Bilbao, J. 2005. Test reference year generation from meteorological and simulated solar radiation data. Sol. En. 78:695-703.
-
(2005)
Sol. En
, vol.78
, pp. 695-703
-
-
Miguel, A.1
Bilbao, J.2
-
12
-
-
4544368574
-
Effect of photooxidation cracks on behavior of thick polypropylene samples
-
Yakimets, I., Lai, D. and Guigon, M. 2004. Effect of photooxidation cracks on behavior of thick polypropylene samples. Pol. Deg. Stab. 86:59-67.
-
(2004)
Pol. Deg. Stab
, vol.86
, pp. 59-67
-
-
Yakimets, I.1
Lai, D.2
Guigon, M.3
|