Failure analysis on a primary superheater tube of a power plant

Author keywords

Clinker; Failure analysis; Hardness; Primary superheater tube; Short term overheating

Indexed keywords

CLINKER; FAILURE MECHANISM; FINITE ELEMENT ANALYSIS; FLOW PATH; HARDNESS MEASUREMENT; IN-SITU; IN-SITU MEASUREMENT; PRIMARY SUPERHEATER TUBE; ROOT CAUSE; SHORT-TERM OVERHEATING; VISUAL INSPECTION;

EID: 70449518434     PISSN: 13506307     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.engfailanal.2009.04.017     Document Type: Article
Times cited : (64)

References (8)
  • 2
    • 7444261375 scopus 로고    scopus 로고
    • Creep failures of overheated boiler, superheater and reformer tubes
    • Jones D.R.H. Creep failures of overheated boiler, superheater and reformer tubes. Eng Fail Anal 11 (2004) 873-893
    • (2004) Eng Fail Anal , vol.11 , pp. 873-893
    • Jones, D.R.H.1
  • 4
    • 70449520273 scopus 로고    scopus 로고
    • ANSYS multiphysics version 11.0. Southpointe 275 Technology Drive Canonsburg PA, ANSYS, Inc, 2008
    • ANSYS multiphysics version 11.0. Southpointe 275 Technology Drive Canonsburg (PA): ANSYS, Inc.; 2008.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.