Volumn 30, Issue 2, 2010, Pages 555-559

Fabrication and positive temperature coefficient of resistivity properties of semiconducting ceramics based on the BaTiO3-(Bi1/2K1/2)TiO3 system

Author keywords

BaTiO3 and titanates; PTC devices

Indexed keywords

BATIO3 AND TITANATES; POSITIVE TEMPERATURE COEFFICIENT OF RESISTIVITIES; PTC DEVICES; ROOM TEMPERATURE; SEMICONDUCTING MATERIALS; SINTERING AID; TIO;

EID: 70350714252     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2009.08.009     Document Type: Article
Times cited : (32)

References (22)
  • 2
    • 0029308839 scopus 로고
    • The positive temperature coefficient of resistivity in barium titanate
    • Huybrechts B., Ishizaka K., and Takata M. The positive temperature coefficient of resistivity in barium titanate. J. Mater. Sci. 30 (1995) 2463-2474
    • (1995) J. Mater. Sci. , vol.30 , pp. 2463-2474
    • Huybrechts, B.1    Ishizaka, K.2    Takata, M.3
  • 3
    • 2342479379 scopus 로고
    • PTC thermistors as self-regulating heating elements
    • Andrich E. PTC thermistors as self-regulating heating elements. Philips Tech. Rev. 30 (1969) 170-177
    • (1969) Philips Tech. Rev. , vol.30 , pp. 170-177
    • Andrich, E.1
  • 8
    • 35548955969 scopus 로고    scopus 로고
    • 3 positive temperature coefficient of resistivity ceramics with electrically heterogeneous structure
    • 3 positive temperature coefficient of resistivity ceramics with electrically heterogeneous structure. Appl. Phys. Lett. 91 (2007) 162904
    • (2007) Appl. Phys. Lett. , vol.91 , pp. 162904
    • Xiang, P.-H.1    Takeda, H.2    Shiosaki, T.3
  • 9
    • 11144220685 scopus 로고
    • Some properties of bismuth perovskites
    • Buhrer C.F. Some properties of bismuth perovskites. J. Chem. Phys. 36 (1962) 798-803
    • (1962) J. Chem. Phys. , vol.36 , pp. 798-803
    • Buhrer, C.F.1
  • 11
    • 0016332944 scopus 로고
    • Ceramic manufacturing technology for the high performance PTC thermistor
    • Ueoka H., and Yodogawa M. Ceramic manufacturing technology for the high performance PTC thermistor. IEEE Trans. Manuf. Technol., MFT-3 (1974) 77-82
    • (1974) IEEE Trans. Manuf. Technol., MFT-3 , pp. 77-82
    • Ueoka, H.1    Yodogawa, M.2
  • 14
    • 0035395364 scopus 로고    scopus 로고
    • Effect of annealing treatments on positive temperature coefficient of resistance properties of barium titanate ceramics and a new model for the positive temperature coefficient of resistance effect
    • Gallego M.M., and West A.R. Effect of annealing treatments on positive temperature coefficient of resistance properties of barium titanate ceramics and a new model for the positive temperature coefficient of resistance effect. J. Appl. Phys. 90 (2001) 394-403
    • (2001) J. Appl. Phys. , vol.90 , pp. 394-403
    • Gallego, M.M.1    West, A.R.2
  • 15
    • 70350739674 scopus 로고    scopus 로고
    • Japan Electronic Materials Manufactures Association Standard EMAS-8202; 1988 [in Japanese].
    • Japan Electronic Materials Manufactures Association Standard EMAS-8202; 1988 [in Japanese].
  • 18
    • 0013418657 scopus 로고
    • Properties of semiconductive barium titanates
    • Saburi O. Properties of semiconductive barium titanates. J. Phys. Soc. Jpn. 14 (1959) 1159-1174
    • (1959) J. Phys. Soc. Jpn. , vol.14 , pp. 1159-1174
    • Saburi, O.1
  • 21


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.