Volumn 24, Issue 9, 2009, Pages 2986-2992

Plastic zone at crack tip: A nanolab for formation and study of metallic glassy nanostructures

Author keywords

[No Author keywords available]

Indexed keywords

BULK METALLIC GLASS; CONTROL NANOSTRUCTURES; DEFORMATION AND FRACTURE; FRACTURE SURFACES; GLASSY NANOSTRUCTURES; NANO SCALE; NANO-CONES; PLASTIC ZONE SIZE; PLASTIC ZONES; ROOM TEMPERATURE;

EID: 70350145019     PISSN: 08842914     EISSN: None     Source Type: Journal    
DOI: 10.1557/jmr.2009.0362     Document Type: Article
Times cited : (22)

References (34)
  • 1
    • 0033016303 scopus 로고    scopus 로고
    • Nanoscale materials
    • J.R. Heath: Nanoscale materials. Acc. Chem. Res. 32, 388 (1999).
    • (1999) Acc. Chem. Res. , vol.32 , pp. 388
    • Heath, J.R.1
  • 2
    • 0037122285 scopus 로고    scopus 로고
    • Ultrafast dephasing of surface plasmon excitation in silver nanoparticles: Influence of particle size, shape, and chemical surrounding
    • J. Bosbach: Ultrafast dephasing of surface plasmon excitation in silver nanoparticles: Influence of particle size, shape, and chemical surrounding. Phys. Rev. Lett. 89, 257404 (2002).
    • (2002) Phys. Rev. Lett. , vol.89 , pp. 257404
    • Bosbach, J.1
  • 3
    • 0028594017 scopus 로고
    • Nanomaterials: A membrane-based synthetic approach
    • C.R. Martin: Nanomaterials: A membrane-based synthetic approach. Science 266, 1961 (1994).
    • (1961) Science , vol.266 , pp. 1994
    • Martin, C.R.1
  • 4
    • 0030056442 scopus 로고
    • Shape-controlled synthesis of colloidal platinum nanoparticles
    • T.S. Ahmadi, Z.L. Wang, T.C. Green, A. Henglein, and MA El-Sayed: Shape-controlled synthesis of colloidal platinum nanoparticles. Science 272, 1924 (1996).
    • (1924) Science , vol.272 , pp. 1996
    • Ahmadi, T.S.1    Wang, Z.L.2    Green, T.C.3    Henglein, A.4    El-Sayed, M.5
  • 5
    • 0037206788 scopus 로고    scopus 로고
    • High tensile ductility in a nanostructured metal
    • Y.M. Wang, M.W. Chen, F.H. Zhou, and E. Ma: High tensile ductility in a nanostructured metal. Nature 419, 912 (2002).
    • (2002) Nature , vol.419 , pp. 912
    • Wang, Y.M.1    Chen, M.W.2    Zhou, F.H.3    Ma, E.4
  • 8
    • 33644932929 scopus 로고    scopus 로고
    • Molecular dynamics simulation of a solid platinum nanowire under uniaxial tensilestrain: Temperature and strain-rate effects
    • S.J.A. Koh, H.P. Lee, C. Lu, and Q.H. Cheng: Molecular dynamics simulation of a solid platinum nanowire under uniaxial tensilestrain: Temperature and strain-rate effects. Phys. Rev. B: Con-dens. Matter 72, 085414 (2005).
    • (2005) Phys. Rev. B: Con-dens. Matter , vol.72 , pp. 085414
    • Koh, S.J.A.1    Lee, H.P.2    Lu, C.3    Cheng, Q.H.4
  • 11
    • 27744436121 scopus 로고    scopus 로고
    • Metallic glasses as structural materials
    • M.F. Ashby and A.L. Greer: Metallic glasses as structural materials. Scr. Mater. 54, 321 (2006).
    • (2006) Scr. Mater. , vol.54 , pp. 321
    • Ashby, M.F.1    Greer, A.L.2
  • 14
    • 30144432185 scopus 로고    scopus 로고
    • Temperature rise at shear bands in metallic glasses
    • J.J. Lewandowski and A.L. Greer: Temperature rise at shear bands in metallic glasses. Nat. Mater. 5, 15 (2006).
    • (2006) Nat. Mater. , vol.5 , pp. 15
    • Lewandowski, J.J.1    Greer, A.L.2
  • 19
    • 0032058320 scopus 로고
    • Fracture toughness and notched toughness of bulk amorphous alloy: Zr-Ti-Ni-Cu-Be
    • P. Lowhaphandu and J.J. Lewandowski: Fracture toughness and notched toughness of bulk amorphous alloy: Zr-Ti-Ni-Cu-Be. Scr. Mater. 38, 1811 (1998).
    • (1811) Scr. Mater. , vol.38 , pp. 1998
    • Lowhaphandu, P.1    Lewandowski, J.J.2
  • 21
    • 0033097356 scopus 로고    scopus 로고
    • Local heating associated with crack tip plasticity in Zr-Ti-Ni-Cu-Be bulk amorphous metals
    • K.M. Flores and R.H. Dauskardt: Local heating associated with crack tip plasticity in Zr-Ti-Ni-Cu-Be bulk amorphous metals. J. Mater. Res. 14, 638 (1999).
    • (1999) J. Mater. Res. , vol.14 , pp. 638
    • Flores, K.M.1    Dauskardt, R.H.2
  • 23
    • 0016507662 scopus 로고
    • The mechanism of fracture in glassy materials capable of some inelastic deformation
    • A.S. Argon and M. Salama: The mechanism of fracture in glassy materials capable of some inelastic deformation. Mater. Sci. Eng. 23,219(1976).
    • (1976) Mater. Sci. Eng. , vol.23 , pp. 219
    • Argon, A.S.1    Salama, M.2
  • 25
    • 0039130878 scopus 로고    scopus 로고
    • Stabilization and high strain-rate superplasticity of metallic supercooled liquid
    • A. Inoue: Stabilization and high strain-rate superplasticity of metallic supercooled liquid. Mater. Sci. Eng., A 267, 171(1999).
    • (1999) Mater. Sci. Eng., A , vol.267 , pp. 171
    • Inoue, A.1
  • 26
    • 44949096628 scopus 로고
    • Effects of test temperature and loading conditions on the tensile properties of a Zr-based bulk metallic glass
    • 26. A.H. Vormelker, O.L. Vatamanu, L. Kecskes, and J.J. Lewandowski: Effects of test temperature and loading conditions on the tensile properties of a Zr-based bulk metallic glass. Mater. Trans. A 39, 1922 (2008).
    • (1922) Mater. Trans. A , vol.39 , Issue.2008
    • Vormelker, A.H.1    Vatamanu, O.L.2    Kecskes, L.3    Lewandowski, J.J.4
  • 27
    • 27744544663 scopus 로고    scopus 로고
    • Intrinsic plasticity or brittleness of metallic glasses
    • J.J. Lewandowski, W.H. Wang, and A.L. Greer: Intrinsic plasticity or brittleness of metallic glasses. Philos. Mag. Lett. 85, 77 (2005).
    • (2005) Philos. Mag. Lett. , vol.85 , pp. 77
    • Lewandowski, J.J.1    Wang, W.H.2    Greer, A.L.3
  • 28
    • 27744492959 scopus 로고    scopus 로고
    • Intrinsic and extrinsic toughening of metallic glasses
    • J.J. Lewandowski, M. Shazly, and A.S. Nouri: Intrinsic and extrinsic toughening of metallic glasses. Scr. Mater. 54, 337 (2006).
    • (2006) Scr. Mater. , vol.54 , pp. 337
    • Lewandowski, J.J.1    Shazly, M.2    Nouri, A.S.3
  • 30
    • 0027677515 scopus 로고
    • Scanning tunneling microscope observations of metallic glass fracture surfaces
    • D.M. Kulawansa, J.T. Dickinson, S.C. Langford, and Y. Watanabe: Scanning tunneling microscope observations of metallic glass fracture surfaces. /. Mater. Res. 8, 2543 (1993).
    • (1993) J. Mater. Res. , vol.8 , pp. 2543
    • Kulawansa, D.M.1    Dickinson, J.T.2    Langford, S.C.3    Watanabe, Y.4
  • 31
    • 0034967611 scopus 로고    scopus 로고
    • Effects of annealing and changes in stress state on fracture toughness of bulk metallic glass
    • J.J. Lewandowski: Effects of annealing and changes in stress state on fracture toughness of bulk metallic glass. Mater. Trans., JIM 42, 633 (2001).
    • (2001) Mater. Trans., JIM , vol.42 , pp. 633
    • Lewandowski, J.J.1
  • 32
  • 33
    • 33744513222 scopus 로고    scopus 로고
    • Critical Poisson's ratio for plasticity in Fe-Mo-C-B-Ln bulk amorphous steel
    • X.J. Gu, A.G. McDermott, S.J. Poon, and G.J. Shiflet: Critical Poisson's ratio for plasticity in Fe-Mo-C-B-Ln bulk amorphous steel. Appl. Phys. Lett. 88, 211905 (2006).
    • (2006) Appl. Phys. Lett. , vol.88 , pp. 211905
    • Gu, X.J.1    McDermott, A.G.2    Poon, S.J.3    Shiflet, G.J.4
  • 34
    • 33646883286 scopus 로고    scopus 로고
    • The correlation between the elastic constants and properties in bulk metallic glasses
    • W.H. Wang: The correlation between the elastic constants and properties in bulk metallic glasses. J. Appl. Phys. 99, 093506 (2006).
    • (2006) J. Appl. Phys. , vol.99 , pp. 093506
    • Wang, W.H.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.