Volumn 132, Issue 3-4, 2009, Pages 410-416

Production of middle distillate through hydrocracking of paraffin wax over NiMo/SiO2-Al2O3 catalysts: Effect of solvent in the preparation of SiO2-Al2O3 by a sol-gel method

Author keywords

Hydrocracking; Middle distillate; NiMo SiO2 Al2O 3; Paraffin wax; Sol gel method

Indexed keywords

ACTIVE SITE; CATALYTIC PERFORMANCE; DISTILLED WATER; HIGH SURFACE AREA; HYDROGENATION REACTIONS; IMPREGNATION METHODS; INTERNAL MASS TRANSFER; LARGE PORE VOLUME; LARGE PORES; METAL SPECIES; MIDDLE DISTILLATE; MIDDLE DISTILLATES; NIMO/SIO2-AL2O 3; SOL-GEL METHOD; SOL-GEL METHODS;

EID: 70349880746     PISSN: 1011372X     EISSN: 1572879X     Source Type: Journal    
DOI: 10.1007/s10562-009-0166-x     Document Type: Article
Times cited : (11)

References (30)
  • 3
    • 0037054736 scopus 로고    scopus 로고
    • Development of heavy oil hydrocracking catalysts using amorphous silica-alumina and zeolites as catalyst supports
    • DOI 10.1016/S0926-860X(02)00121-7, PII S0926860X02001217
    • MA Ali T Tatsumi T Masuda 2002 Appl Catal A Gen 233 77 90 10.1016/S0926-860X(02)00121-7 1:CAS:528:DC%2BD38XkslKisrk%3D (Pubitemid 34661477)
    • (2002) Applied Catalysis A: General , vol.233 , Issue.1-2 , pp. 77-90
    • Ali, M.A.1    Tatsumi, T.2    Masuda, T.3
  • 4
    • 34447128117 scopus 로고    scopus 로고
    • Hydrocracking of petroleum gas oil over NiW/MCM-48-USY composite catalyst
    • DOI 10.1016/j.fuproc.2007.05.001, PII S0378382007001099
    • AM Alsobaai R Zakaria BH Hameed 2007 Fuel Process Technol 88 921 928 10.1016/j.fuproc.2007.05.001 1:CAS:528:DC%2BD2sXns1Khu7w%3D (Pubitemid 47033964)
    • (2007) Fuel Processing Technology , vol.88 , Issue.9 , pp. 921-928
    • Alsobaai, A.M.1    Zakaria, R.2    Hameed, B.H.3
  • 7
    • 0033349905 scopus 로고    scopus 로고
    • Development of deep hydrodesulfurization catalysts. I. CoMo and NiMo catalysts tested with (substituted) dibenzothiophene
    • DOI 10.1016/S0378-3820(99)00033-8
    • WRAM Robinson JAR van Veen VHJ de Beer RA van Santen 1999 Fuel Process Technol 61 89 101 10.1016/S0378-3820(99)00033-8 1:CAS:528:DyaK1MXntVShtbc%3D (Pubitemid 30509825)
    • (1999) Fuel processing technology , vol.61 , Issue.1 , pp. 89-101
    • Robinson, W.R.A.M.1    Van Veen, J.A.R.2    De Beer, V.H.J.3    Van Santen, R.A.4
  • 8
    • 0033320962 scopus 로고    scopus 로고
    • Development of deep hydrodesulfurization catalysts. II. NiW, Pt and Pd catalysts tested with (substituted) dibenzothiophene
    • DOI 10.1016/S0378-3820(99)00032-6
    • WRAM Robinson JAR van Veen VHJ de Beer RA van Santen 1999 Fuel Process Technol 61 103 116 10.1016/S0378-3820(99)00032-6 1:CAS:528:DyaK1MXntVShur8%3D (Pubitemid 30509826)
    • (1999) Fuel processing technology , vol.61 , Issue.1 , pp. 103-116
    • Robinson, W.R.A.M.1    Van Veen, J.A.R.2    De Beer, V.H.J.3    Van Santen, R.A.4
  • 12
    • 66149190347 scopus 로고    scopus 로고
    • 10.1021/ef900042v 1:CAS:528:DC%2BD1MXktlGjsrs%3D
    • D Leckel 2009 Energy Fuel 23 2370 2375 10.1021/ef900042v 1:CAS:528:DC%2BD1MXktlGjsrs%3D
    • (2009) Energy Fuel , vol.23 , pp. 2370-2375
    • Leckel, D.1
  • 13
    • 2142751655 scopus 로고    scopus 로고
    • 10.1023/B:CATL.0000017082.44599.86 1:CAS:528:DC%2BD2cXhsVOrtb8%3D
    • K Fang W Wei J Ren Y Sun 2004 Catal Lett 93 235 242 10.1023/B:CATL. 0000017082.44599.86 1:CAS:528:DC%2BD2cXhsVOrtb8%3D
    • (2004) Catal Lett , vol.93 , pp. 235-242
    • Fang, K.1    Wei, W.2    Ren, J.3    Sun, Y.4
  • 14
    • 0025664874 scopus 로고
    • 10.1016/0016-2361(90)90192-S 1:CAS:528:DyaK3MXks1Sqtg%3D%3D
    • S Mohanty D Kunzru DN Saraf 1990 Fuel 69 1467 1473 10.1016/0016-2361(90) 90192-S 1:CAS:528:DyaK3MXks1Sqtg%3D%3D
    • (1990) Fuel , vol.69 , pp. 1467-1473
    • Mohanty, S.1    Kunzru, D.2    Saraf, D.N.3
  • 15
    • 14544290213 scopus 로고    scopus 로고
    • 10.1016/j.apcata.2004.11.044 1:CAS:528:DC%2BD2MXhslehs7o%3D
    • Y Rezgui M Guemini 2005 Appl Catal A Gen 282 45 53 10.1016/j.apcata.2004. 11.044 1:CAS:528:DC%2BD2MXhslehs7o%3D
    • (2005) Appl Catal A Gen , vol.282 , pp. 45-53
    • Rezgui, Y.1    Guemini, M.2
  • 17
    • 34249775783 scopus 로고    scopus 로고
    • Gas oil hydrocracking on NiW/USY catalyst: Effect of tungsten and nickel loading
    • DOI 10.1016/j.cej.2007.01.021, PII S1385894707000381
    • AM Alsobaai R Zakaria BH Hameed 2007 Chem Eng J 132 77 83 10.1016/j.cej.2007.01.021 1:CAS:528:DC%2BD2sXmtVKhsLk%3D (Pubitemid 46844868)
    • (2007) Chemical Engineering Journal , vol.132 , Issue.1-3 , pp. 77-83
    • Alsobaai, A.M.1    Zakaria, R.2    Hameed, B.H.3
  • 19
    • 0034598493 scopus 로고    scopus 로고
    • 10.1016/S0926-860X(99)00292-6 1:CAS:528:DC%2BD3cXlsFSrug%3D%3D
    • V Calemma S Peratello C Perego 2000 Appl Catal A Gen 190 207 218 10.1016/S0926-860X(99)00292-6 1:CAS:528:DC%2BD3cXlsFSrug%3D%3D
    • (2000) Appl Catal A Gen , vol.190 , pp. 207-218
    • Calemma, V.1    Peratello, S.2    Perego, C.3
  • 23
    • 0000526672 scopus 로고
    • 10.1146/annurev.ms.15.080185.001303 1:CAS:528:DyaL2MXkvFegsrY%3D
    • LC Klein 1985 Ann Rev Mater Sci 15 227 248 10.1146/annurev.ms.15.080185. 001303 1:CAS:528:DyaL2MXkvFegsrY%3D
    • (1985) Ann Rev Mater Sci , vol.15 , pp. 227-248
    • Klein, L.C.1
  • 24
    • 0029540753 scopus 로고
    • 10.1080/07315179508204280 1:CAS:528:DyaK28XlsFKltrs%3D
    • S Wang H Liu L Zhang X Yao 1995 Ferroelectrics Lett 19 89 94 10.1080/07315179508204280 1:CAS:528:DyaK28XlsFKltrs%3D
    • (1995) Ferroelectrics Lett , vol.19 , pp. 89-94
    • Wang, S.1    Liu, H.2    Zhang, L.3    Yao, X.4
  • 25
    • 50349085627 scopus 로고    scopus 로고
    • 10.1016/j.micromeso.2008.02.032 1:CAS:528:DC%2BD1cXhtVOmu7jK
    • G Carja Y Kameshima K Okada 2008 Micropor Mesopor Mat 115 541 547 10.1016/j.micromeso.2008.02.032 1:CAS:528:DC%2BD1cXhtVOmu7jK
    • (2008) Micropor Mesopor Mat , vol.115 , pp. 541-547
    • Carja, G.1    Kameshima, Y.2    Okada, K.3
  • 26
    • 34249316550 scopus 로고    scopus 로고
    • Indium incorporated silica from rice husk and its catalytic activity
    • DOI 10.1016/j.micromeso.2007.01.055, PII S1387181107000728
    • AE Ahmed F Adam 2007 Micropor Mesopor Mat 103 284 295 10.1016/j.micromeso.2007.01.055 1:CAS:528:DC%2BD2sXmtVKht7Y%3D (Pubitemid 46810335)
    • (2007) Microporous and Mesoporous Materials , vol.103 , Issue.1-3 , pp. 284-295
    • Ahmed, A.E.1    Adam, F.2
  • 27
    • 33748687174 scopus 로고    scopus 로고
    • 2 with crystalline framework using a double surfactant system
    • DOI 10.1016/j.micromeso.2006.05.033, PII S1387181106002010
    • Q Sheng Y Cong S Yuan J Zhang M Anpo 2006 Micropor Mesopor Mat 95 220 225 10.1016/j.micromeso.2006.05.033 1:CAS:528:DC%2BD28XhtVSit7vN (Pubitemid 44397674)
    • (2006) Microporous and Mesoporous Materials , vol.95 , Issue.1-3 , pp. 220-225
    • Sheng, Q.1    Cong, Y.2    Yuan, S.3    Zhang, J.4    Anpo, M.5
  • 28
    • 36249016755 scopus 로고    scopus 로고
    • 2 unsupported catalysts prepared by hydrothermal synthesis for hydrodesulfurization of 4,6-dimethyldibenzothiophene
    • DOI 10.1016/j.cattod.2007.07.003, PII S0920586107004531, New Developments in Sulfide Catalysis: Linking Industrial Needs to Fundamental Challenges Proceedings of the 4th International Symposium on Molecular Aspects of Cataslysis by Sulfides (MACS-IV)
    • B Yoosuk JH Kim C Song C Ngamcharussrivichai P Prassassarakich 2008 Catal Today 130 14 23 10.1016/j.cattod.2007.07.003 1:CAS:528:DC%2BD2sXhtlKrtrzN (Pubitemid 350123013)
    • (2008) Catalysis Today , vol.130 , Issue.1 , pp. 14-23
    • Yoosuk, B.1    Kim, J.H.2    Song, C.3    Ngamcharussrivichai, C.4    Prasassarakich, P.5
  • 29
    • 0037504217 scopus 로고    scopus 로고
    • 10.1016/S0021-9517(02)00181-1 1:CAS:528:DC%2BD3sXjtFeitbY%3D
    • L Qu W Zhang PJ Kooyman R Prins 2003 J Catal 215 7 13 10.1016/S0021-9517(02)00181-1 1:CAS:528:DC%2BD3sXjtFeitbY%3D
    • (2003) J Catal , vol.215 , pp. 7-13
    • Qu, L.1    Zhang, W.2    Kooyman, P.J.3    Prins, R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.