Degradation of nano ZnO-glass fiber-unsaturated polyester composites

Author keywords

Composite materials; Fourier transform infrared spectroscopy (FTIR); Nano ZnO; Photo aging; Photoinitiated oxidation; Thermogravimetric analysis; Unsaturated polyester

Indexed keywords

FOURIER TRANSFORM INFRARED SPECTROSCOPY (FTIR); NANO ZNO; PHOTO AGING; PHOTOINITIATED OXIDATION; UNSATURATED POLYESTER;

EID: 69949098346     PISSN: 00218995     EISSN: 10974628     Source Type: Journal    
DOI: 10.1002/app.29988     Document Type: Article
Times cited : (10)

References (27)
  • 7
    • 69949093406 scopus 로고    scopus 로고
    • Higoal Fibreglass Manufactory. Available at Accessed 25 June
    • Higoal Fibreglass Manufactory. Available at: http://hgfrp.cn.alibaba.com/ athena/offerdetail/sale/hgfrp-1338-0869320.html. Accessed 25 June, 2007.
    • (2007)
  • 8
    • 69949099807 scopus 로고    scopus 로고
    • Yaohua-Inline Energy-Saving Dorwin Co. Ltd. Available at Accessed 25 June
    • Yaohua-Inline Energy-Saving Dorwin Co. Ltd. Available at: http://www.yaohua-glass.com/yl2.htm. Accessed 25 June, 2007.
    • (2007)
  • 9
    • 69949088109 scopus 로고    scopus 로고
    • to Toyo Metallising KK (TOYC. JP2007253463-A Accessed 4 October
    • Teranishi, M.; Okutsu, W.; Mikawa, M. (to Toyo Metallising KK (TOYC)).JP2007253463-A. Accessed 4 October, 2007
    • (2007)
    • Teranishi, M.1    Okutsu, W.2    Mikawa, M.3
  • 10
    • 69949092650 scopus 로고    scopus 로고
    • Yaohua GFRP Co Ltd. of Qinhuangdao. Available at Accessed 25 June
    • Yaohua GFRP Co. Ltd. of Qinhuangdao. Available at: www.yaohua-glass.com/ blg2.htm.Accessed 25 June, 2007.
    • (2007)


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.