메뉴 건너뛰기




Volumn 17, Issue 4, 2009, Pages 315-325

Bond strength and morphology of enamel using self-etching adhesive systems with different acidities

Author keywords

Adhesive systems; Bonding; Enamel; Morphology

Indexed keywords


EID: 69249134181     PISSN: 16787757     EISSN: 16787765     Source Type: Journal    
DOI: 10.1590/S1678-77572009000400009     Document Type: Article
Times cited : (31)

References (34)
  • 1
    • 1542389179 scopus 로고    scopus 로고
    • Ultra-morphology of self-etching adhesives on ground enamel: A high resolution SEM study
    • Breschi L, Gorbi P, Falconi M, Mazzotti G, Prati C, Perdigão J. Ultra-morphology of self-etching adhesives on ground enamel: a high resolution SEM study. Am J Dent. 2003;16:57A-62A.
    • (2003) Am J Dent , vol.16
    • Breschi, L.1    Gorbi, P.2    Falconi, M.3    Mazzotti, G.4    Prati, C.5    Perdigão, J.6
  • 2
    • 0346910233 scopus 로고    scopus 로고
    • Effects of the acetone content of single solution dentin bonding agents on the adhesive agents on the adhesive layer thickness and the microtensile bond strength
    • Cho BH, Dickers SH. Effects of the acetone content of single solution dentin bonding agents on the adhesive agents on the adhesive layer thickness and the microtensile bond strength. Dent Mater. 2004;20:107-5.
    • (2004) Dent Mater , vol.20 , pp. 107-105
    • Cho, B.H.1    Dickers, S.H.2
  • 4
    • 1842486855 scopus 로고    scopus 로고
    • Microtensile bond strengths of one- and two-step self-etch adhesives to bur-cut enamel and dentin
    • De Munck J, Van Meerbeek BV, Satoshi I, Vargas M, Yoshida Y, Armstrong S, et al. Microtensile bond strengths of one- and two-step self-etch adhesives to bur-cut enamel and dentin. Am J Dent. 2003;6:414-20.
    • (2003) Am J Dent , vol.6 , pp. 414-420
    • de Munck, J.1    van Meerbeek, B.V.2    Satoshi, I.3    Vargas, M.4    Yoshida, Y.5    Armstrong, S.6
  • 5
    • 0031082960 scopus 로고    scopus 로고
    • The use of extracted teeth for in vitro bonding studies: A review of infection control considerations
    • De Wald JP. The use of extracted teeth for in vitro bonding studies: a review of infection control considerations. Dent Mater. 1997;13:74-81.
    • (1997) Dent Mater , vol.13 , pp. 74-81
    • de Wald, J.P.1
  • 7
    • 12344274728 scopus 로고    scopus 로고
    • Effect of surface preparation on microtensile bond strength of three adhesive systems to bovine enamel
    • Dias WR, Pereira PNR, Swift EJ Jr. Effect of surface preparation on microtensile bond strength of three adhesive systems to bovine enamel. J Adhes Dent. 2004;6:279-85.
    • (2004) J Adhes Dent , vol.6 , pp. 279-285
    • Dias, W.R.1    Pereira, P.N.R.2    Swift Jr., E.J.3
  • 8
  • 9
    • 23944493184 scopus 로고    scopus 로고
    • Water concentration in self-etching primers affects their aggressiveness and bonding efficacy to dentin
    • Hiraishi N, Nishiyama N, Ikemura K, Yau JYY, King NM, Tagami J, et al. Water concentration in self-etching primers affects their aggressiveness and bonding efficacy to dentin. J Dent Res. 2005;84:653-8.
    • (2005) J Dent Res , vol.84 , pp. 653-658
    • Hiraishi, N.1    Nishiyama, N.2    Ikemura, K.3    Yau, J.Y.Y.4    King, N.M.5    Tagami, J.6
  • 10
    • 0036616555 scopus 로고    scopus 로고
    • Microtensile bond strength of self-etching adhesives to ground and unground enamel
    • Ibarra G, Vargas MA, Armstrong SR, Cobb DS. Microtensile bond strength of self-etching adhesives to ground and unground enamel. J Adhes Dent. 2002;4:115-24.
    • (2002) J Adhes Dent , vol.4 , pp. 115-124
    • Ibarra, G.1    Vargas, M.A.2    Armstrong, S.R.3    Cobb, D.S.4
  • 13
    • 0033191255 scopus 로고    scopus 로고
    • Tensile bond strength to and SEM evaluation of ground and intact enamel surfaces
    • Kanemura N, Sano H, Tagami J. Tensile bond strength to and SEM evaluation of ground and intact enamel surfaces. J Dent. 1999;27:523-30.
    • (1999) J Dent , vol.27 , pp. 523-530
    • Kanemura, N.1    Sano, H.2    Tagami, J.3
  • 14
    • 20944451075 scopus 로고    scopus 로고
    • Effect of smear layer thickness and pH of self-etching adhesive systems on bond strength and gap formation
    • Kenshima S, Reis A, Uceda-Gomez N, Tancredo LLF, Rodrigues LE Filho, Nogueira FN, et al. Effect of smear layer thickness and pH of self-etching adhesive systems on bond strength and gap formation. J Adhes Dent. 2005;7:117-26.
    • (2005) J Adhes Dent , vol.7 , pp. 117-126
    • Kenshima, S.1    Reis, A.2    Uceda-Gomez, N.3    Tancredo, L.L.F.4    Rodrigues, L.E.5
  • 17
    • 25144525768 scopus 로고    scopus 로고
    • Chemical aspects of self-etching enamel-dentin adhesives: A systematic review
    • Moszner N, Salz U, Zimmermann J. Chemical aspects of self-etching enamel-dentin adhesives: a systematic review. Dent Mater. 2005;21:895-910.
    • (2005) Dent Mater , vol.21 , pp. 895-910
    • Moszner, N.1    Salz, U.2    Zimmermann, J.3
  • 18
    • 2342579567 scopus 로고    scopus 로고
    • The pka effects of the carboxylic acid in N-methacryloxyl-omega-amino acid on the demineralization and bond strengths to the teeth
    • Nishiyama N, Suzuki K, Takahashi K, Nemoto K. The pka effects of the carboxylic acid in N-methacryloxyl-omega-amino acid on the demineralization and bond strengths to the teeth. Biomaterials. 2004;25:5441-7.
    • (2004) Biomaterials , vol.25 , pp. 5441-5447
    • Nishiyama, N.1    Suzuki, K.2    Takahashi, K.3    Nemoto, K.4
  • 21
    • 0035463789 scopus 로고    scopus 로고
    • Aggressiveness of contemporary self-etching adhesives. Part II: Etching effects on unground enamel
    • Pashley DH, Tay FR. Aggressiveness of contemporary self-etching adhesives. Part II: etching effects on unground enamel. Dent Mater. 2001;17:430-44.
    • (2001) Dent Mater , vol.17 , pp. 430-444
    • Pashley, D.H.1    Tay, F.R.2
  • 22
    • 22944473956 scopus 로고    scopus 로고
    • Enamel bond strengths of pairs of adhesives from the same manufacturer
    • Perdigão J, Gomes G, Duarte S Jr, Lopes MM. Enamel bond strengths of pairs of adhesives from the same manufacturer. Oper Dent. 2005;30:492-9.
    • (2005) Oper Dent , vol.30 , pp. 492-499
    • Perdigão, J.1    Gomes, G.2    Duarte Jr., S.3    Lopes, M.M.4
  • 24
    • 21844432201 scopus 로고    scopus 로고
    • Effect of smear layer thickness and acidity of self-etching solutions on early and long-term bond strength to dentin
    • Reis A, Grandi V, Carlotto L, Bortoli G, Patzlaff RT, Accorinte MLR, et al. Effect of smear layer thickness and acidity of self-etching solutions on early and long-term bond strength to dentin. J Dent. 2005;33:549-59.
    • (2005) J Dent , vol.33 , pp. 549-559
    • Reis, A.1    Grandi, V.2    Carlotto, L.3    Bortoli, G.4    Patzlaff, R.T.5    Accorinte, M.L.R.6
  • 25
    • 0242573333 scopus 로고    scopus 로고
    • Moisture spectrum of demineralized dentin for adhesive systems with different solvent bases
    • Reis A, Loguercio AD, Azevedo CL, Carvalho RM, Singer JM, Grande RHM. Moisture spectrum of demineralized dentin for adhesive systems with different solvent bases. J Adhes Dent. 2003;5:183-92.
    • (2003) J Adhes Dent , vol.5 , pp. 183-192
    • Reis, A.1    Loguercio, A.D.2    Azevedo, C.L.3    Carvalho, R.M.4    Singer, J.M.5    Grande6
  • 26
    • 0035514423 scopus 로고    scopus 로고
    • Adverse surface interactions between one-bottle light-cured adhesives and chemicalcured composites
    • Sanares AM, King NM, Ittagarun A, Tay FR, Pashley DH. Adverse surface interactions between one-bottle light-cured adhesives and chemicalcured composites. Dent Mater. 2001;17:542-56.
    • (2001) Dent Mater , vol.17 , pp. 542-556
    • Sanares, A.M.1    King, N.M.2    Ittagarun, A.3    Tay, F.R.4    Pashley, D.H.5
  • 28
    • 0036580064 scopus 로고    scopus 로고
    • Effects of mechanical properties of adhesive resins on bond strength to dentin
    • Takahashi A, Sato Y, Uno S, Pereira PNR, Sano H. Effects of mechanical properties of adhesive resins on bond strength to dentin. Dent Mater. 2002;18:263-8.
    • (2002) Dent Mater , vol.18 , pp. 263-268
    • Takahashi, A.1    Sato, Y.2    Uno, S.3    Pereira, P.N.R.4    Sano, H.5
  • 30
    • 0035405736 scopus 로고    scopus 로고
    • Aggressiveness of contemporary self-etching systems. I: Depth of penetration beyond dentin smear layers
    • Tay FR, Pashley DH. Aggressiveness of contemporary self-etching systems. I: depth of penetration beyond dentin smear layers. Dent Mater. 2001;17:296-308.
    • (2001) Dent Mater , vol.17 , pp. 296-308
    • Tay, F.R.1    Pashley, D.H.2
  • 31
    • 0141924427 scopus 로고    scopus 로고
    • Microtensile bond strength of an etch & rinse and self-etch adhesive to enamel and dentin as a function of surface treatment
    • Van Meerbeek B, De Munck J, Mattar D, Van Landuyt K, Lambrechts P. Microtensile bond strength of an etch & rinse and self-etch adhesive to enamel and dentin as a function of surface treatment. Oper Dent. 2003;28:647-60.
    • (2003) Oper Dent , vol.28 , pp. 647-660
    • van Meerbeek, B.1    de Munck, J.2    Mattar, D.3    van Landuyt, K.4    Lambrechts5
  • 32
    • 17844399811 scopus 로고    scopus 로고
    • A randomized controlled study evaluating the effectiveness of a two-step self-etch adhesive with and without selective phosphoric-acid etching of enamel
    • Van Meerbeek B, Kanumilli P, De Munck J, Landuyt KV, Lambrechts P, Peumans M. A randomized controlled study evaluating the effectiveness of a two-step self-etch adhesive with and without selective phosphoric-acid etching of enamel. Dent Mater. 2005;21:375-83.
    • (2005) Dent Mater , vol.21 , pp. 375-383
    • van Meerbeek, B.1    Kanumilli, P.2    de Munck, J.3    Landuyt, K.V.4    Lambrechts, P.5    Peumans, M.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.