Volumn 3, Issue 1, 2009, Pages 25-38

On the development of hybrid material concepts for aircraft structures

Author keywords

Aircraft structures; Fibre metal laminates; Hybrid technology; Manufacturing

Indexed keywords

AIRCRAFT STRUCTURE; AIRCRAFT STRUCTURES; FIBRE METAL LAMINATES; FIBRE REINFORCED POLYMERS; HYBRID TECHNOLOGY; MANUFACTURING;

EID: 68349141225     PISSN: 18722121     EISSN: None     Source Type: Journal    
DOI: 10.2174/187221209787259893     Document Type: Article
Times cited : (68)

References (62)
  • 2
    • 0009339803 scopus 로고    scopus 로고
    • Vlot A, Gunnink JW. (Eds.), Kluwer Academic Publishers, Dordrecht, The Netherlands
    • Vlot A, Gunnink JW. (Eds.), Fibre metal laminates, an introduction, Kluwer Academic Publishers, Dordrecht, The Netherlands, 2001.
    • (2001) Fibre Metal Laminates, An Introduction
  • 5
    • 0029755468 scopus 로고    scopus 로고
    • Fatigue delamination growth in carbon fibre-reinforced aluminium laminates
    • Lin CT, Kao PW. Fatigue delamination growth in carbon fibre-reinforced aluminium laminates. Composites Part A 1996; 21A: 9-15.
    • (1996) Composites Part A , vol.21 A , pp. 9-15
    • Lin, C.T.1    Kao, P.W.2
  • 6
    • 0031647570 scopus 로고    scopus 로고
    • An investigation into the fatigue of a hybrid titanium composite laminate
    • Li E, Johnson WS. An investigation into the fatigue of a hybrid titanium composite laminate. J Compos Technol Res 1998; 20 (1):3-12.
    • (1998) J Compos Technol Res , vol.20 , Issue.1 , pp. 3-12
    • Li, E.1    Johnson, W.S.2
  • 9
    • 68349126393 scopus 로고    scopus 로고
    • TUDelft.: NL8100087 (1981)
    • TUDelft.: NL8100087 (1981).
  • 10
    • 68349126391 scopus 로고    scopus 로고
    • TUDelft.: NL8100088 (1981)
    • TUDelft.: NL8100088 (1981).
  • 14
    • 68349151787 scopus 로고
    • US4935291
    • Gunnink, J.W.: US4935291 (1990).
    • (1990)
    • Gunnink, J.W.1
  • 24
    • 68349132657 scopus 로고    scopus 로고
    • US5567535
    • Pettit, R.G.: US5567535 (1996).
    • (1996)
    • Pettit, R.G.1
  • 31
    • 68349130747 scopus 로고    scopus 로고
    • WO03011594A1
    • Rajabali, A.F.: WO03011594A1 (2003).
    • (2003)
    • Rajabali, A.F.1
  • 32
    • 68349159899 scopus 로고    scopus 로고
    • US7223318B2
    • Rajabali, A.F.: US7223318B2 (2007).
    • (2007)
    • Rajabali, A.F.1
  • 42
    • 21244487797 scopus 로고    scopus 로고
    • Formability
    • In: Vlot, A., Gunnink, J.W. (Eds.), Kluwer Academic Publishers, Dordrecht, The Netherlands
    • De Jong, T.W., Kroon, E., Sinke, J., Formability, In: Vlot, A., Gunnink, J.W. (Eds.), Fibre Metal Laminates - An introduction, Kluwer Academic Publishers, Dordrecht, The Netherlands, 2001.
    • (2001) Fibre Metal Laminates - An Introduction
    • de Jong, T.W.1    Kroon, E.2    Sinke, J.3
  • 44
    • 68349132660 scopus 로고    scopus 로고
    • WO08053041A1
    • Beumler, Th.: WO08053041A1 (2008).
    • (2008)
    • Beumler, T.1
  • 49
    • 68349159898 scopus 로고
    • US4359567
    • Evers, R.C.: US4359567 (1982).
    • (1982)
    • Evers, R.C.1
  • 51
    • 0031648859 scopus 로고    scopus 로고
    • Morphological study on poly-p-phenylene-benzobisoxazole (PBO) fiber
    • Kitagawa T, Murase H, Yabuki K. Morphological study on poly-p-phenylene-benzobisoxazole (PBO) fiber. J Polym Sci Part B Polym Phys 1998; 36: 39-48.
    • (1998) J Polym Sci Part B Polym Phys , vol.36 , pp. 39-48
    • Kitagawa, T.1    Murase, H.2    Yabuki, K.3
  • 52
    • 84870979227 scopus 로고    scopus 로고
    • Technical Information
    • Zylon® (PBO fiber), Tyobo Co., LTD
    • Zylon® (PBO fiber) Technical Information (2005), Tyobo Co., LTD. www.toyobo.co.jp/e/seihin/kc/pbo/Technical_Information_2005. pdf
    • (2005)
  • 56
    • 0022241748 scopus 로고
    • Matrix deformation and fracture in graphite-reinforced epoxies
    • Bradley WL, Cohen RN. Matrix deformation and fracture in graphite-reinforced epoxies, ASTM STP 1985; 876: 389-410.
    • (1985) ASTM STP , vol.876 , pp. 389-410
    • Bradley, W.L.1    Cohen, R.N.2
  • 57
    • 0023564904 scopus 로고
    • Matrix resin effects in composite delamination: Mode I fracture aspects
    • Hunston DL, Moulton RJ, Johnston JJ, Bascom WD. Matrix resin effects in composite delamination: mode I fracture aspects, ASTM STP 1987; 937: 74-94.
    • (1987) ASTM STP , vol.937 , pp. 74-94
    • Hunston, D.L.1    Moulton, R.J.2    Johnston, J.J.3    Bascom, W.D.4
  • 58
    • 0029407314 scopus 로고
    • Low velocity impact fatigue studies on glass epoxy composite laminates with varied material and test parameters -effect of incident energy and fibre volume fraction
    • Khan B, Rao RMVGK, Venkataraman N. Low velocity impact fatigue studies on glass epoxy composite laminates with varied material and test parameters -effect of incident energy and fibre volume fraction. J Reinforced Plast Compos 1995; 14:1150-1159.
    • (1995) J Reinforced Plast Compos , vol.14 , pp. 1150-1159
    • Khan, B.1    Rao, R.M.V.G.K.2    Venkataraman, N.3
  • 59
    • 2342429440 scopus 로고    scopus 로고
    • Influence of fiber volume fraction on mode III Interlaminar fracture toughness of glass/epoxy composites
    • Li X, Carlsson LA, Davies P. Influence of fiber volume fraction on mode III Interlaminar fracture toughness of glass/epoxy composites. Compos Sci Technol 2004; 64: 1279-1286.
    • (2004) Compos Sci Technol , vol.64 , pp. 1279-1286
    • Li, X.1    Carlsson, L.A.2    Davies, P.3
  • 60
    • 68349132656 scopus 로고    scopus 로고
    • WO9720647
    • Kingston, W.R.: WO9720647 (1997).
    • (1997)
    • Kingston, W.R.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.