Nucleation and growth mechanism of apatite on a bioactive and degradable ceramic/polymer composite with a thick polymer layer
|
Author keywords
[No Author keywords available]
|
Indexed keywords
ACIDIC CONDITIONS;
APATITE COATING;
APATITE FORMING;
BIOACTIVE CERAMIC;
BONE GRAFTING MATERIALS;
CALCIUM NITRATE TETRA-HYDRATE;
CASTING PROCESS;
CERAMIC/POLYMER COMPOSITES;
CUTTING PROCESS;
DEGRADABILITY;
NUCLEATION AND GROWTH;
PLLA;
POLYMER LAYERS;
SOL-GEL METHODS;
SOLVENT CASTING METHOD;
SURFACE GRINDING;
SURFACE LAYERS;
TETRA-ETHYL-ORTHO-SILICATE;
APATITE;
BIODEGRADABLE POLYMERS;
CALCIUM;
GELATION;
NUCLEATION;
PHOSPHATE MINERALS;
SILICON COMPOUNDS;
SOL-GEL PROCESS;
SURFACES;
|