Optical emission spectroscopy during plasmatron testing of ZrB 2-SiC Ultrahigh-temperature ceramic composites

Author keywords

[No Author keywords available]

Indexed keywords

CERAMIC MATERIALS; GAS DISCHARGE TUBES; LIGHT EMISSION; SCALE (DEPOSITS); SILICA; SILICON CARBIDE; ZIRCONIUM COMPOUNDS;

EID: 67650797093     PISSN: 08878722     EISSN: 15336808     Source Type: Journal    
DOI: 10.2514/1.39974     Document Type: Article
Times cited : (25)

References (36)
  • 1
    • 43349100719 scopus 로고    scopus 로고
    • Topical Issue on Ultra-High-Temperature Ceramics
    • doi:10.1111/j.1551-2916.2008. 02481.x
    • Fuller, J., Blum, Y., and Marschall, J., "Topical Issue on Ultra-High-Temperature Ceramics," Journal of the American Ceramic Society, Vol. 91, No. 5, 2008, pp. 1397-1502. doi:10.1111/j.1551-2916.2008. 02481.x
    • (2008) Journal of the American Ceramic Society , vol.91 , Issue.5 , pp. 1397-1502
    • Fuller, J.1    Blum, Y.2    Marschall, J.3
  • 2
    • 67650998604 scopus 로고    scopus 로고
    • Fuller, J., and Sacks, M., Special Section: Ultra-High Temperature Ceramics, Journal of Materials Science, 39, No. 19, 2004, pp. 5885-6066. doi:10.1023/B:JMSC.0000041685.85043.34
    • Fuller, J., and Sacks, M., "Special Section: Ultra-High Temperature Ceramics," Journal of Materials Science, Vol. 39, No. 19, 2004, pp. 5885-6066. doi:10.1023/B:JMSC.0000041685.85043.34
  • 3
    • 34248350351 scopus 로고    scopus 로고
    • Refractory Diborides of Zirconium and Hafnium
    • doi:10.1111/j.1551-2916.2007.01583.x
    • Fahrenholtz, W. G., Hilmas, G. E., Talmy, I. G., and Zaykoski, J. A., "Refractory Diborides of Zirconium and Hafnium," Journal of the American Ceramic Society, Vol. 90, No. 5, 2007, pp. 1347-1364. doi:10.1111/j.1551-2916.2007.01583.x
    • (2007) Journal of the American Ceramic Society , vol.90 , Issue.5 , pp. 1347-1364
    • Fahrenholtz, W.G.1    Hilmas, G.E.2    Talmy, I.G.3    Zaykoski, J.A.4
  • 4
    • 43349086037 scopus 로고    scopus 로고
    • Thermal Conductivity Characterization of Hafnium Diboride-Based Ultra High Temperature Ceramics
    • doi:10.1111/j.1551-2916.2008.02364.x
    • Gasch, M., Johnson, S., and Marschall, J., "Thermal Conductivity Characterization of Hafnium Diboride-Based Ultra High Temperature Ceramics," Journal of the American Ceramic Society, Vol. 91, No. 5, 2008, pp. 1423-1432. doi:10.1111/j.1551-2916.2008.02364.x
    • (2008) Journal of the American Ceramic Society , vol.91 , Issue.5 , pp. 1423-1432
    • Gasch, M.1    Johnson, S.2    Marschall, J.3
  • 6
    • 4344596443 scopus 로고
    • Oxidation of Boron at Temperatures Between 400 and 1300 °C in Air
    • edited by J. A. Kohn, and W. F. Nye, Plenum, New York
    • Rizzo, H. F., "Oxidation of Boron at Temperatures Between 400 and 1300 °C in Air," Boron-Synthesis, Structure, and Properties, edited by J. A. Kohn, and W. F. Nye, Plenum, New York, 1968, pp. 175-189.
    • (1968) Boron-Synthesis, Structure, and Properties , pp. 175-189
    • Rizzo, H.F.1
  • 7
    • 67650999596 scopus 로고    scopus 로고
    • Roine, A, HSC Chemistry for Windows, Ver. 5.11, Outokumpu Research Oy, Pori, Finland, 2006
    • Roine, A., HSC Chemistry for Windows, Ver. 5.11, Outokumpu Research Oy, Pori, Finland, 2006.
  • 8
    • 84963784490 scopus 로고
    • 2 in the Temperature Range of 800 to 1500 C
    • doi:10.1149/1.2408279
    • 2 in the Temperature Range of 800 to 1500 C," Journal of the Electrochemical Society, Vol. 118, No. 7, 1971, pp. 1195-1199. doi:10.1149/1.2408279
    • (1971) Journal of the Electrochemical Society , vol.118 , Issue.7 , pp. 1195-1199
    • Tripp, W.C.1    Graham, H.C.2
  • 9
    • 84975353152 scopus 로고
    • The Oxidation Kinetics of Zirconium Diboride and Zirconium Carbide at High Temperatures
    • doi:10.1149/1.2426263
    • Kuriakose, A. K., and Margrave, J. L., "The Oxidation Kinetics of Zirconium Diboride and Zirconium Carbide at High Temperatures," Journal of the Electrochemical Society, Vol. 111, No. 7, 1964, pp. 827-831. doi:10.1149/1.2426263
    • (1964) Journal of the Electrochemical Society , vol.111 , Issue.7 , pp. 827-831
    • Kuriakose, A.K.1    Margrave, J.L.2
  • 10
    • 84943821266 scopus 로고
    • High-Temperature Oxidation III. Zirconium and Hafnium Diborides
    • doi:10.1149/1.2424154
    • Berkowitz-Mattuck, J. B., "High-Temperature Oxidation III. Zirconium and Hafnium Diborides," Journal of the Electrochemical Society, Vol. 113, 1966, pp. 908-914. doi:10.1149/1.2424154
    • (1966) Journal of the Electrochemical Society , vol.113 , pp. 908-914
    • Berkowitz-Mattuck, J.B.1
  • 13
    • 34748899460 scopus 로고    scopus 로고
    • 2-SiC Ceramics Under Simulated Atmospheric Re-Entry Conditions
    • doi:10.1016/j.jeurceramsoc.2007.02.201
    • 2-SiC Ceramics Under Simulated Atmospheric Re-Entry Conditions," Journal of the European Ceramic Society, Vol. 27, 2007, pp. 4797-4805. doi:10.1016/j.jeurceramsoc.2007.02.201
    • (2007) Journal of the European Ceramic Society , vol.27 , pp. 4797-4805
    • Monteverde, F.1    Savino, R.2
  • 14
    • 0033323434 scopus 로고    scopus 로고
    • Mechanical, Thermal, and Oxidation Properties of Refractory Hafnium and Zirconium Compounds
    • doi:10.1016/S0955-2219(99)00129-6
    • Opeka, M. M., Talmy, I. G., Wuchina, E. J., Zaykoski, J. A., and Causey, S. J., "Mechanical, Thermal, and Oxidation Properties of Refractory Hafnium and Zirconium Compounds," Journal of the European Ceramic Society, Vol. 19, 1999, pp. 2405-2414. doi:10.1016/S0955-2219(99)00129-6
    • (1999) Journal of the European Ceramic Society , vol.19 , pp. 2405-2414
    • Opeka, M.M.1    Talmy, I.G.2    Wuchina, E.J.3    Zaykoski, J.A.4    Causey, S.J.5
  • 15
    • 4344691574 scopus 로고
    • The Influence of SiC on the Ablation Response of Advanced Refractory Composite Materials
    • Advanced Materials Processes and Technology Information Analysis Center, Rome, NY
    • Bull, J., "The Influence of SiC on the Ablation Response of Advanced Refractory Composite Materials,"19th Conference on Composite Materials and Structures, Pt. 1, Advanced Materials Processes and Technology Information Analysis Center, Rome, NY, 1995, pp. 157-181.
    • (1995) 19th Conference on Composite Materials and Structures , Issue.PART. 1 , pp. 157-181
    • Bull, J.1
  • 16
    • 33846188476 scopus 로고    scopus 로고
    • 2-SiC Oxidation: Formation of a SiC-Depleted Region
    • doi:10.1111/j.1551-2916. 2006.01329.x
    • 2-SiC Oxidation: Formation of a SiC-Depleted Region," Journal of the American Ceramic Society, Vol. 90, No. 1, 2007, pp. 143-148. doi:10.1111/j.1551-2916. 2006.01329.x
    • (2007) Journal of the American Ceramic Society , vol.90 , Issue.1 , pp. 143-148
    • Fahrenholtz, W.G.1
  • 17
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of Structure During the Oxidation of Zirconium Diboride-Silicon Carbide in Air up to 1500 °C
    • doi:10.1016/j.jeurceramsoc.2006.10.012
    • Rezaie, A., Fahrenholtz, W. G., and Hilmas, G. E., "Evolution of Structure During the Oxidation of Zirconium Diboride-Silicon Carbide in Air up to 1500 °C," Journal of the European Ceramic Society, Vol. 27, 2007, pp. 2495-2501. doi:10.1016/j.jeurceramsoc.2006.10.012
    • (2007) Journal of the European Ceramic Society , vol.27 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 18
    • 14744305833 scopus 로고    scopus 로고
    • 2-SiC Composite, Journal of the European Ceramic Society, 25, May 2005, pp. 1025-1031.doi:10.1016/j.jeurceramsoc.2004. 05.009
    • 2-SiC Composite," Journal of the European Ceramic Society, Vol. 25, May 2005, pp. 1025-1031.doi:10.1016/j.jeurceramsoc.2004. 05.009
  • 19
    • 34247200063 scopus 로고    scopus 로고
    • Resistance to Thermal Shock and to Oxidation of Metal Diborides-SiC Ceramics for Aerospace Application
    • doi:10.1111/j.1551-2916.2007.01589.x
    • Monteverde, F., and Scatteia, L., "Resistance to Thermal Shock and to Oxidation of Metal Diborides-SiC Ceramics for Aerospace Application," Journal of the American Ceramic Society, Vol. 90, No. 4, 2007, pp. 1130-1138. doi:10.1111/j.1551-2916.2007.01589.x
    • (2007) Journal of the American Ceramic Society , vol.90 , Issue.4 , pp. 1130-1138
    • Monteverde, F.1    Scatteia, L.2
  • 20
    • 4544273437 scopus 로고    scopus 로고
    • Processing, Properties and Arc Jet Oxidation of Hafnium Diboride/Silicon Carbide Ultra High Temperature Ceramics
    • doi:10.1023/B:JMSC.0000041689.90456.af
    • Gasch, M., Ellerby, D., Irby, E., Beckman, S., Gusman, M., and Johnson, S., "Processing, Properties and Arc Jet Oxidation of Hafnium Diboride/Silicon Carbide Ultra High Temperature Ceramics," Journal of Materials Science, Vol. 39, No. 19, 2004, pp. 5925-5937. doi:10.1023/B:JMSC.0000041689.90456.af
    • (2004) Journal of Materials Science , vol.39 , Issue.19 , pp. 5925-5937
    • Gasch, M.1    Ellerby, D.2    Irby, E.3    Beckman, S.4    Gusman, M.5    Johnson, S.6
  • 21
    • 4544330453 scopus 로고    scopus 로고
    • Opeka, M. M., Talmy, I. G., and Zaykoski, J. A., Oxidation-Based Materials Selection for 2000°C+ Hypersonic Aerosurfaces: Theoretical Considerations and Historical Experience, Journal of Materials Science, 39, No. 19, 2004, pp. 5887-5904. doi:10.1023/B:JMSC. 0000041686.21788.77
    • Opeka, M. M., Talmy, I. G., and Zaykoski, J. A., "Oxidation-Based Materials Selection for 2000°C+ Hypersonic Aerosurfaces: Theoretical Considerations and Historical Experience," Journal of Materials Science, Vol. 39, No. 19, 2004, pp. 5887-5904. doi:10.1023/B:JMSC. 0000041686.21788.77
  • 22
    • 33745299257 scopus 로고    scopus 로고
    • 2 Volatility Diagram
    • doi:10.1111/j.1551-2916.2005.00599.x
    • 2 Volatility Diagram," Journal of the American Ceramic Society, Vol. 88, No. 12, 2005, pp. 3509-3512. doi:10.1111/j.1551-2916.2005.00599.x
    • (2005) Journal of the American Ceramic Society , vol.88 , Issue.12 , pp. 3509-3512
    • Fahrenholtz, W.G.1
  • 24
    • 84964010176 scopus 로고    scopus 로고
    • Aerothermodynamic Design of an Inductively Coupled Plasma Wind Tunnel
    • AIAA Paper 1997-2498, June
    • Bottin, B., Carbonaro, M., Zemsch, S., and Degrez, G., "Aerothermodynamic Design of an Inductively Coupled Plasma Wind Tunnel," AIAA Paper 1997-2498, June 1997.
    • (1997)
    • Bottin, B.1    Carbonaro, M.2    Zemsch, S.3    Degrez, G.4
  • 25
    • 84963995287 scopus 로고    scopus 로고
    • Experimental and Computational Determination of the VKI Plasmatron Operating Envelope
    • AIAA Paper 1999-3607, June
    • Bottin, B., Paris, S., Van Der Haegen, V., and Carbonaro, M., "Experimental and Computational Determination of the VKI Plasmatron Operating Envelope," AIAA Paper 1999-3607, June 1999.
    • (1999)
    • Bottin, B.1    Paris, S.2    Van Der Haegen, V.3    Carbonaro, M.4
  • 27
    • 84915826309 scopus 로고    scopus 로고
    • Effect of Water Vapor on Ignition and Combustion of Boron Lumps in an Oxygen Stream
    • Yoshida, T., and Yuasa, S., "Effect of Water Vapor on Ignition and Combustion of Boron Lumps in an Oxygen Stream," Proceedings of the Combustion Institute, Vol. 28, 2000, pp. 2735-2741.
    • (2000) Proceedings of the Combustion Institute , vol.28 , pp. 2735-2741
    • Yoshida, T.1    Yuasa, S.2
  • 28
    • 0026009959 scopus 로고
    • Ignition and Combustion of Small Boron Lumps in an Oxygen Stream
    • doi:10.1016/0010-2180(91)90101-G
    • Yuasa, S., and Isoda, H., "Ignition and Combustion of Small Boron Lumps in an Oxygen Stream," Combustion and Flame, Vol. 86, 1991, pp. 216-222. doi:10.1016/0010-2180(91)90101-G
    • (1991) Combustion and Flame , vol.86 , pp. 216-222
    • Yuasa, S.1    Isoda, H.2
  • 29
    • 0010512389 scopus 로고    scopus 로고
    • Effects of Pressure and Oxygen Concentration on Ignition and Combustion of Boron in Oxygen/Nitrogen Mixture Streams
    • doi:10.1016/S0010-2180(97)00225-3
    • Yuasa, S., Yoshida, T., Kawashima, M., and Isoda, H., "Effects of Pressure and Oxygen Concentration on Ignition and Combustion of Boron in Oxygen/Nitrogen Mixture Streams," Combustion and Flame, Vol. 113, 1998, pp. 380-387. doi:10.1016/S0010-2180(97)00225-3
    • (1998) Combustion and Flame , vol.113 , pp. 380-387
    • Yuasa, S.1    Yoshida, T.2    Kawashima, M.3    Isoda, H.4
  • 30
  • 32
    • 0011638514 scopus 로고
    • +) Visible Band System of Boron Monoxide, BO
    • doi:10.1016/0022-2852(84) 90234-0
    • +) Visible Band System of Boron Monoxide, BO," Journal of Molecular Spectroscopy, Vol. 105, No. 2, 1984, pp. 465-479. doi:10.1016/0022-2852(84) 90234-0
    • (1984) Journal of Molecular Spectroscopy , vol.105 , Issue.2 , pp. 465-479
    • Coxon, J.A.1    Foster, S.C.2    Naxakis, S.3
  • 36
    • 43349096984 scopus 로고    scopus 로고
    • 2 as Protective Coatings for Ultrahigh Temperature Ceramics
    • doi:10.1111/j.1551-2916.2008.02286.x
    • 2 as Protective Coatings for Ultrahigh Temperature Ceramics," Journal of the American Ceramic Society, Vol. 91, No. 5, 2008, pp. 1448-1452. doi:10.1111/j.1551-2916.2008.02286.x
    • (2008) Journal of the American Ceramic Society , vol.91 , Issue.5 , pp. 1448-1452
    • Bronson, A.1    Chessa, J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.