Degradation of mechanical strength of pyrolysis furnace tubes by high-temperature carburization in a petrochemical plant

Author keywords

Carburization; Heat resistant steel; Intergranular failure; Pyrolysis furnace tubes

Indexed keywords

CARBURIZATION; EXPECTED LIFE; HEAT-RESISTANT STEEL; HIGH TEMPERATURE CARBURIZATION; INTERGRANULAR CARBIDES; INTERGRANULAR FAILURE; INTERGRANULAR MODES; INWARD DIFFUSION; LONGITUDINAL CRACKS; MATRIX; MECHANICAL STRENGTH; MICROSTRUCTURAL ANALYSIS; PROTECTIVE OXIDES; PYROLYSIS FURNACE; PYROLYSIS FURNACE TUBES; SIGMA PHASE;

EID: 67649625172     PISSN: 13506307     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.engfailanal.2009.02.009     Document Type: Article
Times cited : (36)

References (7)
  • 3
    • 17444362756 scopus 로고
    • Norton JF, editor, Luxembourg: Commission of the European Communities;, Publication no. EUR 7773
    • Blackburn J. In: Norton JF, editor. Carburization in high temperature process plant materials. Luxembourg: Commission of the European Communities; 1981. p. 7 [Publication no. EUR 7773].
    • (1981) Carburization in high temperature process plant materials , pp. 7
    • Blackburn, J.1
  • 4
    • 67649607961 scopus 로고
    • Norton JF, editor, Luxembourg: Commission of the European Communities;, Publication no. EUR 7773
    • Norton JF, In: Norton JF, editor. Carburization in high temperature process plant materials. Luxembourg: Commission of the European Communities; 1981. p. 43 [Publication no. EUR 7773].
    • (1981) Carburization in high temperature process plant materials , pp. 43
    • Norton, J.F.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.