Determination of the average nucleation undercooling of primary Al-phase on refining particles from Al-5.0 wt% Ti-1.0 wt% B in Al-based alloys using DSC

Author keywords

Aluminum alloys; Columnar to equiaxed transition; DSC; Grain refining; Nucleation undercooling; Si poisoning

Indexed keywords

AL-BASED ALLOYS; COLUMNAR GRAINS; COLUMNAR TO EQUIAXED TRANSITION; CRITICAL VALUES; DSC; EQUIAXED GRAINS; EQUIAXED GROWTHS; GRAIN REFINING; MAIN PARAMETERS; NI ALLOYS; PARTICLE DENSITIES; POISONING EFFECTS; QUANTITATIVE PREDICTIONS; SI POISONING;

EID: 67349269499     PISSN: 09258388     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jallcom.2008.10.109     Document Type: Article
Times cited : (28)

References (13)
  • 10
    • 0004194076 scopus 로고
    • La calorimétrie différentielle à balayage, The Perkin Elmer Corporation, Reprinted from: IRS
    • Butterworths, London 10
    • J.L. NcNaughton, C.T. Mortimer, La calorimétrie différentielle à balayage, The Perkin Elmer Corporation, Reprinted from: IRS; Physical Chemistry Series 2 (Butterworths, London) 10, 1975.
    • (1975) Physical Chemistry Series , vol.2
    • NcNaughton, J.L.1    Mortimer, C.T.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.