Surface modification of a low-modulus Ti-7.5Mo alloy treated with aqueous NaOH

Author keywords

Alkali treatment; Scanning electron microscopy (SEM); Simulated body fluid (SBF); Titanium alloy; X ray diffraction (XRD)

Indexed keywords

ALKALI TREATMENT; AQUEOUS SOLUTIONS; ARTIFICIAL BONES; BIOACTIVE COATINGS; BIOMEDICAL APPLICATIONS; CHEMICAL TECHNIQUES; COMMERCIALLY PURE TITANIUMS; EXCELLENT CORROSION RESISTANCES; FORMING ABILITY; HARD TISSUE REPLACEMENT; HEAVY LOADS; LIVING BONE; LOW ELASTIC MODULUS; LOW-MODULUS; NAOH CONCENTRATION; NAOH SOLUTIONS; POROUS NETWORK STRUCTURES; PROCESSING COSTS; SIMULATED BODY FLUID (SBF); SIMULATED BODY FLUIDS; SODIUM TITANATES; SURFACE MODIFICATION; X-RAY DIFFRACTION (XRD); XRD;