메뉴 건너뛰기




Volumn 27, Issue 4, 2009, Pages 747-753

Oxidation behavior and mechanical properties degradation of hot-pressed Al2O3/ZrB2/ZrO2 ceramic composites

Author keywords

Alumina; Composites; Oxidation; Zirconium diboride

Indexed keywords

CERAMIC COMPOSITES; COMPOSITES; HIGH-TEMPERATURE OXIDATION BEHAVIORS; OXIDATION BEHAVIORS; OXIDATION TESTS; OXIDATION TIME; OXIDATION VELOCITIES; OXIDATION-KINETICS; XRD ANALYSIS; ZIRCONIUM DIBORIDE;

EID: 64049118904     PISSN: 02634368     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijrmhm.2008.12.006     Document Type: Article
Times cited : (37)

References (28)
  • 2
    • 14744298412 scopus 로고    scopus 로고
    • 2 ceramic tools in dry high-speed machining of hardened steel
    • 2 ceramic tools in dry high-speed machining of hardened steel. J Eur Ceram Soc 25 7 (2005) 1073-1079
    • (2005) J Eur Ceram Soc , vol.25 , Issue.7 , pp. 1073-1079
    • Deng, J.X.1    Cao, T.K.2    Liu, L.L.3
  • 4
    • 0035421104 scopus 로고    scopus 로고
    • The influence of addition of WC particles on mechanical properties of alumina-matrix composite
    • Wang L., Shi J.L., Hua Z.L., Gao J.H., and Yan D.S. The influence of addition of WC particles on mechanical properties of alumina-matrix composite. Mater Lett 50 2-3 (2001) 179-182
    • (2001) Mater Lett , vol.50 , Issue.2-3 , pp. 179-182
    • Wang, L.1    Shi, J.L.2    Hua, Z.L.3    Gao, J.H.4    Yan, D.S.5
  • 6
    • 0036833024 scopus 로고    scopus 로고
    • 3-5 vol.% Cr nanocomposites
    • 3-5 vol.% Cr nanocomposites. J Eur Ceram Soc 22 12 (2002) 1927-1936
    • (2002) J Eur Ceram Soc , vol.22 , Issue.12 , pp. 1927-1936
    • Ji, Y.1    Yeomans, J.A.2
  • 8
    • 0029732469 scopus 로고    scopus 로고
    • 2 influence of a mechano-chemical treatment on the borothermic reduction of titania and zirconia
    • 2 influence of a mechano-chemical treatment on the borothermic reduction of titania and zirconia. J Mater Sci 31 2 (1996) 351-355
    • (1996) J Mater Sci , vol.31 , Issue.2 , pp. 351-355
    • Millet, P.1    Hwang, T.2
  • 12
    • 33748936677 scopus 로고    scopus 로고
    • Oxidation of zirconium diboride-silicon carbide at 1500 °C at a low partial pressure of oxygen
    • Rezaie A., Fahrenholtz W.G., and Hilmas G.E. Oxidation of zirconium diboride-silicon carbide at 1500 °C at a low partial pressure of oxygen. J Am Ceram Soc 89 10 (2006) 3240-3245
    • (2006) J Am Ceram Soc , vol.89 , Issue.10 , pp. 3240-3245
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 13
    • 9444293406 scopus 로고    scopus 로고
    • Fracture resistance behavior of alumina-zirconia composites[J]
    • Szutkowska M. Fracture resistance behavior of alumina-zirconia composites[J]. J Mater Process Technol 153-154 (2004) 868-874
    • (2004) J Mater Process Technol , vol.153-154 , pp. 868-874
    • Szutkowska, M.1
  • 14
    • 0037308603 scopus 로고    scopus 로고
    • Alumina ceramics with partially stabilized zirconia for cutting tools[J]
    • Smuk B., Szutkowska M., and Walter J. Alumina ceramics with partially stabilized zirconia for cutting tools[J]. J Mater Process Technol 133 1-2 (2003) 195-198
    • (2003) J Mater Process Technol , vol.133 , Issue.1-2 , pp. 195-198
    • Smuk, B.1    Szutkowska, M.2    Walter, J.3
  • 15
    • 64049087235 scopus 로고    scopus 로고
    • 10.1016/j.jallcom.2008.05.05
    • Li B., and Deng J. J Alloys Compd (2008) 10.1016/j.jallcom.2008.05.05
    • (2008) J Alloys Compd
    • Li, B.1    Deng, J.2
  • 16
    • 0031276321 scopus 로고    scopus 로고
    • Wear behavior and mechanisms of alumina-based ceramic tools in machining of ferrous and non-ferrous alloys
    • Deng J.X., and Ai X. Wear behavior and mechanisms of alumina-based ceramic tools in machining of ferrous and non-ferrous alloys. Tribol Int 30 11 (1997) 807-813
    • (1997) Tribol Int , vol.30 , Issue.11 , pp. 807-813
    • Deng, J.X.1    Ai, X.2
  • 17
    • 34748844079 scopus 로고    scopus 로고
    • Wear measurements of self-lubricating bearing materials in small oscillatory movement
    • Gawarkiewicz R., and Wasilczuk M. Wear measurements of self-lubricating bearing materials in small oscillatory movement. Wear 263 1-6 (2007) 458-462
    • (2007) Wear , vol.263 , Issue.1-6 , pp. 458-462
    • Gawarkiewicz, R.1    Wasilczuk, M.2
  • 18
    • 0033323434 scopus 로고    scopus 로고
    • Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds
    • Opeka M.M., Talmy I.G., Wuchina E.J., Zaykoski J.A., and Causey S.J. Mechanical, thermal, and oxidation properties of refractory hafnium and zirconium compounds. J Eur Ceram Soc 19 13-14 (1999) 2405-2414
    • (1999) J Eur Ceram Soc , vol.19 , Issue.13-14 , pp. 2405-2414
    • Opeka, M.M.1    Talmy, I.G.2    Wuchina, E.J.3    Zaykoski, J.A.4    Causey, S.J.5
  • 21
    • 0003414401 scopus 로고    scopus 로고
    • Estimated viscosities and thermal conductivities of gases at high temperatures
    • R-132; 1962
    • Svehla R. Estimated viscosities and thermal conductivities of gases at high temperatures. NASA Tech Report R-132; 1962.
    • NASA Tech Report
    • Svehla, R.1
  • 22
    • 0023827489 scopus 로고
    • Oxidation of carbon/carbon composites - a theoretical analysis
    • Luthra K.L. Oxidation of carbon/carbon composites - a theoretical analysis. Carbon 26 2 (1988) 217-224
    • (1988) Carbon , vol.26 , Issue.2 , pp. 217-224
    • Luthra, K.L.1
  • 25
    • 5244338595 scopus 로고
    • Oxidation behavior of sic-whisker-reinforced alumina-zirconia composites
    • Backhaus-Ricoult M. Oxidation behavior of sic-whisker-reinforced alumina-zirconia composites. J Am Ceram Soc 74 8 (1991) 1793-1802
    • (1991) J Am Ceram Soc , vol.74 , Issue.8 , pp. 1793-1802
    • Backhaus-Ricoult, M.1
  • 26
    • 0025414938 scopus 로고
    • Oxidation of silicon carbide-reinforced oxide-matrix composites at 1375 °C to 1575 °C
    • Luthra K.L., and Park H.D. Oxidation of silicon carbide-reinforced oxide-matrix composites at 1375 °C to 1575 °C. J Am Ceram Soc 73 4 (1990) 1014-1023
    • (1990) J Am Ceram Soc , vol.73 , Issue.4 , pp. 1014-1023
    • Luthra, K.L.1    Park, H.D.2
  • 27
    • 0026120612 scopus 로고
    • Tribological properties of boric acid and boric-acid-forming surfaces. Part II. Mechanisms of formation and self-lubrication of boric acid films on boron and boric oxide-containing surfaces.
    • Erdemir A., Fenske G.R., Erck R.A., Nichols F.A., and Busch D.E. Tribological properties of boric acid and boric-acid-forming surfaces. Part II. Mechanisms of formation and self-lubrication of boric acid films on boron and boric oxide-containing surfaces. Lubr Eng 47 3 (1991) 179-184
    • (1991) Lubr Eng , vol.47 , Issue.3 , pp. 179-184
    • Erdemir, A.1    Fenske, G.R.2    Erck, R.A.3    Nichols, F.A.4    Busch, D.E.5
  • 28
    • 33845251815 scopus 로고    scopus 로고
    • Pressureless sintering of large-scale fine structural alumina matrix ceramic guideway materials
    • Liu C.X., Zhang J.H., Sun J.L., and Zhang X.H. Pressureless sintering of large-scale fine structural alumina matrix ceramic guideway materials. Mater Sci Eng: A 444 1-2 (2007) 58-63
    • (2007) Mater Sci Eng: A , vol.444 , Issue.1-2 , pp. 58-63
    • Liu, C.X.1    Zhang, J.H.2    Sun, J.L.3    Zhang, X.H.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.