3
-
-
0042994080
-
Flexural fatigue behavior of resin composite dental restoratives
-
Lohbauer U., von der Horst T., Frankenberger R., Krämer N., and Petschelt A. Flexural fatigue behavior of resin composite dental restoratives. Dental Materials 19 (2003) 435-440
-
(2003)
Dental Materials
, vol.19
, pp. 435-440
-
-
Lohbauer, U.1
von der Horst, T.2
Frankenberger, R.3
Krämer, N.4
Petschelt, A.5
-
8
-
-
0026480109
-
Solvent degradation and reduced fracture toughness in aged composites
-
Ferracane J.L., and Marker V.A. Solvent degradation and reduced fracture toughness in aged composites. Journal of Dental Research 71 (1992) 13-19
-
(1992)
Journal of Dental Research
, vol.71
, pp. 13-19
-
-
Ferracane, J.L.1
Marker, V.A.2
-
9
-
-
0026919822
-
Post-cure heat treatments of composites: properties and fractography
-
Ferracane J.L., and Condon J.R. Post-cure heat treatments of composites: properties and fractography. Dental Materials 8 (1992) 290-295
-
(1992)
Dental Materials
, vol.8
, pp. 290-295
-
-
Ferracane, J.L.1
Condon, J.R.2
-
10
-
-
0032488231
-
In vitro aging of dental composites in water-effect of degree of conversion, filler volume, and filler matrix coupling
-
Ferracane J.L., Berge H.X., and Condon J.R. In vitro aging of dental composites in water-effect of degree of conversion, filler volume, and filler matrix coupling. Journal of Biomedical Materials Research 42 (1998) 465-472
-
(1998)
Journal of Biomedical Materials Research
, vol.42
, pp. 465-472
-
-
Ferracane, J.L.1
Berge, H.X.2
Condon, J.R.3
-
12
-
-
0344563774
-
Fracture mechanics of dental composites
-
Marcel Dekker, Inc. [Chapter 56, 2813-44]
-
Drummond J.L., Botsis J., and Zhao D. Fracture mechanics of dental composites. Encyclopedia of biomaterials and bioengineering (1995), Marcel Dekker, Inc. [Chapter 56, 2813-44]
-
(1995)
Encyclopedia of biomaterials and bioengineering
-
-
Drummond, J.L.1
Botsis, J.2
Zhao, D.3
-
13
-
-
0029335996
-
Fracture toughness of experimental dental composites aged in ethanol
-
Ferracane J.L., and Berge H.X. Fracture toughness of experimental dental composites aged in ethanol. Journal of Dental Research 74 (1995) 1418-1423
-
(1995)
Journal of Dental Research
, vol.74
, pp. 1418-1423
-
-
Ferracane, J.L.1
Berge, H.X.2
-
15
-
-
4644263809
-
Buonocore memorial lecture review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition
-
Manhart J., Chen H., Hamm G., and Hickel R. Buonocore memorial lecture review of the clinical survival of direct and indirect restorations in posterior teeth of the permanent dentition. Operative Dentistry 29 (2004) 481-508
-
(2004)
Operative Dentistry
, vol.29
, pp. 481-508
-
-
Manhart, J.1
Chen, H.2
Hamm, G.3
Hickel, R.4
-
16
-
-
58149326616
-
Properties of heat treated composites: after aging in water
-
Ferracane J.L., Hopkin J.K., and Condon J.R. Properties of heat treated composites: after aging in water. Dental Materials 11 (1995) 354-358
-
(1995)
Dental Materials
, vol.11
, pp. 354-358
-
-
Ferracane, J.L.1
Hopkin, J.K.2
Condon, J.R.3
-
17
-
-
0032246057
-
Effect of water and artificial saliva on the low cyclic fatigue resistance of cobalt-chromium dental alloy
-
Lassila L.J.V., and Vallittu P.K. Effect of water and artificial saliva on the low cyclic fatigue resistance of cobalt-chromium dental alloy. Journal of Prosthetic Dentistry 80 (1998) 708-713
-
(1998)
Journal of Prosthetic Dentistry
, vol.80
, pp. 708-713
-
-
Lassila, L.J.V.1
Vallittu, P.K.2
-
18
-
-
33746594203
-
The effect of periodontal surgery on bite force, occlusal contact area and bite pressure
-
Alkan A., Keskiner I., Arici S., and Sato S. The effect of periodontal surgery on bite force, occlusal contact area and bite pressure. Journal of the American Dental Association 137 (2006) 978-983
-
(2006)
Journal of the American Dental Association
, vol.137
, pp. 978-983
-
-
Alkan, A.1
Keskiner, I.2
Arici, S.3
Sato, S.4
-
19
-
-
0003606756
-
PS070-97, Standard Test Methods for the Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature
-
ASTM
-
ASTM PS070-97, Standard Test Methods for the Determination of Fracture Toughness of Advanced Ceramics at Ambient Temperature; 1997.
-
(1997)
-
-
-
21
-
-
2342464149
-
Evaluation of fracture toughness of a fiber containing dental composite after flexural fatigue
-
Drummond J.L., Lin L., and Miescke K.J. Evaluation of fracture toughness of a fiber containing dental composite after flexural fatigue. Dental Materials 20 (2004) 591-599
-
(2004)
Dental Materials
, vol.20
, pp. 591-599
-
-
Drummond, J.L.1
Lin, L.2
Miescke, K.J.3
-
22
-
-
33947410005
-
Contact versus flexure fatigue of a fiber-filled composite
-
Al-Turki L.I., Drummond J.L., Agojci M., Gosz M., Tyrus J.M., and Lin L. Contact versus flexure fatigue of a fiber-filled composite. Dental Materials 23 (2007) 648-653
-
(2007)
Dental Materials
, vol.23
, pp. 648-653
-
-
Al-Turki, L.I.1
Drummond, J.L.2
Agojci, M.3
Gosz, M.4
Tyrus, J.M.5
Lin, L.6
-
23
-
-
0042994084
-
In vitro characterization of two laboratory-processed resin composites
-
Kakaboura A., Rahiotis C., Zinelis S., Al-Dhamadi Y.A., Silikas N., and Watts D.C. In vitro characterization of two laboratory-processed resin composites. Dental Materials 19 (2003) 393-398
-
(2003)
Dental Materials
, vol.19
, pp. 393-398
-
-
Kakaboura, A.1
Rahiotis, C.2
Zinelis, S.3
Al-Dhamadi, Y.A.4
Silikas, N.5
Watts, D.C.6
|