Volumn 43, Issue 1, 2009, Pages 47-52

Coupled recycling of PVC and glass wastes producing chlorine-free fuels and cement feed stock

Author keywords

[No Author keywords available]

Indexed keywords

CROSS SECTIONS; DRY ATMOSPHERES; EDS ANALYSIS; EFFECTIVE DIFFUSION COEFFICIENTS; EXPERIMENTAL CONDITIONS; FEED STOCKS; GLASS CULLETS; GLASS MATRICES; GLASS PARTICLES; GLASS SURFACES; GLASS WASTES; HYDROTHERMAL TREATMENTS; KINETIC STUDIES; NEUTRALIZATION RATES; POROUS SURFACES; SODA GLASS; SODIUM IONS; STEAM PRESSURES;

EID: 61849129359     PISSN: 0013936X     EISSN: 15205851     Source Type: Journal    
DOI: 10.1021/es800599y     Document Type: Article
Times cited : (6)

References (19)
  • 1
    • 63849216297 scopus 로고    scopus 로고
    • Method and equipment to produce useful gas from halogen-containing combustible materials and alkali-containing substances. Japan
    • Patent 3878994, November 5
    • Horio, M.; Noda, R.; Sung, H.-J. Method and equipment to produce useful gas from halogen-containing combustible materials and alkali-containing substances. Japan Patent 3878994, November 5, 2006.
    • (2006)
    • Horio, M.1    Noda, R.2    Sung, H.-J.3
  • 2
    • 17144421253 scopus 로고    scopus 로고
    • Thermal treatment of waste PVC and chlorine neutralization by waste glass
    • Sung, H.-J.; Noda, R.; Horio, M. Thermal treatment of waste PVC and chlorine neutralization by waste glass. J. Chem. Eng. Jpn. 2005, 38, 220-228.
    • (2005) J. Chem. Eng. Jpn , vol.38 , pp. 220-228
    • Sung, H.-J.1    Noda, R.2    Horio, M.3
  • 3
    • 63849327305 scopus 로고    scopus 로고
    • Production process of fuel and raw material by neutralization of glass wastes and halogen- containing plastic wastes. Japan
    • Patent Disclosure 2006- 229642, August 25, 2006
    • Horio, M.; Noda, R.; Sung, H.-J., Sato, K.; Sueoka, T. Production process of fuel and raw material by neutralization of glass wastes and halogen- containing plastic wastes. Japan Patent Disclosure 2006- 229642, August 25, 2006.
    • Horio, M.1    Noda, R.2    Sung, H.-J.3    Sato, K.4    Sueoka, T.5
  • 5
    • 0000764373 scopus 로고
    • Self-diffusion of sodium ions in a borosilicate glass and a soda-lime glass
    • Wilson, C. G.; Carter, A. C. Self-diffusion of sodium ions in a borosilicate glass and a soda-lime glass. Phys. Chem. Glasses 1964, 5, 111-112.
    • (1964) Phys. Chem. Glasses , vol.5 , pp. 111-112
    • Wilson, C.G.1    Carter, A.C.2
  • 6
    • 0043085792 scopus 로고
    • Na diffusion in soda-lime-aluminosilicate glasses
    • Williams, E. L.; Heckman, R. W. Na diffusion in soda-lime-aluminosilicate glasses. Phys. Chem. Glasses 1964, 5, 166-171.
    • (1964) Phys. Chem. Glasses , vol.5 , pp. 166-171
    • Williams, E.L.1    Heckman, R.W.2
  • 7
    • 0346539865 scopus 로고
    • Self-diffusion of sodium ions in some silicate glasses
    • Terai, R.; Kitaoka, T.; Ueno, T. Self-diffusion of sodium ions in some silicate glasses. Yogyo Kyokai Shi 1969, 77, 88-94.
    • (1969) Yogyo Kyokai Shi , vol.77 , pp. 88-94
    • Terai, R.1    Kitaoka, T.2    Ueno, T.3
  • 8
    • 0038861581 scopus 로고
    • The clouding of soda-lime-silica glass in atmospheres containing sulphur dioxide
    • Coward, J. N.; Turner, W. E. S. The clouding of soda-lime-silica glass in atmospheres containing sulphur dioxide. J. Soc. Glass Technol. 1938, 22, 309-323.
    • (1938) J. Soc. Glass Technol , vol.22 , pp. 309-323
    • Coward, J.N.1    Turner, W.E.S.2
  • 9
    • 3843108544 scopus 로고
    • Surface dealkalization of finished glassware
    • Williams, H. S.; Weyl, W. A. Surface dealkalization of finished glassware. Glass Ind. 1945, 26, 290-292.
    • (1945) Glass Ind , vol.26 , pp. 290-292
    • Williams, H.S.1    Weyl, W.A.2
  • 10
    • 0000886433 scopus 로고
    • The action of water and of sulphur dioxide on glass surfaces
    • Douglas, R. W.; Isard, J. O. The action of water and of sulphur dioxide on glass surfaces. J. Soc. Glass Technol. 1949, 33, 289- 335.
    • (1949) J. Soc. Glass Technol , vol.33 , pp. 289-335
    • Douglas, R.W.1    Isard, J.O.2
  • 11
    • 84977692414 scopus 로고
    • Strengthening of glass surfaces by sulfur trioxide treatment
    • Mochel, E. L.; Nordberg, M. E.; Elmer, T. H. Strengthening of glass surfaces by sulfur trioxide treatment. J. Am. Ceram. Soc. 1966, 49, 585-589.
    • (1966) J. Am. Ceram. Soc , vol.49 , pp. 585-589
    • Mochel, E.L.1    Nordberg, M.E.2    Elmer, T.H.3
  • 12
    • 63849296419 scopus 로고
    • Treatment of newly formed glass articles
    • U.S. patent 3 249 246, May 3
    • Mahoney, W. P. Treatment of newly formed glass articles. U.S. patent 3 249 246, May 3, 1966.
    • (1966)
    • Mahoney, W.P.1
  • 13
    • 63849159550 scopus 로고    scopus 로고
    • Poole, J. P.; Snyder, H. C; Ryder, R. J. Corrosion retarding fluorine treatment of glass surfaces. U.S. patent 3314772, April 18, 1967.
    • Poole, J. P.; Snyder, H. C; Ryder, R. J. Corrosion retarding fluorine treatment of glass surfaces. U.S. patent 3314772, April 18, 1967.
  • 15
    • 0020802642 scopus 로고
    • Fluorine treatment of soda-lime silicate glass surfaces
    • Brow, R. K.; LaCourse, W. Fluorine treatment of soda-lime silicate glass surfaces. J. Am. Ceram. Soc. 1983, 66, C-123.
    • (1983) J. Am. Ceram. Soc , vol.66
    • Brow, R.K.1    LaCourse, W.2
  • 16
    • 0021394511 scopus 로고
    • Dealkalization of glass surfaces utilizing HC1 gas
    • Schaeffer, H. A.; Stengel, M.; Mecha, J. Dealkalization of glass surfaces utilizing HC1 gas. J. Non-Cryst. Solids 1986, 80, 400- 404.
    • (1986) J. Non-Cryst. Solids , vol.80 , pp. 400-404
    • Schaeffer, H.A.1    Stengel, M.2    Mecha, J.3
  • 18
  • 19
    • 0020737770 scopus 로고
    • Diffusion-controlled reaction of water with glass
    • Doremus, R. H. Diffusion-controlled reaction of water with glass. J. Non-Cryst. Solids 1983, 55, 143-147.
    • (1983) J. Non-Cryst. Solids , vol.55 , pp. 143-147
    • Doremus, R.H.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.