메뉴 건너뛰기




Volumn 72, Issue 3, 2009, Pages 232-241

In situ indentation of nanoporous gold thin films in the transmission electron microscope

Author keywords

Dislocations; Gold; Loading rate; Mechanical behavior; Porous materials; TEM

Indexed keywords

DROPS; GOLD; METALLIC FILMS; NANOINDENTATION; PLASTICITY; THIN FILMS; TRANSMISSION ELECTRON MICROSCOPY;

EID: 61449210854     PISSN: 1059910X     EISSN: 10970029     Source Type: Journal    
DOI: 10.1002/jemt.20676     Document Type: Article
Times cited : (33)

References (24)
  • 3
    • 3042857924 scopus 로고    scopus 로고
    • Metallic mesoporous nanocom-posites for electrocatalysis
    • Ding Y, Chen M, Erlebacher J. 2004a. Metallic mesoporous nanocom-posites for electrocatalysis. J Am Chem Soc 126:6876-6877.
    • (2004) J Am Chem Soc , vol.126 , pp. 6876-6877
    • Ding, Y.1    Chen, M.2    Erlebacher, J.3
  • 4
    • 10444247443 scopus 로고    scopus 로고
    • Nanoporous gold leaf: Ancient technology'Vadvanced material
    • Ding Y, Kim Y-J, Erlebacher J. 2004b. Nanoporous gold leaf: "Ancient technology'Vadvanced material. Adv Mater 16:1897-1900.
    • (2004) Adv Mater , vol.16 , pp. 1897-1900
    • Ding, Y.1    Kim, Y.-J.2    Erlebacher, J.3
  • 5
    • 0037768811 scopus 로고    scopus 로고
    • Dealloying of Ag-Au alloys in halide-containing electrolytes. Affect on critical potential and pore size
    • Dursun A, Pugh DV, Corcoran SG. 2003. Dealloying of Ag-Au alloys in halide-containing electrolytes. Affect on critical potential and pore size. J Electrochem Soc 150:355-360.
    • (2003) J Electrochem Soc , vol.150 , pp. 355-360
    • Dursun, A.1    Pugh, D.V.2    Corcoran, S.G.3
  • 10
    • 2442672871 scopus 로고    scopus 로고
    • Formation of nanoporous platinum by selective anodic dissolution of PtZn surface alloy in a Lewis acidic zinc chloride-1-ethyl-3-methylimidazolium chloride ionic liquid
    • Huang J-F, Sun I-W. 2004. Formation of nanoporous platinum by selective anodic dissolution of PtZn surface alloy in a Lewis acidic zinc chloride-1-ethyl-3-methylimidazolium chloride ionic liquid. Chem Mater 16:1829-1831.
    • (2004) Chem Mater , vol.16 , pp. 1829-1831
    • Huang, J.-F.1    Sun, I.-W.2
  • 11
    • 20544440139 scopus 로고    scopus 로고
    • Fabrication and surface functionalization of nanoporous gold by electrochemical alloying/dealloying of Au-Zn in an ionic liquid, and the self-assembly of L-cysteine monolayers
    • Huang J-F, Sun IW. 2005. Fabrication and surface functionalization of nanoporous gold by electrochemical alloying/dealloying of Au-Zn in an ionic liquid, and the self-assembly of L-cysteine monolayers. Adv Funct Mater 15:989-994.
    • (2005) Adv Funct Mater , vol.15 , pp. 989-994
    • Huang, J.-F.1    Sun, I.W.2
  • 12
    • 0037011560 scopus 로고    scopus 로고
    • Fabrication of nanoporous gold nanowires
    • Ji C, Searson PC. 2002. Fabrication of nanoporous gold nanowires. Appl Phys Lett 81:4437-4439.
    • (2002) Appl Phys Lett , vol.81 , pp. 4437-4439
    • Ji, C.1    Searson, P.C.2
  • 13
    • 0038728438 scopus 로고    scopus 로고
    • Synthesis and characterization of nanoporous gold nanowires
    • Ji C, Searson PC. 2003. Synthesis and characterization of nanoporous gold nanowires. J Phys Chem B 107:4494-4499.
    • (2003) J Phys Chem B , vol.107 , pp. 4494-4499
    • Ji, C.1    Searson, P.C.2
  • 15
    • 0000198275 scopus 로고
    • Ductile-brittle transition in random porous Au
    • Li R, Sieradzki K. 1992. Ductile-brittle transition in random porous Au. Phys Rev Lett 68:1168-1171.
    • (1992) Phys Rev Lett , vol.68 , pp. 1168-1171
    • Li, R.1    Sieradzki, K.2
  • 16
    • 0035839858 scopus 로고    scopus 로고
    • Quantitative in situ nano-indentation in an electron microscope
    • Minor AM, Morris JW, Jr, Stach EA. 2001. Quantitative in situ nano-indentation in an electron microscope. Appl Phys Lett 79:1625-1627.
    • (2001) Appl Phys Lett , vol.79 , pp. 1625-1627
    • Minor, A.M.1    Morris Jr, J.W.2    Stach, E.A.3
  • 18
    • 61449136504 scopus 로고    scopus 로고
    • Ph.D. Dissertation, Virginia Polytechnic Institute and State University. 134 p
    • Pugh DV. 2003. Nanoporous Platinum [Ph.D. Dissertation], Virginia Polytechnic Institute and State University. 134 p.
    • (2003) Nanoporous Platinum
    • Pugh, D.V.1
  • 19
    • 0024646784 scopus 로고
    • Computer simulations of corrosion: Selective dissolution of binary alloys
    • Sieradzki K, Corderman RR, Shukla K, Newman RC. 1989. Computer simulations of corrosion: Selective dissolution of binary alloys. Philos Mag A 59:713-746.
    • (1989) Philos Mag A , vol.59 , pp. 713-746
    • Sieradzki, K.1    Corderman, R.R.2    Shukla, K.3    Newman, R.C.4
  • 21
    • 40949113835 scopus 로고    scopus 로고
    • The mechanical behavior of nanoporous gold thin films
    • Sun Y, Ye J, Shan Z, Minor AM, Balk TJ. 2007. The mechanical behavior of nanoporous gold thin films. JOM 59:54-58.
    • (2007) JOM , vol.59 , pp. 54-58
    • Sun, Y.1    Ye, J.2    Shan, Z.3    Minor, A.M.4    Balk, T.J.5
  • 22
    • 40949160523 scopus 로고    scopus 로고
    • Microstructure, stability and thermomechanical behavior of crack-free thin films of nanoporous gold
    • Sun Y, Kucera KP, Burger SA, John Balk TJ. 2008. Microstructure, stability and thermomechanical behavior of crack-free thin films of nanoporous gold. Scr Mater 58:1018-1021.
    • (2008) Scr Mater , vol.58 , pp. 1018-1021
    • Sun, Y.1    Kucera, K.P.2    Burger, S.A.3    John Balk, T.J.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.