Erratum to "Ln0.6Sr0.4Co1-yFeyO3-δ (Ln = La and Nd; y = 0 and 0.5) cathodes with thin yttria-stabilized zirconia electrolytes for intermediate temperature solid oxide fuel cells" [J. Power Sources 187 (2) (2009) 480-486] (DOI:10.1016/j.jpowsour.2008.11.025);Ln0.6Sr0.4Co1-yFeyO3-δ (Ln = La and Nd; y = 0 and 0.5) cathodes with thin yttria-stabilized zirconia electrolytes for intermediate temperature solid oxide fuel cells
|
Author keywords
Cobaltite cathodes; Intermediate temperature solid oxide fuel cells; Thin yttria stabilized zirconia electrolytes
|
Indexed keywords
CATHODES;
ELECTRIC CONDUCTIVITY;
GAS FUEL PURIFICATION;
LANTHANUM;
PEROVSKITE;
SCREEN PRINTING;
SOLID OXIDE FUEL CELLS (SOFC);
STRONTIUM COMPOUNDS;
THERMAL EXPANSION;
YTTRIA STABILIZED ZIRCONIA;
YTTRIUM OXIDE;
ZIRCONIA;
ELECTRICAL CONDUCTIVITY;
ELECTROCHEMICAL PERFORMANCE;
HIGH ELECTRICAL CONDUCTIVITY;
INTERMEDIATE TEMPERATURE SOLID OXIDE FUEL CELL;
PEAK POWER DENSITIES;
THERMAL EXPANSION COEFFICIENTS;
YTTRIA STABILIZED ZIRCONIA ELECTROLYTE;
YTTRIA-STABILIZED ZIRCONIAS (YSZ);
SOLID ELECTROLYTES;
|
EID: 58649104197
PISSN: 03787753
EISSN: None
Source Type: Journal
DOI: 10.1016/j.jpowsour.2009.02.003 Document Type: Erratum |
Times cited : (31)
|
References (22)
|