Volumn 52, Issue 1, 2009, Pages 186-189

Microstructure and texture evolution during warm compression of the magnesium alloy AZ31

Author keywords

AZ31; Electron backscattered diffraction (EBSD); Slip; Texture; Twinning

Indexed keywords

CERIUM ALLOYS; DIFFRACTION; MAGNESIUM; MAGNESIUM ALLOYS; MAGNESIUM PRINTING PLATES; MICROSTRUCTURE; MILITARY OPERATIONS; TEXTURES;

EID: 58349107667     PISSN: 10069321     EISSN: 1862281X     Source Type: Journal    
DOI: 10.1007/s11431-008-0292-5     Document Type: Article
Times cited : (4)

References (20)
  • 1
    • 0035871499 scopus 로고    scopus 로고
    • Magnesium: Properties-applications - Potential
    • 1
    • B. L. Mordike T. Ebert 2001 Magnesium: Properties-applications - potential Mater Sci Eng A 302 1 37 45
    • (2001) Mater Sci Eng A , vol.302 , pp. 37-45
    • Mordike, B.L.1    Ebert, T.2
  • 2
    • 0037732725 scopus 로고    scopus 로고
    • Texture analysis in hexagonal materials
    • 1
    • Y. N. Wang J. C. Huang 2003 Texture analysis in hexagonal materials Mat Chem Phys 81 1 11 26
    • (2003) Mat Chem Phys , vol.81 , pp. 11-26
    • Wang, Y.N.1    Huang, J.C.2
  • 3
    • 1242332600 scopus 로고    scopus 로고
    • Experimental determination and theoretical prediction of twin orientations in magnesium alloy AZ31
    • 8
    • P. Yang Y. Yu L. Chen 2004 Experimental determination and theoretical prediction of twin orientations in magnesium alloy AZ31 Scripta Mater 50 8 1163 1168
    • (2004) Scripta Mater , vol.50 , pp. 1163-1168
    • Yang, P.1    Yu, Y.2    Chen, L.3
  • 4
    • 0037603249 scopus 로고    scopus 로고
    • Texture development and its effect on mechanical properties of an AZ61 Mg alloy fabricated by equal channel angular pressing
    • 11
    • W. J. Kim S. I. Hong Y. S. Kim 2003 Texture development and its effect on mechanical properties of an AZ61 Mg alloy fabricated by equal channel angular pressing Acta Mater 51 11 3293 3307
    • (2003) Acta Mater , vol.51 , pp. 3293-3307
    • Kim, W.J.1    Hong, S.I.2    Kim, Y.S.3
  • 5
    • 0035803001 scopus 로고    scopus 로고
    • Application of texture simulation to understanding mechanical behavior of Mg and solid solution alloys containing Li or y
    • 20
    • S. R. Agnew M. H. Yoo C. N. Tome 2001 Application of texture simulation to understanding mechanical behavior of Mg and solid solution alloys containing Li or Y Acta Mater 49 20 4277 4289
    • (2001) Acta Mater , vol.49 , pp. 4277-4289
    • Agnew, S.R.1    Yoo, M.H.2    Tome, C.N.3
  • 6
    • 0031258156 scopus 로고    scopus 로고
    • Modelling and prediction of mechanical properties for materials with hexagonal symmetry (zinc, titanium and zirconium alloys)
    • 10
    • J. J. Fundenberger M. J. Philippe F. Wagner 1997 Modelling and prediction of mechanical properties for materials with hexagonal symmetry (zinc, titanium and zirconium alloys) Acta Mater 45 10 4041 4055
    • (1997) Acta Mater , vol.45 , pp. 4041-4055
    • Fundenberger, J.J.1    Philippe, M.J.2    Wagner, F.3
  • 7
    • 0000222423 scopus 로고
    • Modelling of texture evolution for materials of hexagonal symmetry-II. Application to zirconium and titanium α or near α alloys
    • 4
    • M. J. Philippe M. Serghat P. V. Houtte 1995 Modelling of texture evolution for materials of hexagonal symmetry-II. Application to zirconium and titanium α or near α alloys Acta Metall 43 4 1619 1630
    • (1995) Acta Metall , vol.43 , pp. 1619-1630
    • Philippe, M.J.1    Serghat, M.2    Houtte, P.V.3
  • 8
    • 0028262817 scopus 로고
    • Modelling of texture evolution for materials of hexagonal symmetry-I. Application to zinc alloys
    • 1
    • M. J. Philippe F. Wagner F. E. Mellab 1994 Modelling of texture evolution for materials of hexagonal symmetry-I. Application to zinc alloys Acta Metall 42 1 239 250
    • (1994) Acta Metall , vol.42 , pp. 239-250
    • Philippe, M.J.1    Wagner, F.2    Mellab, F.E.3
  • 9
    • 1042263855 scopus 로고    scopus 로고
    • Cold rolling textures in AZ31 wrought magnesium alloy
    • 7
    • A. Styczynski C. Hartig J. Bohlen 2004 Cold rolling textures in AZ31 wrought magnesium alloy Scripta Mater 50 7 943 947
    • (2004) Scripta Mater , vol.50 , pp. 943-947
    • Styczynski, A.1    Hartig, C.2    Bohlen, J.3
  • 10
    • 5744227425 scopus 로고    scopus 로고
    • Deformation microstructures and textures of some cold rolled Mg alloys
    • 1-2
    • M. R. Barnett M. D. Nave C. J. Bettles 2004 Deformation microstructures and textures of some cold rolled Mg alloys Mater Sci Eng A 386 1-2 205 211
    • (2004) Mater Sci Eng A , vol.386 , pp. 205-211
    • Barnett, M.R.1    Nave, M.D.2    Bettles, C.J.3
  • 11
    • 0035703496 scopus 로고    scopus 로고
    • Non-basal slip systems in HCP metals and alloys: Source mechanisms
    • M. H. Yoo S. R. Agnew J. R. Morris 2001 Non-basal slip systems in HCP metals and alloys: source mechanisms Mater Sci Eng A 319-321 87 92
    • (2001) Mater Sci Eng A , vol.319-321 , pp. 87-92
    • Yoo, M.H.1    Agnew, S.R.2    Morris, J.R.3
  • 12
    • 0037247325 scopus 로고    scopus 로고
    • A mechanistic understanding of the formability of magnesium: Examining the role of temperature on the deformation mechanisms
    • S. R. Agnew O. Duygulu 2003 A mechanistic understanding of the formability of magnesium: Examining the role of temperature on the deformation mechanisms Mater Sci Forum 419-422 177 188
    • (2003) Mater Sci Forum , vol.419-422 , pp. 177-188
    • Agnew, S.R.1    Duygulu, O.2
  • 13
    • 29444454030 scopus 로고    scopus 로고
    • Influence of grain orientation on twinning during warm compression of wrought Mg-3Al-1Zn
    • 12
    • J. Jiang A. Godfrey Q. Liu 2005 Influence of grain orientation on twinning during warm compression of wrought Mg-3Al-1Zn Mater Sci Technol 21 12 1417 1422
    • (2005) Mater Sci Technol , vol.21 , pp. 1417-1422
    • Jiang, J.1    Godfrey, A.2    Liu, Q.3
  • 14
    • 28944455378 scopus 로고    scopus 로고
    • Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loading
    • 2
    • S. B. Yi C. H. J. Davies H. G. Brokmeier 2006 Deformation and texture evolution in AZ31 magnesium alloy during uniaxial loading Acta Mater 54 2 549 562
    • (2006) Acta Mater , vol.54 , pp. 549-562
    • Yi, S.B.1    Davies, C.H.J.2    Brokmeier, H.G.3
  • 15
    • 23444461727 scopus 로고    scopus 로고
    • Internal strain and texture evolution during deformation twinning in magnesium
    • 1-2
    • D. B. Brown S. R. Agnew M. A. M. Bourke 2005 Internal strain and texture evolution during deformation twinning in magnesium Mater Sci Eng A 399 1-2 1 12
    • (2005) Mater Sci Eng A , vol.399 , pp. 1-12
    • Brown, D.B.1    Agnew, S.R.2    Bourke, M.A.M.3
  • 16
    • 41849150440 scopus 로고    scopus 로고
    • Microtexture evolution via deformation twinning and slip during compression of magnesium alloy AZ31
    • J. Jiang A. Godfrey W. Liu 2008 Microtexture evolution via deformation twinning and slip during compression of magnesium alloy AZ31 Mater Sci Eng A 483 576 579
    • (2008) Mater Sci Eng A , vol.483 , pp. 576-579
    • Jiang, J.1    Godfrey, A.2    Liu, W.3
  • 17
    • 4344568184 scopus 로고    scopus 로고
    • Microstructures and textures of pure magnesium deformed in plane-strain compression
    • 9
    • M. D. Nave M. R. Barnett 2004 Microstructures and textures of pure magnesium deformed in plane-strain compression Scripta Mater 51 9 881 885
    • (2004) Scripta Mater , vol.51 , pp. 881-885
    • Nave, M.D.1    Barnett, M.R.2
  • 18
    • 14644394318 scopus 로고    scopus 로고
    • Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature
    • 7
    • J. Koike R. Ohyama 2005 Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature Acta Mater 53 7 1963 1972
    • (2005) Acta Mater , vol.53 , pp. 1963-1972
    • Koike, J.1    Ohyama, R.2
  • 19
    • 17044430255 scopus 로고    scopus 로고
    • Texture changes during uniaxial compression of Mg-3Al-1Zn
    • P. Backx M. R. Barnett L. Kestens 2004 Texture changes during uniaxial compression of Mg-3Al-1Zn Mater Sci Forum 467-470 429 434
    • (2004) Mater Sci Forum , vol.467-470 , pp. 429-434
    • Backx, P.1    Barnett, M.R.2    Kestens, L.3
  • 20
    • 28944432816 scopus 로고    scopus 로고
    • Texture development in pure Mg and Mg alloy AZ31
    • G. Gottstein T. A. Samman 2005 Texture development in pure Mg and Mg alloy AZ31 Mater Sci Forum 495-497 623 632
    • (2005) Mater Sci Forum , vol.495-497 , pp. 623-632
    • Gottstein, G.1    Samman, T.A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.