Volumn 49, Issue 11, 2008, Pages 2732-2736

Improvement of plasticity in Pd containing Zr-Al-Ni-Cu bulk metallic glass by deformation-induced nano structure change

Author keywords

Casting; Deformation; Metallic glass; Nanocrystallization; Plasticity; Shear band; Structural relaxation

Indexed keywords

ALUMINUM; COOLING; COPPER; DEFORMATION; GLASS; LIQUID METALS; METALLIC SOAPS; NANOCRYSTALLINE ALLOYS; NANOCRYSTALLIZATION; NICKEL; PALLADIUM; PLASTICITY; PRECIPITATION (CHEMICAL); SHEAR BANDS; STRUCTURAL RELAXATION; ZIRCONIUM;

EID: 58149263478     PISSN: 13459678     EISSN: None     Source Type: Journal    
DOI: 10.2320/matertrans.MER2008162     Document Type: Article
Times cited : (10)

References (21)
  • 7
    • 28344444162 scopus 로고    scopus 로고
    • J. Saida, A. D. H. Setyawan, H. Kato and A. Inoue: Appl. Phys. Lett. 87 (2005) 151907-1-3.
    • J. Saida, A. D. H. Setyawan, H. Kato and A. Inoue: Appl. Phys. Lett. 87 (2005) 151907-1-3.
  • 13
    • 0035508343 scopus 로고    scopus 로고
    • L. Q. Xing, Y. Li, K. T. Ramesh, J. Li and T. C. Hufnagel: Phys. Rev. B 64 (2001) 180201-1-4.
    • L. Q. Xing, Y. Li, K. T. Ramesh, J. Li and T. C. Hufnagel: Phys. Rev. B 64 (2001) 180201-1-4.
  • 15
    • 20844441412 scopus 로고    scopus 로고
    • K. B. Kim, J. Das, F. Baier and J. Eckert: Appl. Phys. Lett. 86 (2005) 171909-1-3.
    • K. B. Kim, J. Das, F. Baier and J. Eckert: Appl. Phys. Lett. 86 (2005) 171909-1-3.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.