Volumn 130, Issue 4, 2008, Pages

Formation and characterization of tribofilms

Author keywords

Lubrication; Nanoparticles; Polarity; Tribofilm; Wear

Indexed keywords

ADSORPTION; BIODEGRADATION; DEBRIS; ETHYLENE GLYCOL; GLYCOLS; HYDROCARBONS; LUBRICANTS; LUBRICATING OILS; LUBRICATION; MINERAL OILS; MINERALOGY; MINERALS; NANOPARTICLES; POLYETHYLENE GLYCOLS; POLYETHYLENE OXIDES; QUANTUM CHEMISTRY; SCANNING ELECTRON MICROSCOPY; SILICA; SILICATE MINERALS; TRANSMISSION ELECTRON MICROSCOPY; VEGETABLE OILS;

EID: 57149141509     PISSN: 07424787     EISSN: 15288897     Source Type: Journal    
DOI: 10.1115/1.2958071     Document Type: Article
Times cited : (25)

References (24)
  • 1
    • 3943058285 scopus 로고    scopus 로고
    • X-Ray Photoelectron Spectroscopy Analysis of Antiwear Tribofilms Produced on Boundary-Lubricated Steel Surfaces From Sulfur- and PhosphorusContaining Additives and Metal Deactivator Additive
    • Komvopoulos, K., Do, V., Yamaguchi, E., Yeh, S., and Ryason, P., 2004, "X-Ray Photoelectron Spectroscopy Analysis of Antiwear Tribofilms Produced on Boundary-Lubricated Steel Surfaces From Sulfur- and PhosphorusContaining Additives and Metal Deactivator Additive," Tribol. Trans., 47(3), pp. 321-327.
    • (2004) Tribol. Trans , vol.47 , Issue.3 , pp. 321-327
    • Komvopoulos, K.1    Do, V.2    Yamaguchi, E.3    Yeh, S.4    Ryason, P.5
  • 2
    • 33747177584 scopus 로고    scopus 로고
    • ZDDP and MoDTC Interactions in Boundary Lubrication-The Effect of Temperature and ZDDP/MoDTC Ratio
    • Morina, A., Neville, A., Priest, M., and Green, J. H., 2006, "ZDDP and MoDTC Interactions in Boundary Lubrication-The Effect of Temperature and ZDDP/MoDTC Ratio," Tribol. Int., 39(12), pp. 1545-1557.
    • (2006) Tribol. Int , vol.39 , Issue.12 , pp. 1545-1557
    • Morina, A.1    Neville, A.2    Priest, M.3    Green, J.H.4
  • 4
    • 0141862203 scopus 로고    scopus 로고
    • Friction-Enhancing Properties of ZDDP Antiwear Additive: Part I-Friction and Morphology of ZDDP Reaction Films
    • Taylor, L. J., and Spikes, H. A., 2003, "Friction-Enhancing Properties of ZDDP Antiwear Additive: Part I-Friction and Morphology of ZDDP Reaction Films," Tribol. Trans., 46(3), pp. 303-309.
    • (2003) Tribol. Trans , vol.46 , Issue.3 , pp. 303-309
    • Taylor, L.J.1    Spikes, H.A.2
  • 5
  • 6
    • 0035241790 scopus 로고    scopus 로고
    • A Review of the Mechanisms of Action of Antioxidants, Metal Deactivators, and Corrosion Inhibitors
    • Reyes-Gavilan, J. L., and Odorisio, P., 2001, "A Review of the Mechanisms of Action of Antioxidants, Metal Deactivators, and Corrosion Inhibitors," NLGI Spokesman, 64, pp. 22-33.
    • (2001) NLGI Spokesman , vol.64 , pp. 22-33
    • Reyes-Gavilan, J.L.1    Odorisio, P.2
  • 7
    • 4744357047 scopus 로고    scopus 로고
    • The History and Mechanisms of ZDDP
    • Spikes, H., 2004, "The History and Mechanisms of ZDDP," Tribol. Lett., 17(3), pp. 469-89.
    • (2004) Tribol. Lett , vol.17 , Issue.3 , pp. 469-489
    • Spikes, H.1
  • 8
    • 33747173746 scopus 로고    scopus 로고
    • Low-Friction Tribofilm Formed by the Reaction of ZDDP on Iron Oxide
    • Ito, K., Martin, J., Minfray, C., and Kato, K., 2006, "Low-Friction Tribofilm Formed by the Reaction of ZDDP on Iron Oxide," Tribol. Int., 39(12), pp. 1538-1544.
    • (2006) Tribol. Int , vol.39 , Issue.12 , pp. 1538-1544
    • Ito, K.1    Martin, J.2    Minfray, C.3    Kato, K.4
  • 9
    • 0034245139 scopus 로고    scopus 로고
    • Tribochemical Interactions Between Molybdenum Dithiophosphate and Succinimide Additives
    • Guerret-Piecourt, C., Grossiord, C., Le-Mogne, T., Martin, J. M., and Palermo, T., 2000, "Tribochemical Interactions Between Molybdenum Dithiophosphate and Succinimide Additives," Surf. Interface Anal., 30(1), pp. 646-650.
    • (2000) Surf. Interface Anal , vol.30 , Issue.1 , pp. 646-650
    • Guerret-Piecourt, C.1    Grossiord, C.2    Le-Mogne, T.3    Martin, J.M.4    Palermo, T.5
  • 10
    • 0025172593 scopus 로고
    • A Reciprocating Wear Test for Evaluating Boundary Lubrication
    • Sheasby, J. S., Caughlin, T. A., Blahey, A. G., and Laycock K. R, 1990, "A Reciprocating Wear Test for Evaluating Boundary Lubrication," Tribol, Int., 23(5), pp. 301-307.
    • (1990) Tribol, Int , vol.23 , Issue.5 , pp. 301-307
    • Sheasby, J.S.1    Caughlin, T.A.2    Blahey, A.G.3    Laycock, K.R.4
  • 12
    • 0024471231 scopus 로고
    • Comparison of Microstructural Effects on Two-Body and Three-Body Abrasive Wear
    • Yang, G. H., and Garrison, W. M., Jr., 1989, "Comparison of Microstructural Effects on Two-Body and Three-Body Abrasive Wear," Wear, 129(1), pp. 93-103.
    • (1989) Wear , vol.129 , Issue.1 , pp. 93-103
    • Yang, G.H.1    Garrison Jr., W.M.2
  • 13
    • 0026360717 scopus 로고
    • An Explanation of the Relation Between Wear and Material Hardness in Three-Body Abrasion
    • Fang, L., Zhou, Q. D., and Li, Y. J., 1991, "An Explanation of the Relation Between Wear and Material Hardness in Three-Body Abrasion," Wear, 151, pp. 313-321.
    • (1991) Wear , vol.151 , pp. 313-321
    • Fang, L.1    Zhou, Q.D.2    Li, Y.J.3
  • 14
    • 0038121892 scopus 로고    scopus 로고
    • Three-Body Abrasive Wear Behaviour of Polyaryletherketone Composites
    • Harsha, A. R, Tewari, U. S., and Venkatraman, B., 2003, "Three-Body Abrasive Wear Behaviour of Polyaryletherketone Composites," Wear, 254(7-8), pp. 680-692.
    • (2003) Wear , vol.254 , Issue.7-8 , pp. 680-692
    • Harsha, A.R.1    Tewari, U.S.2    Venkatraman, B.3
  • 15
    • 0028436675 scopus 로고
    • Three-Body Abrasive Wear of Ceramic Materials
    • Yamamoto, T., Olsson, M., and Hogmark, S., 1994, "Three-Body Abrasive Wear of Ceramic Materials," Wear, 174(1-2), pp. 21-31.
    • (1994) Wear , vol.174 , Issue.1-2 , pp. 21-31
    • Yamamoto, T.1    Olsson, M.2    Hogmark, S.3
  • 16
    • 0027575632 scopus 로고
    • Three-Body Abrasive Wear of 0.98% Carbon Steel
    • Das, S., Prasad, B. K., Jha, A. K., Modi, O. R, and Yegneswaran, A. H., 1993, "Three-Body Abrasive Wear of 0.98% Carbon Steel," Wear, 162-164(B), pp. 802-810.
    • (1993) Wear , vol.162-164 , Issue.B , pp. 802-810
    • Das, S.1    Prasad, B.K.2    Jha, A.K.3    Modi, O.R.4    Yegneswaran, A.H.5
  • 17
    • 33644694440 scopus 로고    scopus 로고
    • The Lubrication of DLC Coatings With Mineral and Biodegradable Oils Having Different Polar and Saturation Characteristics
    • Kalin, M., Vizintin, J., Vercammen, K., Barriga, J., and Amsek, A., 2006, "The Lubrication of DLC Coatings With Mineral and Biodegradable Oils Having Different Polar and Saturation Characteristics," Surf. Coat. Technol., 200(14-15), pp. 4515-4522.
    • (2006) Surf. Coat. Technol , vol.200 , Issue.14-15 , pp. 4515-4522
    • Kalin, M.1    Vizintin, J.2    Vercammen, K.3    Barriga, J.4    Amsek, A.5
  • 18
    • 34248360392 scopus 로고    scopus 로고
    • Wear and Surface Characterization of Boronized Pure Iron
    • Asthana, P., Usta, M., Ucisik, A. H., and Liang, H., 2007, "Wear and Surface Characterization of Boronized Pure Iron," ASME J. Tribol., 129, pp. 1-10.
    • (2007) ASME J. Tribol , vol.129 , pp. 1-10
    • Asthana, P.1    Usta, M.2    Ucisik, A.H.3    Liang, H.4
  • 19
    • 0026682032 scopus 로고
    • Influence of Molecular Weight and Composition on the Morphology and Mechanical Properties of SBSPolystyrene-Mineral Oil Blends
    • Flosenzier, L. S., and Torkelson, J. M., 1992, "Influence of Molecular Weight and Composition on the Morphology and Mechanical Properties of SBSPolystyrene-Mineral Oil Blends," Macromolecules, 25(2), pp. 735-742.
    • (1992) Macromolecules , vol.25 , Issue.2 , pp. 735-742
    • Flosenzier, L.S.1    Torkelson, J.M.2
  • 20
    • 2942577381 scopus 로고    scopus 로고
    • Modification of the Chemical Structure of an Environmentally-Friendly Castor Oil Lubricant
    • Di-Hua, T., and Bin, Y., 2004, "Modification of the Chemical Structure of an Environmentally-Friendly Castor Oil Lubricant," Synth. Lubr., 21, pp. 59-64.
    • (2004) Synth. Lubr , vol.21 , pp. 59-64
    • Di-Hua, T.1    Bin, Y.2
  • 22
    • 33745171018 scopus 로고    scopus 로고
    • A Comparison of the Tribological Behaviour of Steel/Steel, Steel/DLC and DLC/DLC Contacts When Lubricated With Mineral and Biodegradable Oils
    • Kalin, M., and Vižintin, J., 2006, "A Comparison of the Tribological Behaviour of Steel/Steel, Steel/DLC and DLC/DLC Contacts When Lubricated With Mineral and Biodegradable Oils," Wear, 261, pp. 22-31.
    • (2006) Wear , vol.261 , pp. 22-31
    • Kalin, M.1    Vižintin, J.2
  • 24
    • 0035338225 scopus 로고    scopus 로고
    • A Study of the Effect of Chemical Structure on Friction and Wear: Part 2-Vegetable Oils and Esters
    • Weller, D. E., Jr., and Perez, J. M., 2001, "A Study of the Effect of Chemical Structure on Friction and Wear: Part 2-Vegetable Oils and Esters," Lubr. Eng., 57(5), pp. 20-26.
    • (2001) Lubr. Eng , vol.57 , Issue.5 , pp. 20-26
    • Weller Jr., D.E.1    Perez, J.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.