메뉴 건너뛰기




Volumn 23, Issue 2, 2009, Pages 804-811

Hydro-abrasive erosion of concrete incorporating ground blast-furnace slag and ground basaltic pumice

Author keywords

Chloride penetration; Concrete; Ground basaltic pumice (GBP); Ground blast furnace slag (GBS); Hydro abrasive erosion; Permeability

Indexed keywords

ABRASIVES; AGGLOMERATION; AGGREGATES; ASTROPHYSICS; BLAST FURNACE PRACTICE; CAPILLARITY; CEMENTS; COMPRESSIVE STRENGTH; CONCRETE AGGREGATES; CONCRETE CONSTRUCTION; EROSION; EXPLOSIVES; FURNACES; ICE; LIQUIDS; SLAGS; SOIL MECHANICS; STRENGTH OF MATERIALS;

EID: 54349111666     PISSN: 09500618     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.conbuildmat.2008.03.003     Document Type: Article
Times cited : (30)

References (20)
  • 2
    • 0032118098 scopus 로고
    • Mechanical properties and durability of concrete made with blended fly ash
    • Naik T., Singh S., and Ramme B. Mechanical properties and durability of concrete made with blended fly ash. ACI Mat J 95 4 (1992) 454-462
    • (1992) ACI Mat J , vol.95 , Issue.4 , pp. 454-462
    • Naik, T.1    Singh, S.2    Ramme, B.3
  • 3
    • 0000099125 scopus 로고
    • Mechanical properties and durability of polypropylene fiber reinforced high-volume fly ash concrete for shotcrete application
    • Malhotra V., Carette G., and Bilodeau A. Mechanical properties and durability of polypropylene fiber reinforced high-volume fly ash concrete for shotcrete application. ACI Mat J 91 5 (1994) 478-486
    • (1994) ACI Mat J , vol.91 , Issue.5 , pp. 478-486
    • Malhotra, V.1    Carette, G.2    Bilodeau, A.3
  • 4
    • 0031224186 scopus 로고    scopus 로고
    • Influence of fly ash on setting and hardening characteristics of concrete systems
    • Naik T., and Singh S. Influence of fly ash on setting and hardening characteristics of concrete systems. ACI Mat J 94 5 (1997) 578-584
    • (1997) ACI Mat J , vol.94 , Issue.5 , pp. 578-584
    • Naik, T.1    Singh, S.2
  • 6
    • 0037399505 scopus 로고    scopus 로고
    • Sulfate resistance of high-performance concrete
    • Shannag M.J., and Shaia H.A. Sulfate resistance of high-performance concrete. Cement Concrete Compos 25 (2003) 363-369
    • (2003) Cement Concrete Compos , vol.25 , pp. 363-369
    • Shannag, M.J.1    Shaia, H.A.2
  • 9
    • 0141719911 scopus 로고    scopus 로고
    • Role of aluminous component of fly ash on the durability of Portland cement-fly ash pastes in marine environment
    • Lorenzo M.P., Goni S., and Guerrero A. Role of aluminous component of fly ash on the durability of Portland cement-fly ash pastes in marine environment. Waste Manage 23 (2003) 785-792
    • (2003) Waste Manage , vol.23 , pp. 785-792
    • Lorenzo, M.P.1    Goni, S.2    Guerrero, A.3
  • 10
    • 33846829858 scopus 로고    scopus 로고
    • Effect of crushed ceramic and basaltic pumice as fine aggregates on concrete mortar properties
    • Binici H. Effect of crushed ceramic and basaltic pumice as fine aggregates on concrete mortar properties. Constr Build Mater 21 (2007) 1191-1197
    • (2007) Constr Build Mater , vol.21 , pp. 1191-1197
    • Binici, H.1
  • 11
    • 2142646133 scopus 로고    scopus 로고
    • Experimental study of abrasion and corrosion resistance on hydraulic high strength concrete
    • Yin Y.G., et al. Experimental study of abrasion and corrosion resistance on hydraulic high strength concrete. Water Res Hydropower Eng 12 (1998) 51-52
    • (1998) Water Res Hydropower Eng , vol.12 , pp. 51-52
    • Yin, Y.G.1
  • 12
    • 2142703982 scopus 로고    scopus 로고
    • A recommendation on technical specification for abrasion and cavitation resistance of concrete in hydraulic structures
    • Lin B.Y. A recommendation on technical specification for abrasion and cavitation resistance of concrete in hydraulic structures. J Nanjing Hydraulic Res Inst 9 (1998) 8-13
    • (1998) J Nanjing Hydraulic Res Inst , vol.9 , pp. 8-13
    • Lin, B.Y.1
  • 13
    • 0030266390 scopus 로고    scopus 로고
    • Accelerated high speed water erosion test for concrete wear debris analysis
    • Momber A.W., and Kovacevic R. Accelerated high speed water erosion test for concrete wear debris analysis. Tibol Trans 39 (1996) 943-949
    • (1996) Tibol Trans , vol.39 , pp. 943-949
    • Momber, A.W.1    Kovacevic, R.2
  • 14
    • 0033083385 scopus 로고    scopus 로고
    • Short-time cavitation erosion of concrete, pre-cracked materials by acoustic emission
    • Momber A.W. Short-time cavitation erosion of concrete, pre-cracked materials by acoustic emission. Theor Appl Fract Mech 31 (1999) 1-17
    • (1999) Theor Appl Fract Mech , vol.31 , pp. 1-17
    • Momber, A.W.1
  • 15
    • 0035100037 scopus 로고    scopus 로고
    • Stress-strain relation for water-driven particle erosion of quasi-brittle materials
    • Momber A.W. Stress-strain relation for water-driven particle erosion of quasi-brittle materials. Theor Appl Fract Mech 35 (2001) 19-37
    • (2001) Theor Appl Fract Mech , vol.35 , pp. 19-37
    • Momber, A.W.1
  • 16
    • 33751535819 scopus 로고    scopus 로고
    • Effects of cement type, water/cement ratio and cement content on sea water resistance of concrete
    • Huseyin Y., Halit Y., and Serdar A. Effects of cement type, water/cement ratio and cement content on sea water resistance of concrete. Build Environ 42 (2007) 1770-1776
    • (2007) Build Environ , vol.42 , pp. 1770-1776
    • Huseyin, Y.1    Halit, Y.2    Serdar, A.3
  • 17
    • 54349109024 scopus 로고    scopus 로고
    • BS EN 196-2:2005, Methods of testing cement - Part 2: Chemical Analysis of cement and BS EN 196-1:2005, Methods of testing cement - Part 1: Determination of strength.
    • BS EN 196-2:2005, Methods of testing cement - Part 2: Chemical Analysis of cement and BS EN 196-1:2005, Methods of testing cement - Part 1: Determination of strength.
  • 18
    • 54349085746 scopus 로고    scopus 로고
    • EN TS 706. Turkish standard of concrete aggregate, Ankara; 1980 (in Turkish).
    • EN TS 706. Turkish standard of concrete aggregate, Ankara; 1980 (in Turkish).
  • 19
    • 54349115089 scopus 로고    scopus 로고
    • EN TS 802. Turkish standard of concrete mix design, Ankara; 1985 (in Turkish).
    • EN TS 802. Turkish standard of concrete mix design, Ankara; 1985 (in Turkish).
  • 20
    • 0037940220 scopus 로고    scopus 로고
    • Field indicator of chloride penetration depth
    • Meck E., and Sirivivatnanon V. Field indicator of chloride penetration depth. Cement Concrete Res 33 (2003) 1113-1117
    • (2003) Cement Concrete Res , vol.33 , pp. 1113-1117
    • Meck, E.1    Sirivivatnanon, V.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.