Volumn 60, Issue 2, 2009, Pages 104-107

Hot working characteristics of cobalt in the temperature range 600-950 °C

Author keywords

Cobalt; Compression; Dynamic recrystallization; Hot working; Strain rate sensitivity

Indexed keywords

COBALT; COMPRESSION TESTING; DATA COMPRESSION; DEFORMATION; DYNAMIC RECRYSTALLIZATION; METAL WORKING; RECRYSTALLIZATION (METALLURGY); SENSITIVITY ANALYSIS; STRAIN RATE; TRANSITION METALS;

EID: 54249158664     PISSN: 13596462     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.scriptamat.2008.09.012     Document Type: Article
Times cited : (41)