메뉴 건너뛰기




Volumn , Issue , 2005, Pages 245-268

Influence of the weld pool geometry on solidification crack formation

Author keywords

[No Author keywords available]

Indexed keywords


EID: 54249093932     PISSN: None     EISSN: None     Source Type: Book    
DOI: 10.1007/3-540-27460-X_13     Document Type: Chapter
Times cited : (15)

References (13)
  • 1
    • 1442331170 scopus 로고    scopus 로고
    • Hot cracking resistance of laser and hybrid welded austenitic stainless steels
    • Schobbert H, Böllinghaus Th, Wolf M (2003) Hot cracking resistance of laser and hybrid welded austenitic stainless steels. Trends in Welding Research 6: 76-81
    • (2003) Trends in Welding Research , vol.6 , pp. 76-81
    • Schobbert, H.1    Böllinghaus, Th.2    Wolf, M.3
  • 2
    • 0012351849 scopus 로고
    • The technological strength of metals while crystallizing during welding
    • Prokhorov N (1962) The technological strength of metals while crystallizing during welding. Welding Production 9(4): 1-8
    • (1962) Welding Production , vol.9 , Issue.4 , pp. 1-8
    • Prokhorov, N.1
  • 4
    • 0042862606 scopus 로고
    • Fundamental investigation on solidification structure in weld metal
    • Matsuda F, Hashimoto T, Senda (1969) Fundamental investigation on solidification structure in weld metal. Trans Nat Res Inst Metals 11: 43-58
    • (1969) Trans Nat Res Inst Metals , vol.11 , pp. 43-58
    • Matsuda, F.1    Senda, H.T.2
  • 7
    • 2442717936 scopus 로고    scopus 로고
    • A modified hot tearing criterion for steels
    • Rindler W et. al (2002) A Modified Hot Tearing Criterion for Steels. In: Mathematical Modelling of Weld Phenomena 6, pp 819-835
    • (2002) Mathematical Modelling of Weld Phenomena , vol.6 , pp. 819-835
  • 9
    • 84892243078 scopus 로고    scopus 로고
    • Interfacially driven mass transport in joining and coating technologies
    • (Book 692), The Royal Society, Cambridge
    • Olson DL, Edwards R (1998) Interfacially driven mass transport in joining and coating technologies. In: Marangoni and Interfacial Phenomena in Materials Processing (Book 692), The Royal Society, Cambridge, pp 113-126
    • (1998) Marangoni and Interfacial Phenomena in Materials Processing , pp. 113-126
    • Olson, D.L.1    Edwards, R.2
  • 10
    • 0000756710 scopus 로고
    • The varestraint test
    • prCEN ISO/TR 17641-3 Destructive tests on welds in metallic materials - Hot cracking tests for weldments - Part 3 - Externally loaded tests11 Savage W, Lundin C (1965) The Varestraint Test. Weld Res Suppl 10: 433-442
    • (1965) Weld Res Suppl , vol.10 , pp. 433-442
    • Savage W.Lundin, C.1
  • 11
    • 84892244121 scopus 로고
    • Versatile weld metal cracking test
    • Mc Keown D (1970) Versatile Weld Metal Cracking Test. Met Constr 8: 351-352
    • (1970) Met Constr , vol.8 , pp. 351-352
    • Mc Keown, D.1
  • 12
    • 0029725631 scopus 로고    scopus 로고
    • Weldability of commercial Al-Cu-Li alloys
    • Transtec Publications
    • Lippold J.C, Lin, W (1996) Weldability of commercial Al-Cu-Li alloys. In: Proc of ICAA5, Transtec Publications, pp 1685-1690
    • (1996) Proc of ICAA5 , pp. 1685-1690
    • Lippold, J.C.1    Lin, W.2
  • 13
    • 5844331086 scopus 로고
    • The MVT-Test - A novel procedure for testing of the hot cracking susceptibility during welding (in German)
    • Wilken K, Kleistner H (1982) The MVT-Test - A novel procedure for testing of the hot cracking susceptibility during welding (in German). Material und Technik 1: 3-10
    • (1982) Material und Technik , vol.1 , pp. 3-10
    • Wilken, K.1    Kleistner, H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.