Factors inducing intergranular fracture in nickel-free high nitrogen austenitic stainless steel produced by solution nitriding

Author keywords

Austenite; Deformation induced martensite; Dislocation pile up; Grain boundary segregation; High nitrogen steel; Impurity; Intergranular fracture; Planar dislocation array; Stress concentration

Indexed keywords

ALLOYS; AUSTENITE; AUSTENITIC STAINLESS STEEL; AUSTENITIC STEEL; BRITTLE FRACTURE; CHROMIUM; CONCENTRATION (PROCESS); CRYSTAL GROWTH; DEFORMATION; FRACTURE; FRACTURE FIXATION; GRAIN BOUNDARIES; GRAIN SIZE AND SHAPE; IMPURITIES; METALLIC COMPOUNDS; NICKEL; NITRIDING; NITROGEN; NONMETALS; STEEL CORROSION; STEEL METALLURGY; STRESS CONCENTRATION; TENSILE TESTING;

EID: 49749153428     PISSN: 09151559     EISSN: None     Source Type: Journal    
DOI: 10.2355/isijinternational.48.861     Document Type: Article
Times cited : (33)

References (22)
  • 7
    • 0003405397 scopus 로고    scopus 로고
    • Uptake of Nitrogen, High Nitrogen Steels - Structure, Properties, Application
    • Springer, Berlin, 203
    • V. G. Gavriljuk and H. Berns: Uptake of Nitrogen, High Nitrogen Steels - Structure, Properties, Application-, Springer, Berlin, (1999), 203.
    • (1999)
    • Gavriljuk, V.G.1    Berns, H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.