메뉴 건너뛰기




Volumn 91, Issue 7, 2008, Pages 2236-2242

Kinetics and mechanism of hot corrosion of γ-Y 2Si 2O 7 in thin-film Na 2SO 4 molten salt

Author keywords

[No Author keywords available]

Indexed keywords

APPARENT ACTIVATION ENERGIES; BARRIER COATINGS; CANDIDATE MATERIALS; CORROSION SCALE; GAS PRODUCTS; HIGH MELTING POINTS; HIGH TEMPERATURES; HOT CORROSIONS; KEY FACTORS; KINETIC CURVES; KINETICS AND MECHANISMS; LINEAR THERMAL EXPANSION COEFFICIENTS; LOW THERMAL CONDUCTIVITIES; MOLTEN SALTS; STRUCTURAL APPLICATIONS; THERMAL STABILITIES; THERMO-GRAVIMETRIC ANALYZERS; THIN SILICA FILMS; THIN-FILM;

EID: 49649108256     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2008.02439.x     Document Type: Article
Times cited : (34)

References (24)
  • 2
    • 0023406534 scopus 로고
    • Review, Relationships Between Processing, Microstructure and Properties of Dense and Reaction-Bonded Silicon Nitride
    • G. Ziegler, J. Neinrich, and G. Wötting, "Review, Relationships Between Processing, Microstructure and Properties of Dense and Reaction-Bonded Silicon Nitride," J. Mater. Sci., 22, 3041-86 (1987).
    • (1987) J. Mater. Sci , vol.22 , pp. 3041-3086
    • Ziegler, G.1    Neinrich, J.2    Wötting, G.3
  • 4
    • 0027282886 scopus 로고
    • Corrosion of Silicon-Based Ceramics in Combustion Environments
    • N. S. Jacobson, "Corrosion of Silicon-Based Ceramics in Combustion Environments," J. Am. Ceram. Soc., 76 [1] 3-28 (1993).
    • (1993) J. Am. Ceram. Soc , vol.76 , Issue.1 , pp. 3-28
    • Jacobson, N.S.1
  • 5
    • 0023964038 scopus 로고
    • Molten-Salt Corrosion of Silicon Nitride: 1, Sodium Carbonate
    • N. S. Jacobson and D. Fox, "Molten-Salt Corrosion of Silicon Nitride: 1, Sodium Carbonate," J. Am. Ceram. Soc., 71 [2] 128-38 (1988).
    • (1988) J. Am. Ceram. Soc , vol.71 , Issue.2 , pp. 128-138
    • Jacobson, N.S.1    Fox, D.2
  • 7
    • 18844447781 scopus 로고    scopus 로고
    • Thermal Barrier Coating Materials
    • D. R. Clarke and S. R. Phillpot, "Thermal Barrier Coating Materials," Mater. Today, 8 [6] 22-9 (2005).
    • (2005) Mater. Today , vol.8 , Issue.6 , pp. 22-29
    • Clarke, D.R.1    Phillpot, S.R.2
  • 8
    • 0031118047 scopus 로고    scopus 로고
    • High Temperature Strength and Oxidation Behavior of Hot Pressed Silicon Nitride-Disilicate Ceramics
    • H. J. Choi, J. G. Lee, and Y. W. Kim, "High Temperature Strength and Oxidation Behavior of Hot Pressed Silicon Nitride-Disilicate Ceramics," J. Mater. Sci., 32, 1937-42 (1997).
    • (1997) J. Mater. Sci , vol.32 , pp. 1937-1942
    • Choi, H.J.1    Lee, J.G.2    Kim, Y.W.3
  • 10
    • 0001524703 scopus 로고
    • Synthesis and Study of Yttrialite
    • J. Ito and H. Johnson, "Synthesis and Study of Yttrialite," Am. Mineral., 53, 1940-52 (1968).
    • (1968) Am. Mineral , vol.53 , pp. 1940-1952
    • Ito, J.1    Johnson, H.2
  • 12
    • 0002654927 scopus 로고
    • The Crystal Chemistry of Rare-Earth Silicates
    • J. Feslche, "The Crystal Chemistry of Rare-Earth Silicates," Struct. Bonding, 13, 99-197 (1973).
    • (1973) Struct. Bonding , vol.13 , pp. 99-197
    • Feslche, J.1
  • 14
    • 34547681889 scopus 로고    scopus 로고
    • 7: A Novel Machinable Silicate Ceramics, Mechanical Properties and Machinability
    • 7: A Novel Machinable Silicate Ceramics, Mechanical Properties and Machinability," J. Am. Ceram. Soc., 90 [8] 2535-41 (2007).
    • (2007) J. Am. Ceram. Soc , vol.90 , Issue.8 , pp. 2535-2541
    • Sun, Z.Q.1    Zhou, Y.C.2    Li, M.S.3    Wang, J.Y.4
  • 15
    • 0023960583 scopus 로고
    • Molten-Salt Corrosion of Silicon Nitride: 2, Sodium Sulfate
    • N. S. Jacobson and D. Fox, "Molten-Salt Corrosion of Silicon Nitride: 2, Sodium Sulfate," J. Am. Ceram. Soc., 71 [2] 139-48 (1988).
    • (1988) J. Am. Ceram. Soc , vol.71 , Issue.2 , pp. 139-148
    • Jacobson, N.S.1    Fox, D.2
  • 16
    • 0022506399 scopus 로고
    • Kinetics andMechanism of Corrosion SiC byMolten Salts
    • N. S. Jacobson, "Kinetics andMechanism of Corrosion SiC byMolten Salts," J. Am. Ceram. Soc., 69 [1] 74-82 (1986).
    • (1986) J. Am. Ceram. Soc , vol.69 , Issue.1 , pp. 74-82
    • Jacobson, N.S.1
  • 17
    • 0036466923 scopus 로고    scopus 로고
    • Hot-Corrosion of Material: A Fluxing Mechanism
    • R. A. Rapp, "Hot-Corrosion of Material: A Fluxing Mechanism," Corros. Sci., 44, 209-21 (2002).
    • (2002) Corros. Sci , vol.44 , pp. 209-221
    • Rapp, R.A.1
  • 19
    • 3142693710 scopus 로고    scopus 로고
    • Phase Equilibria Diagrams
    • V3.0.1, ACS, Westervill, OH, Fig. 09202
    • ACerS-NIST Phase Equilibria Diagrams, CD-ROM Database, V3.0.1, ACS, Westervill, OH, Fig. 09202.
    • CD-ROM Database
    • ACerS-NIST1
  • 20
    • 3142693710 scopus 로고    scopus 로고
    • Phase Equilibria Diagrams
    • V3.0.1, ACS, Westervill, OH, Fig. 10022
    • ACerS-NIST Phase Equilibria Diagrams, CD-ROM Database, V3.0.1, ACS, Westervill, OH, Fig. 10022.
    • CD-ROM Database
    • ACerS-NIST1
  • 23
    • 0038246560 scopus 로고
    • Fluxing Mechanism of Hot Corrosion and its Limitation
    • in Chinese
    • Y. S. Zhang, "Fluxing Mechanism of Hot Corrosion and its Limitation," J. Chinese Soc. Corros. Protect., 12 [1] 1-10 (1992) (in Chinese).
    • (1992) J. Chinese Soc. Corros. Protect , vol.12 , Issue.1 , pp. 1-10
    • Zhang, Y.S.1
  • 24
    • 29744461202 scopus 로고    scopus 로고
    • Hot Corrosion Mechanism of Composite Alumina/Yttria-Stablized Zirconia Coating in Molten Sulfate-Vanadate Salt
    • N. Wu, Z. Chen, and S. X. Mao, "Hot Corrosion Mechanism of Composite Alumina/Yttria-Stablized Zirconia Coating in Molten Sulfate-Vanadate Salt," J. Am. Ceram. Soc., 88 [3] 675-82 (2005).
    • (2005) J. Am. Ceram. Soc , vol.88 , Issue.3 , pp. 675-682
    • Wu, N.1    Chen, Z.2    Mao, S.X.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.