Long-term performance of cables based on chlorosulphonated polyethylene

Author keywords

25 years ageing; Accelerated ageing; Cable; Chlorosulphonated polyethylene; Extrapolation

Indexed keywords

ACCELERATION; CROSSLINKING; DATA REDUCTION; ELASTIC MODULI; EXTRAPOLATION; NUCLEAR POWER PLANTS; POLYVINYL CHLORIDES; PYROLYSIS; TENSILE TESTING;

EID: 4944256265     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2004.02.017     Document Type: Article
Times cited : (11)

References (16)
  • 1
    • 0001404806 scopus 로고
    • Mark H.F., Bikales N., Overberger C.G., Menges G., Kroschwitz J.I., New York: Wiley
    • Clough R.L., Gillen K.T. Mark H.F., Bikales N., Overberger C.G., Menges G., Kroschwitz J.I. Encyclopedia of Polymer Science and Engineering. 13: 1988;667 Wiley, New York.
    • (1988) Encyclopedia of Polymer Science and Engineering , vol.13 , pp. 667
    • Clough, R.L.1    Gillen, K.T.2
  • 16
    • 4944219771 scopus 로고    scopus 로고
    • Stockholm, Sweden: aging of electrical components in nuclear power plants: relationships between mechanical and chemical degradation after artificial aging and dielectric behaviour during LOCA
    • Spång K, SKI report H-14008-C Swedish Nuclear Power Inspectorate, Stockholm, Sweden: aging of electrical components in nuclear power plants: relationships between mechanical and chemical degradation after artificial aging and dielectric behaviour during LOCA, 1997.
    • (1997) SKI Report H-14008-C Swedish Nuclear Power Inspectorate
    • Spång, K.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.