Volumn 37, Issue 19, 2004, Pages 7123-7131

A new route to organoboron polymers via highly selective polymer modification reactions

Author keywords

[No Author keywords available]

Indexed keywords

EXCHANGE REACTIONS; LEWIS ACIDS; ORGANOBORON POLYMERS; POLYMER MODIFICATION REACTIONS;

EID: 4744364056     PISSN: 00249297     EISSN: None     Source Type: Journal    
DOI: 10.1021/ma035880r     Document Type: Article
Times cited : (93)

References (116)
  • 8
    • 0000945374 scopus 로고
    • See for example: (a) Roberts, M. F.; Jenekhe, S. A.; Cameron, A.; Mcmillan, M.; Perlstein, J. Chem. Mater. 1994, 6, 658-670. (b) Connolly, J. W.; Dudis, D. S.; Kumar, S.; Gelbaum, L. T.; Venkatasubramanian, N. Chem. Mater. 1996, 8, 54-59. (c) Genoud, F.; Kulszewicz-Bajer, I.; Bedel, A.; Oddou, J.-L.; Jeandey, C.; Pron, A. Chem. Mater. 2000, 12, 744-749.
    • (1994) J. Chem. Mater. , vol.6 , pp. 658-670
    • Roberts, M.F.1    Jenekhe, S.A.2    Cameron, A.3    Mcmillan, M.4    Perlstein5
  • 9
    • 0002177403 scopus 로고    scopus 로고
    • See for example: (a) Roberts, M. F.; Jenekhe, S. A.; Cameron, A.; Mcmillan, M.; Perlstein, J. Chem. Mater. 1994, 6, 658-670. (b) Connolly, J. W.; Dudis, D. S.; Kumar, S.; Gelbaum, L. T.; Venkatasubramanian, N. Chem. Mater. 1996, 8, 54-59. (c) Genoud, F.; Kulszewicz-Bajer, I.; Bedel, A.; Oddou, J.-L.; Jeandey, C.; Pron, A. Chem. Mater. 2000, 12, 744-749.
    • (1996) Chem. Mater. , vol.8 , pp. 54-59
    • Connolly, J.W.1    Dudis, D.S.2    Kumar, S.3    Gelbaum, L.T.4    Venkatasubramanian, N.5
  • 10
    • 0033802998 scopus 로고    scopus 로고
    • See for example: (a) Roberts, M. F.; Jenekhe, S. A.; Cameron, A.; Mcmillan, M.; Perlstein, J. Chem. Mater. 1994, 6, 658-670. (b) Connolly, J. W.; Dudis, D. S.; Kumar, S.; Gelbaum, L. T.; Venkatasubramanian, N. Chem. Mater. 1996, 8, 54-59. (c) Genoud, F.; Kulszewicz-Bajer, I.; Bedel, A.; Oddou, J.-L.; Jeandey, C.; Pron, A. Chem. Mater. 2000, 12, 744-749.
    • (2000) Chem. Mater. , vol.12 , pp. 744-749
    • Genoud, F.1    Kulszewicz-Bajer, I.2    Bedel, A.3    Oddou, J.-L.4    Jeandey, C.5    Pron, A.6
  • 41
    • 0036497922 scopus 로고    scopus 로고
    • (f) Keller, T. M. Carbon 2002, 40, 225-229.
    • (2002) Carbon , vol.40 , pp. 225-229
    • Keller, T.M.1
  • 70
    • 0034229155 scopus 로고    scopus 로고
    • w = 90 700) and polydispersity (PDI = 1.33) has been synthesized via ATRP with a different ligand system, but a kinetic analysis has not been reported: (a) McQuillan, B. W.; Paguio, S. Fusion Technol. 2000, 38, 108-109; for the nitroxide-mediated polymerization of 4-trimethylsilystyrene see: (b) David-Quillot, F.; Duchêne, A.; Catala, J.-M.; Balland-Longeau, A. Fusion Sci. Technol. 2002, 41, 253-256.
    • (2000) Fusion Technol. , vol.38 , pp. 108-109
    • McQuillan, B.W.1    Paguio, S.2
  • 71
    • 0036565159 scopus 로고    scopus 로고
    • w = 90 700) and polydispersity (PDI = 1.33) has been synthesized via ATRP with a different ligand system, but a kinetic analysis has not been reported: (a) McQuillan, B. W.; Paguio, S. Fusion Technol. 2000, 38, 108-109; for the nitroxide-mediated polymerization of 4-trimethylsilystyrene see: (b) David-Quillot, F.; Duchêne, A.; Catala, J.-M.; Balland-Longeau, A. Fusion Sci. Technol. 2002, 41, 253-256.
    • (2002) Fusion Sci. Technol. , vol.41 , pp. 253-256
    • David-Quillot, F.1    Duchêne, A.2    Catala, J.-M.3    Balland-Longeau, A.4
  • 74
    • 0031237343 scopus 로고    scopus 로고
    • see also refs 21 and 22
    • A comparison with kinetic data for the polymerization of styrene under similar conditions shows that 4-trimethyl-silylstyrene polymerizes at a faster rate. See: Qiu, J.; Matyjaszewski, K. Macromolecules 1997, 30, 5643-5648; see also refs 21 and 22.
    • (1997) Macromolecules , vol.30 , pp. 5643-5648
    • Qiu, J.1    Matyjaszewski, K.2
  • 75
    • 0030662031 scopus 로고    scopus 로고
    • A slow elimination of HBr has been observed experimentally in the ATRP of styrene in solution, and the kinetics for this process have been simulated. See: (a) Matyjaszewski, K.; Davis, K.; Patten, T. E.; Wei, M. Tetrahedron 1997, 53, 15321-15329. (b) Matyjaszewski, K.; Patten, T. E.; Xia, J. J. Am. Chem. Soc. 1997, 119, 674-680. Lutz, J.-F. Matyjaszewski, K. Macromol. Chem. Phys. 2002, 203, 1385-1395.
    • (1997) Tetrahedron , vol.53 , pp. 15321-15329
    • Matyjaszewski, K.1    Davis, K.2    Patten, T.E.3    Wei, M.4
  • 76
    • 0031040483 scopus 로고    scopus 로고
    • A slow elimination of HBr has been observed experimentally in the ATRP of styrene in solution, and the kinetics for this process have been simulated. See: (a) Matyjaszewski, K.; Davis, K.; Patten, T. E.; Wei, M. Tetrahedron 1997, 53, 15321-15329. (b) Matyjaszewski, K.; Patten, T. E.; Xia, J. J. Am. Chem. Soc. 1997, 119, 674-680. Lutz, J.-F. Matyjaszewski, K. Macromol. Chem. Phys. 2002, 203, 1385-1395.
    • (1997) J. Am. Chem. Soc. , vol.119 , pp. 674-680
    • Matyjaszewski, K.1    Patten, T.E.2    Xia, J.3
  • 77
    • 0037194023 scopus 로고    scopus 로고
    • A slow elimination of HBr has been observed experimentally in the ATRP of styrene in solution, and the kinetics for this process have been simulated. See: (a) Matyjaszewski, K.; Davis, K.; Patten, T. E.; Wei, M. Tetrahedron 1997, 53, 15321-15329. (b) Matyjaszewski, K.; Patten, T. E.; Xia, J. J. Am. Chem. Soc. 1997, 119, 674-680. Lutz, J.-F. Matyjaszewski, K. Macromol. Chem. Phys. 2002, 203, 1385-1395.
    • (2002) Macromol. Chem. Phys. , vol.203 , pp. 1385-1395
    • Lutz, J.-F.1    Matyjaszewski, K.2
  • 79
    • 0035781101 scopus 로고    scopus 로고
    • (b) Fischer, H. Chem. Rev. 2001, 101, 3581-3610.
    • (2001) Chem. Rev. , vol.101 , pp. 3581-3610
    • Fischer, H.1
  • 83
    • 4744351473 scopus 로고    scopus 로고
    • note
    • Preliminary studies in our laboratory indicate that poly(4- trimethylsilylstyrene) can be extended with styrene to give block copolymers; these results will be reported elsewhere.
  • 85
  • 86
    • 4744348887 scopus 로고    scopus 로고
    • note
    • n = 5000 to 30 000). However, the polymer modification reactions proceed generally more slowly than the analogous reactions with molecular model compounds.
  • 88
    • 4744362194 scopus 로고    scopus 로고
    • note
    • The polymers PS-BOEt and PS-BOBu are somewhat hydrolytically sensitive. Exposure to wet solvents leads to varying amounts of cross-linked materials. However, even partially cross-linked material readily redissolves upon treatment with pinacol to yield the air-stable polymer PS-BPin. Thermogravimetric analysis (TGA) showed also high thermal stability of PS-BPin up to temperatures of ca. 360°C.
  • 97
    • 4744374028 scopus 로고    scopus 로고
    • note
    • The amount of incorporated thiophene was estimated to an average of 3 units per polymer by sulfur elemental analysis.
  • 104
    • 4744372645 scopus 로고    scopus 로고
    • note
    • GPC data for polymers PS-BBr, PS-BTh, and PS-BPf could not be obtained because the polymers do not elute from the separation columns.
  • 106
    • 0038337748 scopus 로고    scopus 로고
    • For a related dendritic system decorated with up to 12 (perfluoroaryl)borane Lewis acid centers, see: Roesler, R.; Har, B. J. N.; Piers, W. E. Organometallics 2002, 21, 4300-4302.
    • (2002) Organometallics , vol.21 , pp. 4300-4302
    • Roesler, R.1    Har, B.J.N.2    Piers, W.E.3
  • 107
    • 2642648668 scopus 로고    scopus 로고
    • For the use of polymeric borates as catalyst components see, for example: (a) Roscoe, S. B.; Fréchet, J. M. J.; Walzer, J. F.; Dias, A. J. Science 1998, 280, 270-273. (b) Mager, M.; Becke, S.; Windisch, H.; Denninger, U. Angew. Chem., Int. Ed. 2001, 40, 1898-1902. (c) Turner, H. W. Exxon Chemical Patents Inc.: US, 1995; US 5427991. (d) Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663. (e) Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225.
    • (1998) Science , vol.280 , pp. 270-273
    • Roscoe, S.B.1    Fréchet, J.M.J.2    Walzer, J.F.3    Dias, A.J.4
  • 108
    • 0035906944 scopus 로고    scopus 로고
    • For the use of polymeric borates as catalyst components see, for example: (a) Roscoe, S. B.; Fréchet, J. M. J.; Walzer, J. F.; Dias, A. J. Science 1998, 280, 270-273. (b) Mager, M.; Becke, S.; Windisch, H.; Denninger, U. Angew. Chem., Int. Ed. 2001, 40, 1898-1902. (c) Turner, H. W. Exxon Chemical Patents Inc.: US, 1995; US 5427991. (d) Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663. (e) Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225.
    • (2001) Angew. Chem., Int. Ed. , vol.40 , pp. 1898-1902
    • Mager, M.1    Becke, S.2    Windisch, H.3    Denninger, U.4
  • 109
    • 2642648668 scopus 로고    scopus 로고
    • Exxon Chemical Patents Inc.: US; US 5427991
    • For the use of polymeric borates as catalyst components see, for example: (a) Roscoe, S. B.; Fréchet, J. M. J.; Walzer, J. F.; Dias, A. J. Science 1998, 280, 270-273. (b) Mager, M.; Becke, S.; Windisch, H.; Denninger, U. Angew. Chem., Int. Ed. 2001, 40, 1898-1902. (c) Turner, H. W. Exxon Chemical Patents Inc.: US, 1995; US 5427991. (d) Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663. (e) Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225.
    • (1995)
    • Turner, H.W.1
  • 110
    • 2642648668 scopus 로고    scopus 로고
    • Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663
    • For the use of polymeric borates as catalyst components see, for example: (a) Roscoe, S. B.; Fréchet, J. M. J.; Walzer, J. F.; Dias, A. J. Science 1998, 280, 270-273. (b) Mager, M.; Becke, S.; Windisch, H.; Denninger, U. Angew. Chem., Int. Ed. 2001, 40, 1898-1902. (c) Turner, H. W. Exxon Chemical Patents Inc.: US, 1995; US 5427991. (d) Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663. (e) Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225.
  • 111
    • 2642648668 scopus 로고    scopus 로고
    • Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225
    • For the use of polymeric borates as catalyst components see, for example: (a) Roscoe, S. B.; Fréchet, J. M. J.; Walzer, J. F.; Dias, A. J. Science 1998, 280, 270-273. (b) Mager, M.; Becke, S.; Windisch, H.; Denninger, U. Angew. Chem., Int. Ed. 2001, 40, 1898-1902. (c) Turner, H. W. Exxon Chemical Patents Inc.: US, 1995; US 5427991. (d) Ono, M.; Hinokuma, S.; Miyake, S.; Inazawa, S. Japan Polyolefins Co., Ltd.: BE, DE, FR, GB, IT, NL, 1996, EP 710663. (e) Kanamaru, M.; Okamoto, T.; Okuda, F.; Kamisawa, M.; Idemitsu Petro-chemical Co., Ltd.: Japan, 2000; JP 2000212225.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.