Volumn 130, Issue 2, 2008, Pages 0217061-0217067

Analysis of laminations in X52 steel pipes by nonlinear by finite element

Author keywords

[No Author keywords available]

Indexed keywords

FINITE ELEMENT METHOD; GAS PIPELINES; HYDROGEN; IRON; NONMETALS; PIPE; PIPELINES; RELIABILITY; SOUR GAS; STEEL; STEEL PIPE; STRESSES;

EID: 47149097843     PISSN: 00949930     EISSN: None     Source Type: Journal    
DOI: 10.1115/1.2894295     Document Type: Article
Times cited : (6)

References (9)
  • 1
    • 0019031617 scopus 로고
    • Effects of Hydrogen on the Properties of Iron and Steel
    • Hirth, J., 1980, "Effects of Hydrogen on the Properties of Iron and Steel," Metall. Trans. A, 11A, pp. 861-890.
    • (1980) Metall. Trans. A , vol.11 A , pp. 861-890
    • Hirth, J.1
  • 2
    • 11144346835 scopus 로고    scopus 로고
    • Mecánica de Fractura en Ductos de Recolección y Transporte de Hidrocarburos
    • México
    • Velázquez, J. L. G., and Hallen, J. M., 1998, Mecánica de Fractura en Ductos de Recolección y Transporte de Hidrocarburos, 3er Congreso de Ductos PEMEX, México, 1, pp. 183-191.
    • (1998) 3er Congreso de Ductos PEMEX , vol.1 , pp. 183-191
    • Velázquez, J.L.G.1    Hallen, J.M.2
  • 3
    • 34547494519 scopus 로고
    • Formation and Analysis of Stack Cracks in Pipeline Steel
    • Zacaria, M. Y. B., and Davies, T. T., 1993, "Formation and Analysis of Stack Cracks in Pipeline Steel," J. Mater. Sci., 28, pp. 322-328.
    • (1993) J. Mater. Sci , vol.28 , pp. 322-328
    • Zacaria, M.Y.B.1    Davies, T.T.2
  • 4
    • 0018039594 scopus 로고
    • The Extension of Hydrogen Blister-Crack Array in Line Pipe Steels
    • Makkio, Iino, 1978, "The Extension of Hydrogen Blister-Crack Array in Line Pipe Steels," Metall. Trans. A, 9A, pp. 1581-1590.
    • (1978) Metall. Trans. A , vol.9 A , pp. 1581-1590
    • Makkio, I.1
  • 5
    • 0032629991 scopus 로고    scopus 로고
    • The Interaction of Two Parallel Semi-Elliptical Surface Cracks Under Tension and Bending
    • Moussa, W. A., Bell, R., and Tan, C. L., 1999, "The Interaction of Two Parallel Semi-Elliptical Surface Cracks Under Tension and Bending," ASME J. Pressure Vessel Technol., 121, pp. 323-326.
    • (1999) ASME J. Pressure Vessel Technol , vol.121 , pp. 323-326
    • Moussa, W.A.1    Bell, R.2    Tan, C.L.3
  • 6
    • 34547532706 scopus 로고    scopus 로고
    • Hydrogen-Induced Crack Growth Rate in Steel Plates Exposed to Sour Environment
    • González, J. L., Ramírez, R., and Hallen, J. M., 1997, "Hydrogen-Induced Crack Growth Rate in Steel Plates Exposed to Sour Environment," Corros. Sci., 53, pp. 12-21.
    • (1997) Corros. Sci , vol.53 , pp. 12-21
    • González, J.L.1    Ramírez, R.2    Hallen, J.M.3
  • 8
    • 47149086897 scopus 로고    scopus 로고
    • Theory Reference-Ansys, 2001, Structures with Material Nonlinearities, SAS IP Inc.
    • Theory Reference-Ansys, 2001, Structures with Material Nonlinearities, SAS IP Inc.
  • 9
    • 11144328754 scopus 로고    scopus 로고
    • On the Hydrogen Induced Cracking of Pipeline Steel Under Wet Hydrogen Sulfide Environment
    • Ikeda, A., and Morita, Y., 1997, "On the Hydrogen Induced Cracking of Pipeline Steel Under Wet Hydrogen Sulfide Environment," Second International Congress of Hydrogen in Metals.
    • (1997) Second International Congress of Hydrogen in Metals
    • Ikeda, A.1    Morita, Y.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.