Textures and mechanical behavior of Mg-3.3%Li alloy after ECAP

Author keywords

Equal channel angular pressing; Magnesium alloy; Mechanical properties; Recrystallization; Texture

Indexed keywords

CRYSTALLIZATION; MAGNESIUM ALLOYS; MICROSTRUCTURE; NEUTRON DIFFRACTION; SHEAR STRESS; SINGLE CRYSTALS; STRAIN; TEXTURES; TRANSMISSION ELECTRON MICROSCOPY;