Volumn 145, Issue 3, 2004, Pages 155-162
|
Nickel particles prepared from nickel nitrate with and without urea by spray pyrolysis
|
Author keywords
Crystallization; Nickel particles; Reduction; Sintering; Spray pyrolysis; Urea
|