메뉴 건너뛰기




Volumn 86, Issue 1, 2008, Pages 41-47

Wear-corrosion performance of Si-DLC coatings on Ti-6A1-4V substrate

Author keywords

Biomaterial; Corrosion; DLC; Ti; Wear

Indexed keywords

BENZENE; CARBON; CHEMICAL VAPOR DEPOSITION; COATINGS; DIAMONDS; ELECTRIC LOAD MANAGEMENT; METALLIZING; PLASMA DEPOSITION; PULSED LASER DEPOSITION; SILICON; SILICON ALLOYS; THIN FILMS; TITANIUM ALLOYS;

EID: 44849099238     PISSN: 15493296     EISSN: 15524965     Source Type: Journal    
DOI: 10.1002/jbm.a.31632     Document Type: Article
Times cited : (27)

References (16)
  • 1
    • 1242272814 scopus 로고    scopus 로고
    • Gucombining double acute accentleryucombining double acute accentz H, Çimenoǧlu H. Effect of thermal oxidation on corrosion and corrosion-wear behavior of a Ti-6A1-4V alloy. Biomaterials 2004;25:3325-3333.
    • Gucombining double acute accentleryucombining double acute accentz H, Çimenoǧlu H. Effect of thermal oxidation on corrosion and corrosion-wear behavior of a Ti-6A1-4V alloy. Biomaterials 2004;25:3325-3333.
  • 2
    • 0024000360 scopus 로고
    • Measurement of erosion-corrosion synergism with a slurry wear test apparatus
    • Madsen BW. Measurement of erosion-corrosion synergism with a slurry wear test apparatus. Wear 1988;123:127-142.
    • (1988) Wear , vol.123 , pp. 127-142
    • Madsen, B.W.1
  • 3
    • 0030385093 scopus 로고    scopus 로고
    • Characterization of synergistic effects between erosion and corrosion in an aqueous environment using electrochemical techniques
    • Zhou S, Stack MM, Newman RC. Characterization of synergistic effects between erosion and corrosion in an aqueous environment using electrochemical techniques. Corrosion 1996;52:934-946.
    • (1996) Corrosion , vol.52 , pp. 934-946
    • Zhou, S.1    Stack, M.M.2    Newman, R.C.3
  • 5
    • 17644394245 scopus 로고    scopus 로고
    • TiN and Ti-O/TiN films fabricated by PIII-D for enhance-ment of corrosion and wear resistance of Ti-6A1-4V
    • Wan GJ, Huang N, Leng YX, Yang P, Chen JY, Wang J, Sun H. TiN and Ti-O/TiN films fabricated by PIII-D for enhance-ment of corrosion and wear resistance of Ti-6A1-4V. Surf Coat Technol 2004;186:136-140.
    • (2004) Surf Coat Technol , vol.186 , pp. 136-140
    • Wan, G.J.1    Huang, N.2    Leng, Y.X.3    Yang, P.4    Chen, J.Y.5    Wang, J.6    Sun, H.7
  • 6
    • 1842560233 scopus 로고    scopus 로고
    • Applications of plasma coating in artificial joints: An overview
    • Liang H, Shi B, Fairchild A, Cale T. Applications of plasma coating in artificial joints: An overview. Vacuum 2004;73:317-326.
    • (2004) Vacuum , vol.73 , pp. 317-326
    • Liang, H.1    Shi, B.2    Fairchild, A.3    Cale, T.4
  • 7
    • 0035449379 scopus 로고    scopus 로고
    • Triboelectrochemical investigation of the friction and wear behaviour of TiN coating in a neutral solution
    • Barril S, Mischler S, Landolt D. Triboelectrochemical investigation of the friction and wear behaviour of TiN coating in a neutral solution. Tribol Int 2001;34:599-608.
    • (2001) Tribol Int , vol.34 , pp. 599-608
    • Barril, S.1    Mischler, S.2    Landolt, D.3
  • 8
    • 0034310618 scopus 로고    scopus 로고
    • Deposition of Si-DLC films with high hardness, low stress and high deposition rates
    • Damasceno JC, Camargo SS Jr, Freire FL Jr, Carius R. Deposition of Si-DLC films with high hardness, low stress and high deposition rates. Surf Coat Technol 2000;133:247-252.
    • (2000) Surf Coat Technol , vol.133 , pp. 247-252
    • Damasceno, J.C.1    Camargo Jr, S.S.2    Freire Jr, F.L.3    Carius, R.4
  • 9
    • 17644372716 scopus 로고    scopus 로고
    • Effect of Si-incorporation on wear-corrosion properties of diamond-like carbon films
    • Kim HG, Ahn SH, Kim JG, Park SJ, Lee KR. Effect of Si-incorporation on wear-corrosion properties of diamond-like carbon films. Thin Solid Films 2005;482:299-304.
    • (2005) Thin Solid Films , vol.482 , pp. 299-304
    • Kim, H.G.1    Ahn, S.H.2    Kim, J.G.3    Park, S.J.4    Lee, K.R.5
  • 12
    • 0031245446 scopus 로고    scopus 로고
    • Structural dependence of mechanical properties of Si incorporated diamond-like carbon films deposited by RF plasma-assisted chemical vapour deposition
    • Lee KR, Kim MG, Cho SJ, Eun KY, Seong TY. Structural dependence of mechanical properties of Si incorporated diamond-like carbon films deposited by RF plasma-assisted chemical vapour deposition. Thin Solid Films 1997;308:263-267.
    • (1997) Thin Solid Films , vol.308 , pp. 263-267
    • Lee, K.R.1    Kim, M.G.2    Cho, S.J.3    Eun, K.Y.4    Seong, T.Y.5
  • 13
    • 84860818879 scopus 로고
    • Standard Practice for Calculation of Corrosion Rates and Related Information from Electrochemical Measurements
    • ASTM Standard G102-90, Philadelphia, PA: American Society for Testing and Materials;
    • ASTM Standard G102-90. Standard Practice for Calculation of Corrosion Rates and Related Information from Electrochemical Measurements, Annual Book of ASTM Standards. Philadelphia, PA: American Society for Testing and Materials; 1994.
    • (1994) Annual Book of ASTM Standards
  • 14
    • 0011647536 scopus 로고    scopus 로고
    • Aqueous corrosion behavior of weathering steel and carbon steel in acid-chloride environments
    • Choi YS, Kim JG. Aqueous corrosion behavior of weathering steel and carbon steel in acid-chloride environments. Corrosion 2000;56:1202-1210.
    • (2000) Corrosion , vol.56 , pp. 1202-1210
    • Choi, Y.S.1    Kim, J.G.2
  • 15
    • 0027667571 scopus 로고
    • Determination of coating deterioration with EIS, Part 2: Development of a method for field testing of protective coatings
    • Tsai CH, Mansfeld F. Determination of coating deterioration with EIS, Part 2: Development of a method for field testing of protective coatings. Corrosion 1993;49:726-737.
    • (1993) Corrosion , vol.49 , pp. 726-737
    • Tsai, C.H.1    Mansfeld, F.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.