Correlation between ultrasonic velocity and indentation-based mechanical properties with microstructure in Nimonic 263
|
Author keywords
Ageing; Ball indentation; Intermetallic precipitation; Mechanical properties; Nimonic 263; Ultrasonic velocity
|