메뉴 건너뛰기




Volumn 13, Issue 4, 2004, Pages 421-430

Diamond-coated cutting tools for biomedical applications

Author keywords

Biomedical applications; CVD diamond; Dental burs; Microtools; Wear

Indexed keywords

BIOMEDICAL APPLICATIONS; CVD DIAMONDS; DENTAL BURS; MICROTOOLS; WEAR;

EID: 4344588344     PISSN: 10599495     EISSN: None     Source Type: Journal    
DOI: 10.1361/1059949041848819     Document Type: Conference Paper
Times cited : (17)

References (36)
  • 2
    • 0026360656 scopus 로고
    • Mechanical applications of thin and thick diamond films
    • M. Murakawa and S. Takeuchi: "Mechanical Applications of Thin and Thick Diamond Films,"Surf. Coat. Technol., 1991, 49, pp. 359-64.
    • (1991) Surf. Coat. Technol. , vol.49 , pp. 359-364
    • Murakawa, M.1    Takeuchi, S.2
  • 3
    • 0026833177 scopus 로고
    • Practical properties of chemical vapour deposition diamond tools
    • T. Yaskiki, T. Nakamura, N. Fujimori, and T. Nakai: "Practical Properties of Chemical Vapour Deposition Diamond Tools,"Surf. Coat. Technol., 1992, 52, pp. 81-85.
    • (1992) Surf. Coat. Technol. , vol.52 , pp. 81-85
    • Yaskiki, T.1    Nakamura, T.2    Fujimori, N.3    Nakai, T.4
  • 4
    • 0027578321 scopus 로고
    • Chemically vapor deposited diamond as a cutting tool material - A study of failure mechanisms
    • J. Reineck, S. Soderbery, P. Eckholm, and K. Westergren: "Chemically Vapor Deposited Diamond as a Cutting Tool Material - A Study of Failure Mechanisms,"Surf. Coat. Technol., 1993, 57, pp. 47-50.
    • (1993) Surf. Coat. Technol. , vol.57 , pp. 47-50
    • Reineck, J.1    Soderbery, S.2    Eckholm, P.3    Westergren, K.4
  • 5
    • 0027568723 scopus 로고
    • Implementation of large-scale deposition of diamond films by combustion synthesis
    • H.-Z. Wang, R.-H. Song, and S.-P. Tang: "Implementation of Large-Scale Deposition of Diamond Films by Combustion Synthesis,"Diam. Relat. Mater., 1993, 2, pp. 304-10.
    • (1993) Diam. Relat. Mater. , vol.2 , pp. 304-310
    • Wang, H.-Z.1    Song, R.-H.2    Tang, S.-P.3
  • 6
    • 0028671123 scopus 로고
    • Superhard coatings for metal cutting applications
    • A. Inspector, C.E. Bauer, and E.J. Oles: "Superhard Coatings for Metal Cutting Applications,"Surf. Coat. Technol., 1994, 68/69, pp. 359-68.
    • (1994) Surf. Coat. Technol. , vol.68-69 , pp. 359-368
    • Inspector, A.1    Bauer, C.E.2    Oles, E.J.3
  • 7
    • 0004076374 scopus 로고
    • R.E. Clausing, L.L. Horton, J.C. Angus, and P. Koidl, ed., Plenum Press, New York
    • B. Lux and R. Haubner; Diamond and Diamond-Like Films and Coatings, R.E. Clausing, L.L. Horton, J.C. Angus, and P. Koidl, ed., Plenum Press, New York, 1991, NATO-ISI Series B, Physics, 265, p. 579.
    • (1991) Diamond and Diamond-like Films and Coatings
    • Lux, B.1    Haubner, R.2
  • 8
    • 4344677244 scopus 로고    scopus 로고
    • B. Lux and R. Haubner; Diamond and Diamond-Like Films and Coatings, R.E. Clausing, L.L. Horton, J.C. Angus, and P. Koidl, ed., Plenum Press, New York, 1991, NATO-ISI Series B, Physics, 265, p. 579.
    • NATO-ISI Series B, Physics , vol.265 , pp. 579
  • 9
    • 36449000665 scopus 로고
    • Effect of the chemical nature of transition-metal substrates on chemical-vapor deposition of diamond
    • X. Chen and J. Narayan: "Effect of the Chemical Nature of Transition-Metal Substrates on Chemical-Vapor Deposition of Diamond,"J. Appl. Phys., 1993, 74, p.1468.
    • (1993) J. Appl. Phys. , vol.74 , pp. 1468
    • Chen, X.1    Narayan, J.2
  • 10
    • 0002436741 scopus 로고    scopus 로고
    • Diamond deposition on noble metals
    • W. Klass, R. Haubner, and B. Lux: "Diamond Deposition on Noble Metals,"Diam. Relat. Mater., 1997, 6, pp. 240-46.
    • (1997) Diam. Relat. Mater. , vol.6 , pp. 240-246
    • Klass, W.1    Haubner, R.2    Lux, B.3
  • 11
    • 84974270262 scopus 로고
    • Effect of the chemical nature of transition-metal substrates on chemical-vapor deposition of diamond
    • W. Zhu, P.C. Yang, J.T. Glass, and F. Arezzo: "Effect of the Chemical Nature of Transition-Metal Substrates on Chemical-Vapor Deposition of Diamond,"J. Mater. Res., 1995, 10, p. 1455.
    • (1995) J. Mater. Res. , vol.10 , pp. 1455
    • Zhu, W.1    Yang, P.C.2    Glass, J.T.3    Arezzo, F.4
  • 12
    • 0029719183 scopus 로고    scopus 로고
    • Diamond deposition on cutting tools
    • B. Lux and R. Haubner: "Diamond Deposition on Cutting Tools,"Ceram. Int., 1996, 22, pp. 347-51.
    • (1996) Ceram. Int. , vol.22 , pp. 347-351
    • Lux, B.1    Haubner, R.2
  • 14
    • 0027702057 scopus 로고
    • Diamond deposition on chromium, cobalt and nickel substrates by microwave plasma chemical vapour deposition
    • R. Haubner, A. Lindlbauer, and B. Lux: "Diamond Deposition on Chromium, Cobalt and Nickel Substrates by Microwave Plasma Chemical Vapour Deposition,"Diam. Relat. Mater., 1993, 2, pp. 1505-15.
    • (1993) Diam. Relat. Mater. , vol.2 , pp. 1505-1515
    • Haubner, R.1    Lindlbauer, A.2    Lux, B.3
  • 15
    • 0026206337 scopus 로고
    • Chemical vapour deposition diamond coatings on cemented carbide tools
    • J. Oake, X.X. Pan, R. Haubner, and B. Lux: "Chemical Vapour Deposition Diamond Coatings on Cemented Carbide Tools."Surf. Coat. Technol., 1991, 47, pp. 600-07.
    • (1991) Surf. Coat. Technol. , vol.47 , pp. 600-607
    • Oake, J.1    Pan, X.X.2    Haubner, R.3    Lux, B.4
  • 16
    • 0025701285 scopus 로고
    • The improvement of the adhesion strength of diamond films
    • K. Saijo, M. Yagi, K. Shibuki, and S. Takatsu: "The Improvement of the Adhesion Strength of Diamond Films,"Surf. Coat. Technol., 1990, 43/44, pp. 30-40.
    • (1990) Surf. Coat. Technol. , vol.43-44 , pp. 30-40
    • Saijo, K.1    Yagi, M.2    Shibuki, K.3    Takatsu, S.4
  • 17
    • 0030283436 scopus 로고    scopus 로고
    • Selective dissolution of the cobalt binder from scraps of cemented tungsten carbide in acids containing additives
    • J.C. Lin, J.Y. Lin, and S.P. Jou: "Selective Dissolution of the Cobalt Binder from Scraps of Cemented Tungsten Carbide in Acids Containing Additives,"Hydrometall., 1996, 43, p. 47.
    • (1996) Hydrometall. , vol.43 , pp. 47
    • Lin, J.C.1    Lin, J.Y.2    Jou, S.P.3
  • 18
    • 0032194631 scopus 로고    scopus 로고
    • Enhanced nucleation of diamond films on pretreated substrates
    • V. Buck and F. Deuerler: "Enhanced Nucleation of Diamond Films on Pretreated Substrates,"Diam. Relat. Mater., 1998, 7, pp. 1544-52.
    • (1998) Diam. Relat. Mater. , vol.7 , pp. 1544-1552
    • Buck, V.1    Deuerler, F.2
  • 19
    • 0000717414 scopus 로고    scopus 로고
    • Diamond nucleation and growth on different cutting tool materials: Influence of substrate pre-treatments
    • E. Capelli, F. Pinzari, P. Ascarelli, and G. Righini: "Diamond Nucleation and Growth on Different Cutting Tool Materials: Influence of Substrate Pre-Treatments,"Diam. Relat. Mater., 1996, 5, pp. 292-98.
    • (1996) Diam. Relat. Mater. , vol.5 , pp. 292-298
    • Capelli, E.1    Pinzari, F.2    Ascarelli, P.3    Righini, G.4
  • 20
    • 0032188470 scopus 로고    scopus 로고
    • Highly adherent diamond coatings deposited onto WC-Co cemented carbides via barrier interlayers
    • J. Lopez, V.G. Babaev, V.V. Khvostov, and J.M. Albella: "Highly Adherent Diamond Coatings Deposited Onto WC-Co Cemented Carbides Via Barrier Interlayers,"J. Mater. Res., 1998, 13, p. 2841.
    • (1998) J. Mater. Res. , vol.13 , pp. 2841
    • Lopez, J.1    Babaev, V.G.2    Khvostov, V.V.3    Albella, J.M.4
  • 21
    • 0034745885 scopus 로고    scopus 로고
    • Diamond coatings on tungsten carbide and their erosive wear properties
    • S. Amirhaghi, H.S. Reehal, R.J.K Wood, and D.W. Wheeler: "Diamond Coatings on Tungsten Carbide and Their Erosive Wear Properties,"Surf. Coat. Technol. 2001, 135, pp. 126-38.
    • (2001) Surf. Coat. Technol. , vol.135 , pp. 126-138
    • Amirhaghi, S.1    Reehal, H.S.2    Wood, R.J.K.3    Wheeler, D.W.4
  • 22
    • 0242684606 scopus 로고    scopus 로고
    • Dry turning of alumina/aluminum composites with CVD diamond coated co-cemented tungsten carbide tools
    • R. Polini, F. Casadei, P. D'Antonio, and E. Traversa "Dry Turning of Alumina/Aluminum Composites With CVD Diamond Coated Co-Cemented Tungsten Carbide Tools,"Surf. Coat. Technol., 2003, 166, pp. 127-34.
    • (2003) Surf. Coat. Technol. , vol.166 , pp. 127-134
    • Polini, R.1    Casadei, F.2    D'Antonio, P.3    Traversa, E.4
  • 23
    • 0004729613 scopus 로고
    • Nucleation control of diamond synthesized by microwave plasma Cvd on cemented carbide substrate
    • H. Itoh, T. Osaki, H. Iwahara, and H. Sakamoto, "Nucleation Control of Diamond Synthesized by Microwave Plasma Cvd on Cemented Carbide Substrate,"J. Mater. Sci., 1991, 26, pp. 3763-68.
    • (1991) J. Mater. Sci. , vol.26 , pp. 3763-3768
    • Itoh, H.1    Osaki, T.2    Iwahara, H.3    Sakamoto, H.4
  • 24
    • 0010631361 scopus 로고    scopus 로고
    • Nucleation and initial growth of bias-assisted HFCVD diamond on boron nitride films
    • M.C. Polo, W. Wang, G. Sanshez, J. Andujar, and J. Esteve: "Nucleation and Initial Growth of Bias-Assisted HFCVD Diamond on Boron Nitride Films,"Diam. Relat. Mater., 1997, 6, pp. 579-83.
    • (1997) Diam. Relat. Mater. , vol.6 , pp. 579-583
    • Polo, M.C.1    Wang, W.2    Sanshez, G.3    Andujar, J.4    Esteve, J.5
  • 25
    • 0034074527 scopus 로고    scopus 로고
    • Quantitative determination of the adhesive fracture toughness of CVD diamond to WC-co cemented carbide
    • S. Kamiya, H. Takahashi, R. Polini, and E. Traversa, "Quantitative Determination of the Adhesive Fracture Toughness of CVD Diamond to WC-Co Cemented Carbide,"Diam. Relat. Mater., 2000, 9, pp. 191-94.
    • (2000) Diam. Relat. Mater. , vol.9 , pp. 191-194
    • Kamiya, S.1    Takahashi, H.2    Polini, R.3    Traversa, E.4
  • 26
    • 0036508459 scopus 로고    scopus 로고
    • Application of diamond coatings onto small dental tools
    • H. Sein, W. Ahmed, and C. Rego: "Application of Diamond Coatings Onto Small Dental Tools,"Diam. Relat. Mater., 2002, 11, pp. 731-35.
    • (2002) Diam. Relat. Mater. , vol.11 , pp. 731-735
    • Sein, H.1    Ahmed, W.2    Rego, C.3
  • 30
    • 0034074527 scopus 로고    scopus 로고
    • Quantitative determination of the adhesive fracture toughness of CVD diamond to WC-Co cemented carbide
    • S. Kamiya, H. Takahashi, R. Polini, and E. Traversa: "Quantitative Determination of the Adhesive Fracture Toughness of CVD Diamond to WC-Co Cemented Carbide,"Diam. Retat. Mater., 2000, 9, pp. 191-94.
    • (2000) Diam. Retat. Mater. , vol.9 , pp. 191-194
    • Kamiya, S.1    Takahashi, H.2    Polini, R.3    Traversa, E.4
  • 31
    • 12444298461 scopus 로고
    • Quantitative measurement of residual biaxial stress by raman-spectroscopy in diamond grown on a Ti alloy by chemical-vapor deposition
    • J.W. Ager and M.D. Drory: "Quantitative Measurement of Residual Biaxial Stress by Raman-Spectroscopy in Diamond Grown on a Ti Alloy by Chemical-Vapor Deposition,"Phys. Rev. B., 1993, 48, pp. 2601-07.
    • (1993) Phys. Rev. B. , vol.48 , pp. 2601-2607
    • Ager, J.W.1    Drory, M.D.2
  • 33
    • 0018547749 scopus 로고
    • Investigation and performance of dental drills in clinical practice
    • M.S. Pines and A. Schulman: "Investigation and Performance of Dental Drills in Clinical Practice,"Journal of the American Dental Association, 1979, 99, pp. 831-33.
    • (1979) Journal of the American Dental Association , vol.99 , pp. 831-833
    • Pines, M.S.1    Schulman, A.2
  • 35
    • 0037472625 scopus 로고    scopus 로고
    • Stress distribution in diamond films grown on cemented WC-Co dental burs using modified hot-filament CVD
    • H. Sein, W. Ahmed, M.J. Jackson, N. Ali, and J. Gracio: "Stress Distribution in Diamond Films Grown on Cemented WC-Co Dental Burs Using Modified Hot-Filament CVD,"Surf. Coat. Technol., 2003, 163-164, pp. 196-202.
    • (2003) Surf. Coat. Technol. , vol.163-164 , pp. 196-202
    • Sein, H.1    Ahmed, W.2    Jackson, M.J.3    Ali, N.4    Gracio, J.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.