2
-
-
0025492382
-
Fracture surface analysis of dental ceramics: clinically failed restorations
-
Kelly J.R., Giordano R., Pober R., and Cima M.J. Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont 3 (1990) 430-440
-
(1990)
Int J Prosthodont
, vol.3
, pp. 430-440
-
-
Kelly, J.R.1
Giordano, R.2
Pober, R.3
Cima, M.J.4
-
3
-
-
0028709614
-
Fracture surface characterization of clinically failed all-ceramic crowns
-
Thompson J.Y., Anusavice K.J., Naman A., and Morris H.F. Fracture surface characterization of clinically failed all-ceramic crowns. J Dent Res 73 (1994) 1824-1832
-
(1994)
J Dent Res
, vol.73
, pp. 1824-1832
-
-
Thompson, J.Y.1
Anusavice, K.J.2
Naman, A.3
Morris, H.F.4
-
5
-
-
0029258587
-
Predicting lifetimes of materials and material structures
-
Ritter J.E. Predicting lifetimes of materials and material structures. Dent Mater 11 (1995) 142-146
-
(1995)
Dent Mater
, vol.11
, pp. 142-146
-
-
Ritter, J.E.1
-
6
-
-
0036132150
-
Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses
-
De Aza A.H., Chevalier J., Fantozzi G., Schehl M., and Torrecillas R. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses. Biomaterials 23 (2002) 937-945
-
(2002)
Biomaterials
, vol.23
, pp. 937-945
-
-
De Aza, A.H.1
Chevalier, J.2
Fantozzi, G.3
Schehl, M.4
Torrecillas, R.5
-
7
-
-
84977695915
-
Influence of water vapor on crack propagation in soda-lime glass
-
Wiederhorn S.M. Influence of water vapor on crack propagation in soda-lime glass. J Am Ceram Soc 50 (1967) 407-414
-
(1967)
J Am Ceram Soc
, vol.50
, pp. 407-414
-
-
Wiederhorn, S.M.1
-
8
-
-
0025674828
-
Crack velocity functions and thresholds in brittle solids
-
Wan K.T., Lathabai S., and Lawn B.R. Crack velocity functions and thresholds in brittle solids. J Eur Ceram Soc 6 (1990) 259-268
-
(1990)
J Eur Ceram Soc
, vol.6
, pp. 259-268
-
-
Wan, K.T.1
Lathabai, S.2
Lawn, B.R.3
-
9
-
-
0021517155
-
Slow fracture model based on strained silicate structures
-
Michalske T.A., and Bunker B.C. Slow fracture model based on strained silicate structures. J Appl Phys 56 (1984) 2686-2693
-
(1984)
J Appl Phys
, vol.56
, pp. 2686-2693
-
-
Michalske, T.A.1
Bunker, B.C.2
-
10
-
-
0022501121
-
Fatigue of dental ceramics in a simulated oral environment
-
Morena R., Beaudreau G.M., Lockwood P.E., Evans A.L., and Fairhurst C.W. Fatigue of dental ceramics in a simulated oral environment. J Dent Res 65 (1986) 993-997
-
(1986)
J Dent Res
, vol.65
, pp. 993-997
-
-
Morena, R.1
Beaudreau, G.M.2
Lockwood, P.E.3
Evans, A.L.4
Fairhurst, C.W.5
-
11
-
-
1842732685
-
Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics
-
Guazzato M., Albakry M., Ringer S.P., and Swain M.V. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part I. Pressable and alumina glass-infiltrated ceramics. Dent Mater 20 (2004) 441-448
-
(2004)
Dent Mater
, vol.20
, pp. 441-448
-
-
Guazzato, M.1
Albakry, M.2
Ringer, S.P.3
Swain, M.V.4
-
12
-
-
0030133772
-
Modeling the caries-inhibitory effects of dental materials
-
Featherstone J.D. Modeling the caries-inhibitory effects of dental materials. Dent Mater 12 (1996) 194-197
-
(1996)
Dent Mater
, vol.12
, pp. 194-197
-
-
Featherstone, J.D.1
-
13
-
-
0033287532
-
Morphology of initial lesions of enamel treated with different commercial dentifrices using a pH cycling model: scanning electron microscopy observations
-
Itthagarun A., Wei S.H., and Wefel J.S. Morphology of initial lesions of enamel treated with different commercial dentifrices using a pH cycling model: scanning electron microscopy observations. Int Dent J 49 (1999) 352-360
-
(1999)
Int Dent J
, vol.49
, pp. 352-360
-
-
Itthagarun, A.1
Wei, S.H.2
Wefel, J.S.3
-
14
-
-
0020316440
-
Alternating demineralization and remineralization of artificial enamel lesions
-
Ten Cate J.M., and Duijsters P.P. Alternating demineralization and remineralization of artificial enamel lesions. Caries Res 16 (1982) 201-210
-
(1982)
Caries Res
, vol.16
, pp. 201-210
-
-
Ten Cate, J.M.1
Duijsters, P.P.2
-
16
-
-
0015616877
-
Effect of eletrolyte pH on propagation in glass
-
Wiederhorn S.M., and Johnson H. Effect of eletrolyte pH on propagation in glass. J Am Ceram Soc 56 (1973) 192-197
-
(1973)
J Am Ceram Soc
, vol.56
, pp. 192-197
-
-
Wiederhorn, S.M.1
Johnson, H.2
-
17
-
-
0016535098
-
Effect of test environment on stress-corrosion susceptibility of glass
-
Ritter J., and Laporte R. Effect of test environment on stress-corrosion susceptibility of glass. J Am Ceram Soc 58 (1975) 265-267
-
(1975)
J Am Ceram Soc
, vol.58
, pp. 265-267
-
-
Ritter, J.1
Laporte, R.2
-
18
-
-
84987319332
-
Glass surface cracks caused by alkaline solution containing an alkaline-earth element
-
Tomozawa M., Oka Y., and Wahl M.J. Glass surface cracks caused by alkaline solution containing an alkaline-earth element. J Am Ceram Soc 64 (1981) 32-33
-
(1981)
J Am Ceram Soc
, vol.64
, pp. 32-33
-
-
Tomozawa, M.1
Oka, Y.2
Wahl, M.J.3
-
19
-
-
0019634575
-
Effect of corrosion processes on subcritical crack-growth in glass
-
Simmons C., and Freiman S. Effect of corrosion processes on subcritical crack-growth in glass. J Eur Ceram Soc 64 (1981) 683-686
-
(1981)
J Eur Ceram Soc
, vol.64
, pp. 683-686
-
-
Simmons, C.1
Freiman, S.2
-
20
-
-
43049100207
-
-
ASTM-C1161. Flexural strength of advanced ceramics at ambient temperature. 2002.
-
ASTM-C1161. Flexural strength of advanced ceramics at ambient temperature. 2002.
-
-
-
-
21
-
-
0011098350
-
Standard test method for determination of slow crack growth parameters of advanced ceramics by constant stress-rate flexural testing at ambient temperature
-
American Society for Testing and Materials p. 1-9
-
ASTM-C1368-00. Standard test method for determination of slow crack growth parameters of advanced ceramics by constant stress-rate flexural testing at ambient temperature. Annual book of ASTM vol. 15 (2001), American Society for Testing and Materials p. 1-9
-
(2001)
Annual book of ASTM
, vol.15
-
-
ASTM-C1368-001
-
22
-
-
0022702131
-
Fracture toughness of commercial dental porcelains
-
Morena R., Lockwood P.E., and Fairhurst C.W. Fracture toughness of commercial dental porcelains. Dent Mater 2 (1986) 58-62
-
(1986)
Dent Mater
, vol.2
, pp. 58-62
-
-
Morena, R.1
Lockwood, P.E.2
Fairhurst, C.W.3
-
23
-
-
84987335986
-
A critical of indentation techniques for measuring fracture toughness: in direct crack measurements
-
Anstis G. A critical of indentation techniques for measuring fracture toughness: in direct crack measurements. J Am Ceram Soc 64 (1981) 533-538
-
(1981)
J Am Ceram Soc
, vol.64
, pp. 533-538
-
-
Anstis, G.1
-
24
-
-
0021943027
-
Chemical and histological changes during development of artificial caries
-
Featherstone J.D., Holmen L., Thylstrup A., Fredebo L., and Shariati M. Chemical and histological changes during development of artificial caries. Caries Res 19 (1985) 1-10
-
(1985)
Caries Res
, vol.19
, pp. 1-10
-
-
Featherstone, J.D.1
Holmen, L.2
Thylstrup, A.3
Fredebo, L.4
Shariati, M.5
-
25
-
-
0037104975
-
Ion leaching from dental ceramics during static in vitro corrosion testing
-
Milleding P., Haraldsson C., and Karlsson S. Ion leaching from dental ceramics during static in vitro corrosion testing. J Biomed Mater Res 61 (2002) 541-550
-
(2002)
J Biomed Mater Res
, vol.61
, pp. 541-550
-
-
Milleding, P.1
Haraldsson, C.2
Karlsson, S.3
-
26
-
-
43049085376
-
Vickers indentation: a powerful tool for the analysis of fatigue behavior on glass
-
The American Ceramic Society, Westerville
-
Sglavo V.M., and Bertoldi M. Vickers indentation: a powerful tool for the analysis of fatigue behavior on glass. Indentation techniques in ceramic material characterization (2004), The American Ceramic Society, Westerville
-
(2004)
Indentation techniques in ceramic material characterization
-
-
Sglavo, V.M.1
Bertoldi, M.2
-
27
-
-
27644548221
-
Fracture toughness of dental porcelains evaluated by IF, SCF, and SEPB methods
-
Yoshimura H.N., Cesar P.F., Miranda Jr. W.G., Gonzaga C.C., and Okada C.Y. Fracture toughness of dental porcelains evaluated by IF, SCF, and SEPB methods. J Am Ceram Soc 88 (2005) 1680-1683
-
(2005)
J Am Ceram Soc
, vol.88
, pp. 1680-1683
-
-
Yoshimura, H.N.1
Cesar, P.F.2
Miranda Jr., W.G.3
Gonzaga, C.C.4
Okada, C.Y.5
-
28
-
-
33746675666
-
Relationship between fracture toughness and flexural strength in dental porcelains
-
Cesar P.F., Yoshimura H.N., Miranda Jr. W.G., Miyazaki C.L., Muta L.M., and Rodrigues Filho L.E. Relationship between fracture toughness and flexural strength in dental porcelains. J Biomed Mater Res B: Appl Biomater 78 (2006) 265-273
-
(2006)
J Biomed Mater Res B: Appl Biomater
, vol.78
, pp. 265-273
-
-
Cesar, P.F.1
Yoshimura, H.N.2
Miranda Jr., W.G.3
Miyazaki, C.L.4
Muta, L.M.5
Rodrigues Filho, L.E.6
-
29
-
-
38449089370
-
Mechanical properties and microstructure of zinc oxide varistor ceramics
-
Yoshimura H.N., Molisani A.L., Narita N.E., Manholeti J.L.A., and Cavenaghi J.M. Mechanical properties and microstructure of zinc oxide varistor ceramics. Mater Sci Forum 530 (2006) 408-413
-
(2006)
Mater Sci Forum
, vol.530
, pp. 408-413
-
-
Yoshimura, H.N.1
Molisani, A.L.2
Narita, N.E.3
Manholeti, J.L.A.4
Cavenaghi, J.M.5
-
30
-
-
0035735409
-
Evidence of a critical leucite particle size for microcracking in dental porcelains
-
Mackert Jr. J.R., Twiggs S.W., Russell C.M., and Williams A.L. Evidence of a critical leucite particle size for microcracking in dental porcelains. J Dent Res 80 (2001) 1574-1579
-
(2001)
J Dent Res
, vol.80
, pp. 1574-1579
-
-
Mackert Jr., J.R.1
Twiggs, S.W.2
Russell, C.M.3
Williams, A.L.4
-
31
-
-
26044441332
-
Correlation between fracture toughness and leucite content in dental porcelains
-
Cesar P.F., Yoshimura H.N., Miranda Jr. W.G., and Okada C.Y. Correlation between fracture toughness and leucite content in dental porcelains. J Dent 33 (2005) 721-729
-
(2005)
J Dent
, vol.33
, pp. 721-729
-
-
Cesar, P.F.1
Yoshimura, H.N.2
Miranda Jr., W.G.3
Okada, C.Y.4
-
32
-
-
43049111242
-
-
National Institute of Standards and Technology, Washington
-
Quinn GD. Fractography of ceramics and glasses (2007), National Institute of Standards and Technology, Washington
-
(2007)
Fractography of ceramics and glasses
-
-
Quinn GD1
-
33
-
-
0029270958
-
Influence of indentation crack configuration on strength and fatigue behavior of soda-lime silicate glass
-
Sglavo V., and Green D. Influence of indentation crack configuration on strength and fatigue behavior of soda-lime silicate glass. Acta Metall Mater 43 (1995) 965-972
-
(1995)
Acta Metall Mater
, vol.43
, pp. 965-972
-
-
Sglavo, V.1
Green, D.2
-
34
-
-
43049114768
-
-
ASTM-1421. Standard test methods for determination of fracture toughness of advanced ceramics at ambient temperature. 1999.
-