Volumn 14, Issue 5 SUPPL. 1, 2007, Pages 130-136

Materials Resistance to Liquid Zinc Corrosion on Surface of Sink Roll

Author keywords

coating; corrosion; liquid zinc; sink roll; spray

Indexed keywords


EID: 42949090417     PISSN: 1006706X     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1006-706X(08)60066-7     Document Type: Article
Times cited : (35)

References (24)
  • 1
    • 84971447685 scopus 로고    scopus 로고
    • Applications of Liquid Zinc Corrosion Resistant Coatings for Hot Zinc Galvanizing Equipment [J]
    • Xu Y., Sun H., Yu M., et al. Applications of Liquid Zinc Corrosion Resistant Coatings for Hot Zinc Galvanizing Equipment [J]. Corrosion Science and Protection Technology 16 6 (2004) 378-380
    • (2004) Corrosion Science and Protection Technology , vol.16 , Issue.6 , pp. 378-380
    • Xu, Y.1    Sun, H.2    Yu, M.3
  • 2
    • 42949121009 scopus 로고    scopus 로고
    • Present Status on Hot Galvanizing in China [J]
    • Li J. Present Status on Hot Galvanizing in China [J]. Steel Rolling 121 13 (2004) 74-76
    • (2004) Steel Rolling , vol.121 , Issue.13 , pp. 74-76
    • Li, J.1
  • 4
    • 42949120493 scopus 로고    scopus 로고
    • Summarization of Liquid Zn Corrosion Resistant Material [J]
    • Gao K., and Li S. Summarization of Liquid Zn Corrosion Resistant Material [J]. Steel Wire Products 27 3 (2001) 50-52
    • (2001) Steel Wire Products , vol.27 , Issue.3 , pp. 50-52
    • Gao, K.1    Li, S.2
  • 5
    • 34248194403 scopus 로고    scopus 로고
    • Progress in Research on Liquid Zinc Corrosion of Bath Hardware [J]
    • Wang W., Wang Y., Lin J., et al. Progress in Research on Liquid Zinc Corrosion of Bath Hardware [J]. Journal of Iron and Steel Research 19 3 (2007) 1-5
    • (2007) Journal of Iron and Steel Research , vol.19 , Issue.3 , pp. 1-5
    • Wang, W.1    Wang, Y.2    Lin, J.3
  • 6
    • 3142583753 scopus 로고    scopus 로고
    • Mechanism of Liquid Zinc Corrosion on Metals [J]
    • Cao X., Wen M., and Jiang X. Mechanism of Liquid Zinc Corrosion on Metals [J]. Journal of Iron and Steel Research 10 4 (1998) 54-58
    • (1998) Journal of Iron and Steel Research , vol.10 , Issue.4 , pp. 54-58
    • Cao, X.1    Wen, M.2    Jiang, X.3
  • 7
    • 42949119176 scopus 로고    scopus 로고
    • Corrosion of Metals by Molten Zinc and the Countermeasure [J]
    • Han W., and Wang G. Corrosion of Metals by Molten Zinc and the Countermeasure [J]. Journal of Heibei University of Technology 30 3 (2001) 46-49
    • (2001) Journal of Heibei University of Technology , vol.30 , Issue.3 , pp. 46-49
    • Han, W.1    Wang, G.2
  • 8
    • 33746762305 scopus 로고    scopus 로고
    • Study and Applications of Materials Resistant to Liquid Zinc Corrosion [J]
    • Cao X., Jiang X., Wen M., et al. Study and Applications of Materials Resistant to Liquid Zinc Corrosion [J]. Transactions of Metal Heat Treatmen 18 2 (1997) 25-29
    • (1997) Transactions of Metal Heat Treatmen , vol.18 , Issue.2 , pp. 25-29
    • Cao, X.1    Jiang, X.2    Wen, M.3
  • 9
    • 33747477483 scopus 로고    scopus 로고
    • Study on Corrosion Strength of Boronizing Layer Against Melt Zinc [J]
    • Wang G., and Han W. Study on Corrosion Strength of Boronizing Layer Against Melt Zinc [J]. Journal of Heibei University of Technology 30 5 (2001) 79-84
    • (2001) Journal of Heibei University of Technology , vol.30 , Issue.5 , pp. 79-84
    • Wang, G.1    Han, W.2
  • 11
    • 0041725599 scopus 로고    scopus 로고
    • High Temperature Batch Hot-Dip Galvanizing. Part 1: General Description of Coatings Formed at 560°C [J]
    • Verma A., and Ooij V. High Temperature Batch Hot-Dip Galvanizing. Part 1: General Description of Coatings Formed at 560°C [J]. Surface and Coatings Technology 89 1-2 (1997) 132-142
    • (1997) Surface and Coatings Technology , vol.89 , Issue.1-2 , pp. 132-142
    • Verma, A.1    Ooij, V.2
  • 12
    • 0033370366 scopus 로고    scopus 로고
    • Control of the Growth of Zinc-Iron Phases in the Hot-Dip Galvanizing Process [J]
    • Culcasi J., Sere P., and Elsner C. Control of the Growth of Zinc-Iron Phases in the Hot-Dip Galvanizing Process [J]. Surface and Coatings Technology 122 1 (1999) 21-23
    • (1999) Surface and Coatings Technology , vol.122 , Issue.1 , pp. 21-23
    • Culcasi, J.1    Sere, P.2    Elsner, C.3
  • 13
    • 0031353525 scopus 로고    scopus 로고
    • Supermeniscus Interactions Between Molten Zinc and Bath Hardwar Materials in Galvanizing [J]
    • Brunnock M., and Jones R. Supermeniscus Interactions Between Molten Zinc and Bath Hardwar Materials in Galvanizing [J]. Ironmaking and Steelmaking 24 (1997) 40-46
    • (1997) Ironmaking and Steelmaking , Issue.24 , pp. 40-46
    • Brunnock, M.1    Jones, R.2
  • 14
    • 0032180967 scopus 로고    scopus 로고
    • Degradation Behavior of Boronized Carbon and High Alloy Steel in Aluminum and Zinc [J]
    • Tsipas D. Degradation Behavior of Boronized Carbon and High Alloy Steel in Aluminum and Zinc [J]. Materials Letters 37 (1998) 128-131
    • (1998) Materials Letters , vol.37 , pp. 128-131
    • Tsipas, D.1
  • 15
    • 2442652982 scopus 로고    scopus 로고
    • Fabrication of the Boride Coating and its Anti-corrosion Property in Zinc Melt [J]
    • Wang J., Li K., Shu D., et al. Fabrication of the Boride Coating and its Anti-corrosion Property in Zinc Melt [J]. Jonrnal of Shanghai Jiaotong University 37 12 (2003) 1840-1843
    • (2003) Jonrnal of Shanghai Jiaotong University , vol.37 , Issue.12 , pp. 1840-1843
    • Wang, J.1    Li, K.2    Shu, D.3
  • 16
    • 33747497028 scopus 로고    scopus 로고
    • Improvement of Corrosion Resistance of Boronizing Layer Molten Zinc by Addition of Rare-earth Element [J]
    • Ma R., Cao X., and WEN M. Improvement of Corrosion Resistance of Boronizing Layer Molten Zinc by Addition of Rare-earth Element [J]. Journal of Chinese Society for Corrosion and Protection 26 3 (2006) 180-183
    • (2006) Journal of Chinese Society for Corrosion and Protection , vol.26 , Issue.3 , pp. 180-183
    • Ma, R.1    Cao, X.2    WEN, M.3
  • 17
    • 0028750773 scopus 로고
    • Durability of sprayed WC/Co coating in Al-added zinc bath [J]
    • Kazumi T., Tomoki T., Yoshifumi K., et al. Durability of sprayed WC/Co coating in Al-added zinc bath [J]. ISIJ International 34 10 (1994) 828
    • (1994) ISIJ International , vol.34 , Issue.10 , pp. 828
    • Kazumi, T.1    Tomoki, T.2    Yoshifumi, K.3
  • 19
    • 33748698896 scopus 로고    scopus 로고
    • Corrosion of 316 Stainless Steel/WC-Co Coating in Liquid Zinc [J]
    • Wang W., Lin J., Wang Y., et al. Corrosion of 316 Stainless Steel/WC-Co Coating in Liquid Zinc [J]. Journal of Aeronautical Materials 26 4 (2006) 56-60
    • (2006) Journal of Aeronautical Materials , vol.26 , Issue.4 , pp. 56-60
    • Wang, W.1    Lin, J.2    Wang, Y.3
  • 20
    • 42949123355 scopus 로고    scopus 로고
    • Durability of the Coatings Sprayed by the High Velocity Oxygen Fuel Immerged in Liquid Zinc Bath [J]
    • Xin G., Gao Y., and Hei Z. Durability of the Coatings Sprayed by the High Velocity Oxygen Fuel Immerged in Liquid Zinc Bath [J]. Journal of Dalian Maritime university 28 1 (2002) 103-107
    • (2002) Journal of Dalian Maritime university , vol.28 , Issue.1 , pp. 103-107
    • Xin, G.1    Gao, Y.2    Hei, Z.3
  • 21
    • 42949097915 scopus 로고    scopus 로고
    • Study on the Material of Inside Heating Casting for Galvanizing by Dipping [J]
    • Liu Y., Yan D., and Zou D. Study on the Material of Inside Heating Casting for Galvanizing by Dipping [J]. Shandong Ceramics 29 6 (2006) 16-19
    • (2006) Shandong Ceramics , vol.29 , Issue.6 , pp. 16-19
    • Liu, Y.1    Yan, D.2    Zou, D.3
  • 22
    • 34548258653 scopus 로고    scopus 로고
    • Development of Durable Spray Coating in Molten Al and Al-Zn alloys. ATSC 2005 (Nagoya, Japan)
    • Mizuno H., Kitamura J., Tawada S., et al. Development of Durable Spray Coating in Molten Al and Al-Zn alloys. ATSC 2005 (Nagoya, Japan). Asian Thermal Spray Committee (2005) 81-82
    • (2005) Asian Thermal Spray Committee , pp. 81-82
    • Mizuno, H.1    Kitamura, J.2    Tawada, S.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.