메뉴 건너뛰기




Volumn 85, Issue 2, 2008, Pages 509-518

In vitro biostability evaluation of polyurethane composites in acidic, basic, oxidative, and neutral solutions

Author keywords

Biomaterial; Biostability; Chemical resistance; Composite; Hydration; Oxidation

Indexed keywords

BIOACTIVITY; BIOMATERIALS; CHEMICAL RESISTANCE; COMPOSITE MATERIALS; DEGRADATION; HYDRATION;

EID: 42649102352     PISSN: 15524973     EISSN: 15524981     Source Type: Journal    
DOI: 10.1002/jbm.b.30973     Document Type: Article
Times cited : (10)

References (24)
  • 2
    • 1642505726 scopus 로고    scopus 로고
    • Bioinert, biodegradable and injectable polymeric matrix composites for hard tissue replacement: State of the art and recent developments
    • Mano JF, Sousa RA, Boesel LF, Neves NM, Reis RL. Bioinert, biodegradable and injectable polymeric matrix composites for hard tissue replacement: State of the art and recent developments. Compos Sci Technol 2004;64:789-817.
    • (2004) Compos Sci Technol , vol.64 , pp. 789-817
    • Mano, J.F.1    Sousa, R.A.2    Boesel, L.F.3    Neves, N.M.4    Reis, R.L.5
  • 4
    • 0017861743 scopus 로고
    • Carbon fiber-reinforced carbon as a potential implant material
    • Adams D, Williams DF, Hill J. Carbon fiber-reinforced carbon as a potential implant material. J Biomed Mater Res 1978;12:35-42.
    • (1978) J Biomed Mater Res , vol.12 , pp. 35-42
    • Adams, D.1    Williams, D.F.2    Hill, J.3
  • 5
    • 0019761155 scopus 로고
    • Carbon fiber-reinforced polyethylene (CPE) for total knee replacement prostheses: A clinical experience
    • Halcomb FJ, Bardos D. Carbon fiber-reinforced polyethylene (CPE) for total knee replacement prostheses: A clinical experience. Trans Am Soc Artif Intern Organs 1981;27:364-368.
    • (1981) Trans Am Soc Artif Intern Organs , vol.27 , pp. 364-368
    • Halcomb, F.J.1    Bardos, D.2
  • 6
    • 0022504260 scopus 로고
    • The problem of surface damage in polyethylene total knee components
    • Wright TM, Bartel DL. The problem of surface damage in polyethylene total knee components. Clin Orthop Relat Res 1986;205:67-74.
    • (1986) Clin Orthop Relat Res , vol.205 , pp. 67-74
    • Wright, T.M.1    Bartel, D.L.2
  • 8
    • 0023689745 scopus 로고
    • Analysis of surface damage in retrieved carbon fiber-reinforced and plain polyethylene tibial components from posterior stabilized total knee replacements
    • Wright TM, Rimnac CM, Faris PM, Bansal M. Analysis of surface damage in retrieved carbon fiber-reinforced and plain polyethylene tibial components from posterior stabilized total knee replacements. J Bone Joint Surg Am 1988;70:1312-1319.
    • (1988) J Bone Joint Surg Am , vol.70 , pp. 1312-1319
    • Wright, T.M.1    Rimnac, C.M.2    Faris, P.M.3    Bansal, M.4
  • 9
    • 0028518641 scopus 로고
    • Long-term durability of the interface in FRP composites after exposure to simulated physiologic saline environments
    • Meyer MR, Friedman RJ, Del Schutte H Jr, Latour RA Jr. Long-term durability of the interface in FRP composites after exposure to simulated physiologic saline environments. J Biomed Mater Res 1994;28:1221-1231.
    • (1994) J Biomed Mater Res , vol.28 , pp. 1221-1231
    • Meyer, M.R.1    Friedman, R.J.2    Del Schutte Jr, H.3    Latour Jr., R.A.4
  • 10
    • 0027686740 scopus 로고
    • Development of FRP composite structural biomaterials: Fatigue strength of the fiber/matrix interfacial bond in simulated in vivo environments
    • Latour RA Jr, Black J. Development of FRP composite structural biomaterials: Fatigue strength of the fiber/matrix interfacial bond in simulated in vivo environments. J Biomed Mater Res 1993;27:1281-1291.
    • (1993) J Biomed Mater Res , vol.27 , pp. 1281-1291
    • Latour Jr, R.A.1    Black, J.2
  • 11
    • 0026864047 scopus 로고
    • Development of FRP composite structural biomaterials: Ultimate strength of the fiber/matrix interfacial bond in in vivo simulated environments
    • Latour RA Jr, Black J. Development of FRP composite structural biomaterials: Ultimate strength of the fiber/matrix interfacial bond in in vivo simulated environments. J Biomed Mater Res 1992;26:593-606.
    • (1992) J Biomed Mater Res , vol.26 , pp. 593-606
    • Latour Jr, R.A.1    Black, J.2
  • 12
    • 33747436928 scopus 로고    scopus 로고
    • In vitro flexural properties of hydroxyapatite and self-reinforced poly(L-lactic acid)
    • Wright-Charlesworth DD, King JA, Miller DM, Lim CH. In vitro flexural properties of hydroxyapatite and self-reinforced poly(L-lactic acid). J Biomed Mater Res A 2006;78:541-549.
    • (2006) J Biomed Mater Res A , vol.78 , pp. 541-549
    • Wright-Charlesworth, D.D.1    King, J.A.2    Miller, D.M.3    Lim, C.H.4
  • 13
    • 0024102233 scopus 로고
    • Polyether polyurethanes: Biostable or not?
    • Stokes K.Polyether polyurethanes: Biostable or not? J Biomater Appl 1988;3:229-259.
    • (1988) J Biomater Appl , vol.3 , pp. 229-259
    • Stokes, K.1
  • 15
    • 0029278286 scopus 로고
    • Glass wool-H2O2/CoCl2 test system for in vitro evaluation of biodegradative stress cracking in polyurethane elastomers
    • Zhao Q, Casas-Bejar J, Urbanski P, Stokes K. Glass wool-H2O2/CoCl2 test system for in vitro evaluation of biodegradative stress cracking in polyurethane elastomers. J Biomed Mater Res 1995;29:467-75.
    • (1995) J Biomed Mater Res , vol.29 , pp. 467-475
    • Zhao, Q.1    Casas-Bejar, J.2    Urbanski, P.3    Stokes, K.4
  • 17
    • 0345168927 scopus 로고    scopus 로고
    • Effect of strain and strain rate on fatigue-accelerated biodegradation of polyurethane
    • Wiggins MJ, Anderson JM, Hiltner A. Effect of strain and strain rate on fatigue-accelerated biodegradation of polyurethane. J Biomed Mater Res A 2003;66:463-475.
    • (2003) J Biomed Mater Res A , vol.66 , pp. 463-475
    • Wiggins, M.J.1    Anderson, J.M.2    Hiltner, A.3
  • 18
    • 3342986332 scopus 로고    scopus 로고
    • Oxidative mechanisms of poly(carbonate urethane) and poly(ether urethane) biodegradation: In vivo and in vitro correlations
    • Christenson EM, Anderson JM, Hiltner A. Oxidative mechanisms of poly(carbonate urethane) and poly(ether urethane) biodegradation: In vivo and in vitro correlations. J Biomed Mater Res A 2004;70:245-255.
    • (2004) J Biomed Mater Res A , vol.70 , pp. 245-255
    • Christenson, E.M.1    Anderson, J.M.2    Hiltner, A.3
  • 20
    • 85047696707 scopus 로고    scopus 로고
    • Biodegradation of polyether polyurethane inner insulation in bipolar pacemaker leads
    • Wiggins MJ, Wilkoff B, Anderson JM, Hiltner A. Biodegradation of polyether polyurethane inner insulation in bipolar pacemaker leads. J Biomed Mater Res 2001;58:302-307.
    • (2001) J Biomed Mater Res , vol.58 , pp. 302-307
    • Wiggins, M.J.1    Wilkoff, B.2    Anderson, J.M.3    Hiltner, A.4
  • 23
    • 0033567864 scopus 로고    scopus 로고
    • In vitro modulation of macrophage phenotype and inhibition of polymer degradation by dexamethasone in a human macrophage/Fe/stress system
    • Casas J, Zhao Q, Donovan M, Schroeder P, Stokes K, Untereker D. In vitro modulation of macrophage phenotype and inhibition of polymer degradation by dexamethasone in a human macrophage/Fe/stress system. J Biomed Mater Res 1999;46:475-484.
    • (1999) J Biomed Mater Res , vol.46 , pp. 475-484
    • Casas, J.1    Zhao, Q.2    Donovan, M.3    Schroeder, P.4    Stokes, K.5    Untereker, D.6
  • 24
    • 33644811753 scopus 로고    scopus 로고
    • Chemical and biochemical degradation of polymers
    • Ratner BD, Hoffman AS, Schoen FJ, Lemons JE, editors, 2nd ed. New York: Elsevier;
    • Coury A. Chemical and biochemical degradation of polymers. In: Ratner BD, Hoffman AS, Schoen FJ, Lemons JE, editors. Biomaterials Science: An Introduction to Materials in Medicine, 2nd ed. New York: Elsevier; 2004. p 411-429.
    • (2004) Biomaterials Science: An Introduction to Materials in Medicine , pp. 411-429
    • Coury, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.