Volumn 18, Issue 2, 2008, Pages 383-387

New fracture morphology of amorphous Fe78Si9B13 alloy

Author keywords

amorphous Fe78Si9B13 alloy; damage cavity; periodic striation pattern

Indexed keywords

CRACKS; FRACTURE; IRON ALLOYS; MORPHOLOGY; SCANNING ELECTRON MICROSCOPY; SILICON ALLOYS;

EID: 42049121153     PISSN: 10036326     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1003-6326(08)60067-9     Document Type: Article
Times cited : (5)

References (17)
  • 1
    • 0015315810 scopus 로고
    • Plastic flow and fracture of metallic glass (tensile plastic flow and fracture behavior of PdSi based alloys in glassy microcrystalline and crystalline states, noting shear deformation bands) [J]
    • LEAMY H., WANG T., and CHEN H. Plastic flow and fracture of metallic glass (tensile plastic flow and fracture behavior of PdSi based alloys in glassy microcrystalline and crystalline states, noting shear deformation bands) [J]. Met Trans 3 (1972) 699-708
    • (1972) Met Trans , vol.3 , pp. 699-708
    • LEAMY, H.1    WANG, T.2    CHEN, H.3
  • 2
  • 3
    • 0016535214 scopus 로고
    • Flow and fracture in amorphous alloys [J]
    • PAMPILLO C. Flow and fracture in amorphous alloys [J]. J Mater Sci 10 (1975) 1194-1227
    • (1975) J Mater Sci , vol.10 , pp. 1194-1227
    • PAMPILLO, C.1
  • 4
    • 0033907537 scopus 로고    scopus 로고
    • Stabilization of metallic supercooled liquid and bulk amorphous alloys [J]
    • INOUE A. Stabilization of metallic supercooled liquid and bulk amorphous alloys [J]. Acta Mater 48 (2000) 279-306
    • (2000) Acta Mater , vol.48 , pp. 279-306
    • INOUE, A.1
  • 6
    • 33748973745 scopus 로고    scopus 로고
    • Evolution of nanoscale morphology on fracture surface of brittle metallic glass [J]
    • (1-3)
    • WANG G., WANG Y., LIU Y., PAN M., ZHAO D., and WANG W. Evolution of nanoscale morphology on fracture surface of brittle metallic glass [J]. Appl Phys Lett 89 (2006) 121909 (1-3)
    • (2006) Appl Phys Lett , vol.89 , pp. 121909
    • WANG, G.1    WANG, Y.2    LIU, Y.3    PAN, M.4    ZHAO, D.5    WANG, W.6
  • 7
    • 0042821692 scopus 로고    scopus 로고
    • Fracture mechanisms in bulk metallic glassy materials [J]
    • (1-4).
    • ZHANG Z., HE G., ECKERT J., and SCHULTZ L. Fracture mechanisms in bulk metallic glassy materials [J]. Phys Rev Lett 91 4 (2003) 045505 (1-4).
    • (2003) Phys Rev Lett , vol.91 , Issue.4 , pp. 045505
    • ZHANG, Z.1    HE, G.2    ECKERT, J.3    SCHULTZ, L.4
  • 8
    • 18144381586 scopus 로고    scopus 로고
    • Unified tensile fracture criterion [J]
    • (1-4).
    • ZHANG Z., and ECKERT J. Unified tensile fracture criterion [J]. Phys Rev Lett 94 (2005) 094301 (1-4).
    • (2005) Phys Rev Lett , vol.94 , pp. 094301
    • ZHANG, Z.1    ECKERT, J.2
  • 9
    • 34247616087 scopus 로고    scopus 로고
    • Fracture instability in brittle Mg-based bulk metallic glasses [J]
    • PAN D., ZHANG H., WANG A., WANG Z., and HU Z. Fracture instability in brittle Mg-based bulk metallic glasses [J]. J Alloys Compd 438 1/2 (2007) 145-149
    • (2007) J Alloys Compd , vol.438 , Issue.1-2 , pp. 145-149
    • PAN, D.1    ZHANG, H.2    WANG, A.3    WANG, Z.4    HU, Z.5
  • 10
    • 33748958634 scopus 로고    scopus 로고
    • Formation of nanowaves in compressive fracture of a less-brittle bulk metallic glass [J]
    • (1-3).
    • SHEN J., LIANG W., and SUN J. Formation of nanowaves in compressive fracture of a less-brittle bulk metallic glass [J]. Appl Phys Lett 89 (2006) 121908 (1-3).
    • (2006) Appl Phys Lett , vol.89 , pp. 121908
    • SHEN, J.1    LIANG, W.2    SUN, J.3
  • 11
    • 33750722131 scopus 로고    scopus 로고
    • Periodic corrugation on dynamic fracture surface in a brittle bulk metallic glass [J]
    • (1-3).
    • XI X., ZHAO D., PAN M., WANG W., WU Y., and LEWANDOWSKI J. Periodic corrugation on dynamic fracture surface in a brittle bulk metallic glass [J]. Appl Phys Lett 89 (2006) 181911 (1-3).
    • (2006) Appl Phys Lett , vol.89 , pp. 181911
    • XI, X.1    ZHAO, D.2    PAN, M.3    WANG, W.4    WU, Y.5    LEWANDOWSKI, J.6
  • 12
    • 0037170202 scopus 로고    scopus 로고
    • Crack front waves and the dynamics of a rapidly moving crack [J]
    • (1-4).
    • SHARON E., COHEN G., and FINEBERG J. Crack front waves and the dynamics of a rapidly moving crack [J]. Phys Rev Lett 88 8 (2002) 085503 (1-4).
    • (2002) Phys Rev Lett , vol.88 , Issue.8 , pp. 085503
    • SHARON, E.1    COHEN, G.2    FINEBERG, J.3
  • 13
    • 0346686247 scopus 로고    scopus 로고
    • Interaction of shear waves and propagating cracks [J]
    • (1-4).
    • BONAMY D., and RAVI-CHANDAR K. Interaction of shear waves and propagating cracks [J]. Phys Rev Lett 91 23 (2003) 235502 (1-4).
    • (2003) Phys Rev Lett , vol.91 , Issue.23 , pp. 235502
    • BONAMY, D.1    RAVI-CHANDAR, K.2
  • 15
    • 0016507662 scopus 로고
    • Mechanism of fracture in glassy materials capable of some inelastic deformation [J]
    • ARGON A., and SALAMA M. Mechanism of fracture in glassy materials capable of some inelastic deformation [J]. Mater Sci Eng 23 22 (1976) 219-230
    • (1976) Mater Sci Eng , vol.23 , Issue.22 , pp. 219-230
    • ARGON, A.1    SALAMA, M.2
  • 16
    • 18144420831 scopus 로고    scopus 로고
    • Fracture of brittle metallic glasses: Brittleness or plasticity [J]
    • (1-4).
    • XI X., ZHAO D., PAN M., WANG W., WU Y., and LEWANDOWSKI J. Fracture of brittle metallic glasses: Brittleness or plasticity [J]. Phys Rev Lett 94 (2005) 125510 (1-4).
    • (2005) Phys Rev Lett , vol.94 , pp. 125510
    • XI, X.1    ZHAO, D.2    PAN, M.3    WANG, W.4    WU, Y.5    LEWANDOWSKI, J.6
  • 17
    • 0002836944 scopus 로고    scopus 로고
    • Ductility of bulk nanocrystalline composites and metallic glasses at room temperature [J]
    • FAN C., and INOUE A. Ductility of bulk nanocrystalline composites and metallic glasses at room temperature [J]. Appl Phys Lett 77 (2000) 46-68
    • (2000) Appl Phys Lett , vol.77 , pp. 46-68
    • FAN, C.1    INOUE, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.