1
-
-
0033686782
-
Flexural strength and toughness of liquid phase sintered silicon carbide
-
Magnani G., Minoccari G.L., and Pilotti L. Flexural strength and toughness of liquid phase sintered silicon carbide. Ceram. Int. 26 5 (2000) 495-500
-
(2000)
Ceram. Int.
, vol.26
, Issue.5
, pp. 495-500
-
-
Magnani, G.1
Minoccari, G.L.2
Pilotti, L.3
-
2
-
-
0034517072
-
Potential of SiC as a heat exchanger material in combined cycle plant
-
Steen M., and Ranzani L. Potential of SiC as a heat exchanger material in combined cycle plant. Ceram. Int. 26 8 (2000) 849-854
-
(2000)
Ceram. Int.
, vol.26
, Issue.8
, pp. 849-854
-
-
Steen, M.1
Ranzani, L.2
-
3
-
-
0035155565
-
Reaction mechanism and microstructure development of strain tolerant in situ SiC-BN composites
-
Zhang G.J., Beppu Y., Ohji T., and Kanzaki S. Reaction mechanism and microstructure development of strain tolerant in situ SiC-BN composites. Acta Mater. 49 (2001) 77
-
(2001)
Acta Mater.
, vol.49
, pp. 77
-
-
Zhang, G.J.1
Beppu, Y.2
Ohji, T.3
Kanzaki, S.4
-
4
-
-
84985107903
-
Phase and property studies of SiC-BN Composites
-
Ruh R., Zangvil A., and Wills R.R. Phase and property studies of SiC-BN Composites. Adv. Ceram. Mater. 3 4 (1988) 411
-
(1988)
Adv. Ceram. Mater.
, vol.3
, Issue.4
, pp. 411
-
-
Ruh, R.1
Zangvil, A.2
Wills, R.R.3
-
5
-
-
38149109419
-
-
Z.-H. Yang, Microstructure and properties of in-situ formed SiC-BN ceramic matrix composites, Master thesis, Harbin Institute of Technology, PR China, 2003.
-
-
-
-
6
-
-
0033700818
-
Oxidation of SiC powders in SiC/alumina/zirconia compacts
-
Lin Y.-J., and Chen L.-J. Oxidation of SiC powders in SiC/alumina/zirconia compacts. Ceram. Int. 26 (2000) 593-598
-
(2000)
Ceram. Int.
, vol.26
, pp. 593-598
-
-
Lin, Y.-J.1
Chen, L.-J.2
-
7
-
-
0032626259
-
High-temperature oxidation of boron nitride. II. Boron nitride layers in composites
-
Jacobson N.S., Morscher G.N., Bryant D.R., and Tressler R.E. High-temperature oxidation of boron nitride. II. Boron nitride layers in composites. J. Am. Ceram. Soc. 82 6 (1999) 1473-1482
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, Issue.6
, pp. 1473-1482
-
-
Jacobson, N.S.1
Morscher, G.N.2
Bryant, D.R.3
Tressler, R.E.4
-
8
-
-
0025460632
-
Effects of active oxidation on the flexural strength of α-silicon carbide
-
Kim H.E., and Moorhead A.J. Effects of active oxidation on the flexural strength of α-silicon carbide. J. Am. Ceram. Soc. 73 7 (1990) 1868-1872
-
(1990)
J. Am. Ceram. Soc.
, vol.73
, Issue.7
, pp. 1868-1872
-
-
Kim, H.E.1
Moorhead, A.J.2
-
9
-
-
0022893202
-
Effective sintering aids for silicon carbide ceramics: reactivities of silicon carbide with various additives
-
Negita K. Effective sintering aids for silicon carbide ceramics: reactivities of silicon carbide with various additives. J. Am. Ceram. Soc. 69 12 (1986) C308-C310
-
(1986)
J. Am. Ceram. Soc.
, vol.69
, Issue.12
-
-
Negita, K.1
|