메뉴 건너뛰기




Volumn 63, Issue 9, 1993, Pages 1209-1210

Visible light emission from a pn junction of porous silicon and microcrystalline silicon carbide

Author keywords

[No Author keywords available]

Indexed keywords


EID: 36449006096     PISSN: 00036951     EISSN: None     Source Type: Journal    
DOI: 10.1063/1.109773     Document Type: Article
Times cited : (41)

References (17)
  • 16
    • 84954068054 scopus 로고
    • Botha-Si and a-SiC films which are prepared by glow discharge (GD) plasma CVD or ECR plasma CVD show PL at a room temperature if they contain a large amount of hydrogen. However, PL is not observed at a room temperature for [formula omitted] and [formula omitted] deposited by GD CVD or ECR plasma CVD because hydrogen content in their films is less than several percent. See, for example
    • (1981) Jpn. J. Appl. Phys. , vol.20 , pp. L793
    • Hata, N.1    Yamasaki, S.2    Oheda, H.3    Matsuda, A.4    Okushi, H.5    Tanaka, K.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.