1
-
-
33845384374
-
Compressive failure of unidirectional hybrid fibre-reinforced epoxy composites containing carbon and silicon carbide fibres
-
Sudarisman, Davies I.J., and Hamada H. Compressive failure of unidirectional hybrid fibre-reinforced epoxy composites containing carbon and silicon carbide fibres. Composites Part A 38 (2007) 1070-1074
-
(2007)
Composites Part A
, vol.38
, pp. 1070-1074
-
-
Sudarisman1
Davies, I.J.2
Hamada, H.3
-
2
-
-
34147125410
-
A self-healing carbon fibre reinforced polymer for aerospace applications
-
Williams G., Trask R., and Bond I. A self-healing carbon fibre reinforced polymer for aerospace applications. Composites Part A 38 (2007) 1525-1532
-
(2007)
Composites Part A
, vol.38
, pp. 1525-1532
-
-
Williams, G.1
Trask, R.2
Bond, I.3
-
3
-
-
0037330624
-
The assessment of novel materials and processes for the impact tolerant design of stiffened composite aerospace structures
-
Greenhalgh E., and Hiley M. The assessment of novel materials and processes for the impact tolerant design of stiffened composite aerospace structures. Composites Part A 34 (2003) 151-161
-
(2003)
Composites Part A
, vol.34
, pp. 151-161
-
-
Greenhalgh, E.1
Hiley, M.2
-
5
-
-
28244486010
-
Synthesis of phosphorus-based flame retardant systems and their use in an epoxy resin
-
Toldy A., Tóth N., Anna P., and Marosi G. Synthesis of phosphorus-based flame retardant systems and their use in an epoxy resin. Polym Degrad Stab 91 (2006) 585-592
-
(2006)
Polym Degrad Stab
, vol.91
, pp. 585-592
-
-
Toldy, A.1
Tóth, N.2
Anna, P.3
Marosi, G.4
-
6
-
-
33646497481
-
Nanostructured layered copper hydroxy dodecyl sulfate: a potential fire retardant for poly(vinyl ester) (PVE)
-
Kandare E., Chigwada G., Wang D., Wilkie C.A., and Hossenlopp J.M. Nanostructured layered copper hydroxy dodecyl sulfate: a potential fire retardant for poly(vinyl ester) (PVE). Polym Degrad Stab 91 (2006) 1781-1790
-
(2006)
Polym Degrad Stab
, vol.91
, pp. 1781-1790
-
-
Kandare, E.1
Chigwada, G.2
Wang, D.3
Wilkie, C.A.4
Hossenlopp, J.M.5
-
7
-
-
33646352241
-
Probing synergism, antagonism, and additive effects in poly(vinyl ester) (PVE) composites with fire retardants
-
Kandare E., Chigwada G., Wang D., Wilkie C.A., and Hossenlopp J.M. Probing synergism, antagonism, and additive effects in poly(vinyl ester) (PVE) composites with fire retardants. Polym Degrad Stab 91 (2006) 1209-1218
-
(2006)
Polym Degrad Stab
, vol.91
, pp. 1209-1218
-
-
Kandare, E.1
Chigwada, G.2
Wang, D.3
Wilkie, C.A.4
Hossenlopp, J.M.5
-
8
-
-
0030284196
-
Complex char formation in flame-retarded fibre-intumescent combinations-II. Thermal analytical studies
-
Kandola B.K., and Horrocks R.A. Complex char formation in flame-retarded fibre-intumescent combinations-II. Thermal analytical studies. Polym Degrad Stab 54 (1996) 289-303
-
(1996)
Polym Degrad Stab
, vol.54
, pp. 289-303
-
-
Kandola, B.K.1
Horrocks, R.A.2
-
9
-
-
0000110496
-
Evidence of interaction in flame-retardant fibre-intumescent combinations by thermal analytical techniques
-
Kandola B.K., Horrocks S., and Horrocks R.A. Evidence of interaction in flame-retardant fibre-intumescent combinations by thermal analytical techniques. Thermochimica Acta 294 (1997) 113-125
-
(1997)
Thermochimica Acta
, vol.294
, pp. 113-125
-
-
Kandola, B.K.1
Horrocks, S.2
Horrocks, R.A.3
-
10
-
-
0030191871
-
Complex char formation in flame retarded fibre-intumescent combinations: 1. scanning electron microscopic studies
-
Horrocks R.A., Anand S.C., and Sanderson D. Complex char formation in flame retarded fibre-intumescent combinations: 1. scanning electron microscopic studies. Polymer 37 (1996) 3197-3206
-
(1996)
Polymer
, vol.37
, pp. 3197-3206
-
-
Horrocks, R.A.1
Anand, S.C.2
Sanderson, D.3
-
11
-
-
33846828759
-
Thermal oxidative degradation kinetics of flame-retarded polypropylene with intumescent flame-retardant master batches in situ prepared in twin-screw extruder
-
Chen Y., and Wang Q. Thermal oxidative degradation kinetics of flame-retarded polypropylene with intumescent flame-retardant master batches in situ prepared in twin-screw extruder. Polym Degrad Stab 92 (2007) 280-291
-
(2007)
Polym Degrad Stab
, vol.92
, pp. 280-291
-
-
Chen, Y.1
Wang, Q.2
-
12
-
-
33748774406
-
Intumescent fire protective coating: toward a better understanding of their mechanism of action
-
Jimenez M., Duquesne S., and Bourbigot S. Intumescent fire protective coating: toward a better understanding of their mechanism of action. Thermochimica Acta 449 (2006) 16-26
-
(2006)
Thermochimica Acta
, vol.449
, pp. 16-26
-
-
Jimenez, M.1
Duquesne, S.2
Bourbigot, S.3
-
13
-
-
0036064587
-
A study of the global kinetics of thermal degradation of a fibre-intumescent mixture
-
Neininger S.M., Staggs J.E.J., Horrocks A.R., and Hill N.J. A study of the global kinetics of thermal degradation of a fibre-intumescent mixture. Polym Degrad Stab 77 (2002) 187-194
-
(2002)
Polym Degrad Stab
, vol.77
, pp. 187-194
-
-
Neininger, S.M.1
Staggs, J.E.J.2
Horrocks, A.R.3
Hill, N.J.4
-
14
-
-
34948903500
-
-
Neininger SM. Mathematical modelling of intumescent-interactive flame retardant composites, Ph.D. dissertation, University of Bolton (formerly Bolton Institute of Higher Education); 2002.
-
-
-
-
15
-
-
0027847926
-
Thermal oxidative degradation of an epoxy resin
-
Rose N., Le Bras M., Delobel R., Costes B., and Henry Y. Thermal oxidative degradation of an epoxy resin. Polym Degrad Stab 42 (1993) 307-316
-
(1993)
Polym Degrad Stab
, vol.42
, pp. 307-316
-
-
Rose, N.1
Le Bras, M.2
Delobel, R.3
Costes, B.4
Henry, Y.5
-
16
-
-
0028715492
-
Thermal oxidative degradation of epoxy resins: evaluation of their heat resistance using invariant kinetic parameters
-
Rose N., Le Bras M., Bourbigot S., and Delobel R. Thermal oxidative degradation of epoxy resins: evaluation of their heat resistance using invariant kinetic parameters. Polym Degrad Stab 45 (1994) 387-397
-
(1994)
Polym Degrad Stab
, vol.45
, pp. 387-397
-
-
Rose, N.1
Le Bras, M.2
Bourbigot, S.3
Delobel, R.4
-
17
-
-
0001688435
-
Mechanisms of thermal degradation of fire-retardant melamine salts
-
Nelson G.L. (Ed), American Chemical Society, Washington, DC
-
Costa L., Camino G., and Luda di Cortemiglia M.P. Mechanisms of thermal degradation of fire-retardant melamine salts. In: Nelson G.L. (Ed). Fire and polymers: hazards, identification and prevention (1990), American Chemical Society, Washington, DC 211-238
-
(1990)
Fire and polymers: hazards, identification and prevention
, pp. 211-238
-
-
Costa, L.1
Camino, G.2
Luda di Cortemiglia, M.P.3
-
18
-
-
0025258209
-
Thermal degradation of dipentaerythritol diphosphate, model compound for fire retardant intumescent systems: part I - overall thermal degradation
-
Camino G., Martinasso G., and Costa L. Thermal degradation of dipentaerythritol diphosphate, model compound for fire retardant intumescent systems: part I - overall thermal degradation. Polym Degrad Stab 27 (1990) 285-296
-
(1990)
Polym Degrad Stab
, vol.27
, pp. 285-296
-
-
Camino, G.1
Martinasso, G.2
Costa, L.3
-
19
-
-
0025232991
-
Thermal degradation of dipentaerythritol diphosphate, model compound for fire retardant intumescent systems: part II - intumescent step
-
Camino G., Martinasso G., Costa L., and Gobetto R. Thermal degradation of dipentaerythritol diphosphate, model compound for fire retardant intumescent systems: part II - intumescent step. Polym Degrad Stab 28 (1990) 17-38
-
(1990)
Polym Degrad Stab
, vol.28
, pp. 17-38
-
-
Camino, G.1
Martinasso, G.2
Costa, L.3
Gobetto, R.4
|